# US 2026/0062781 A1 · High-strength oil casing resistant to co2 and microbial corrosion and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0062781 A1
- Document ID: US20260062781A1
- Status: Published application
- Kind: A1
- Application number: 19/105,937
- Filed: 2023-08-30
- Published: 2026-03-05
- Earliest claimed: 2022-08-30
- Assignees: Baoshan Iron & Steel Co., Ltd.
- Applicants: Baoshan Iron & Steel Co., Ltd.
- Inventors: Yameng Qi; Xiong Zhou; Chunxia Zhang; Zhonghua Zhang; Zhan Gao
- Web page: https://patentgrep.com/patent/US20260062781A1

## CPC

- C22C 38/58: with more than 1.5% by weight of manganese
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 1/25: Hardening, combined with annealing between 300 degrees Celsius and 600 degrees Celsius, i.e. heat refining ("Vergüten")
- C21D 1/26: Methods of annealing
- C21D 6/004: {containing Cr and Ni}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/00: Modifying the physical properties of ferrous metals or ferrous alloys by deformation combined with, or followed by, heat treatment (hardening articles or materials formed by forging or rolling with no further heating beyond that required for the formation C21D1/02)
- C21D 8/10: during manufacturing of tubular bodies
- C21D 9/0068: {for particular articles not mentioned below}
- C21D 9/08: for tubular bodies or pipes
- C21D 9/085: {Cooling or quenching}
- C21D 9/14: wear-resistant or pressure-resistant pipes
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/16: containing copper
- C22C 38/18: containing chromium
- C22C 38/20: with copper
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/54: with boron
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)

## Abstract

The present disclosure provides a high-strength oil casing resistant to CO2 and microbial corrosion and a manufacturing method therefor. The oil casing comprises, in addition to Fe and inevitable impurities, the following chemical elements in percentage by mass: C: 0.06-0.20%, Cr: 1.5-7.0%, Cu: 0.3-3.5%, P≤0.015, S≤0.007. For the oil casing of the present disclosure, an oil casing with CO2-SRB-TGB corrosion resistance, a yield strength of ≥758 MPa, preferably ≥800 MPa, and a full-sized impact energy at 0° C. of ≥80J, preferably ≥95J can be obtained by controlling the amounts of Cr and Cu added and the contents of impurity elements P and S, optimizing the proportion of chemical elements, and combining TMCP manufacturing process, controlling the rolling temperature, the temperature before cooling and the cooling rate.

## Claims

### Claim 1

An oil casing, wherein the oil casing comprises, in addition to Fe and inevitable impurities, the following chemical elements in percentage by mass: C: 0.06%-0.20%, Cr: 1.5%-7.0%, Cu: 0.3%-3.5%, P≤0.050% and S≤0.010%, preferably P≤0.015% and S≤0.007%.

### Claim 2 (depends on 1)

The oil casing according to claim 1, wherein the oil casing further comprises REM in percentage by mass: 0.07%-0.75%, preferably 0.10%-0.75%.

### Claim 3 (depends on 2)

The oil casing according to claim 2, wherein the REM comprises one or both of La and Ce, and contents of La and Ce in percentage by mass satisfy the following inequality: 0.07%≤La+Ce≤0.35%, preferably 0.15%≤La+Ce≤0.35%.

### Claim 4 (depends on 1)

The oil casing according to claim 1, wherein a Cr content is 3.0-7.0%, preferably 3.0-5.0%; and/or a Cu content is 1.5%-3.5%.

### Claim 5 (depends on 1)

The oil casing according to claim 1, wherein the oil casing further comprises the following chemical elements in percentage by mass: Si: 0.1%-1.0%, Mn: 0.10%-2.5%, Ni: 0.5%-3.5%, Mo: 0.1%-3.5%, Nb: 0.02%-0.15%, V: 0.01%-0.20%, Al: 0.01%-0.08%, B: 0.0010%-0.008%.

### Claim 6 (depends on 5)

The oil casing according to claim 5, wherein the oil casing satisfies one or more of the following:
Mn: 0.5-2.5%;
Ni: 1.0-3.5%;
Mo: 1.0-3.5%; and
V: 0.06-0.20%.

### Claim 7 (depends on 1)

The oil casing according to claim 1, wherein the oil casing has an average corrosion rate of <0.0250 mm/a and a local corrosion rate of <0.0450 mm/a measured according to ASTM G111-97 (2013) standard.

### Claim 8 (depends on 1)

The oil casing according to claim 1, wherein the oil casing has a yield strength of ≥758 MPa, preferably ≥800 MPa, a full-sized impact energy at 0° C. of ≥80 J, preferably ≥95 J; and/or, a microstructure of tempered sorbite.

### Claim 9 (depends on 1)

A method for manufacturing the oil casing according to claim 1, wherein the method comprises the following steps:
S1: performing smelting and casting on molten steel, and then forging or rolling to obtain a pipe blank;
S2: performing heating, heat holding, piercing, continuous-rolling, and stretch reducing or sizing on the pipe blank of step S1, obtaining a pierced billet; wherein a rolling temperature in the continuous-rolling step is 900-970° C.;
S3: cooling the pierced billet of step S2 to room temperature, obtaining an oil casing; preferably, water-cooling the pierced billet of step S2, wherein a temperature of the pierced billet before cooling is ≥870° C. and a cooling rate is 20-60° C./s.

### Claim 10 (depends on 9)

The method according to claim 9, wherein in step S2, a temperature of the heating is 1220-1280° C., and a time of the heat holding is 1-4 hours.

### Claim 11 (depends on 9)

The method according to claim 9, wherein in step S2, a temperature of the piercing is 1170-1250° C.

### Claim 12 (depends on 9)

The method according to claim 9, wherein the method further comprises the following steps:
S4: performing a tempering heat treatment on the oil casing of step S3, wherein a tempering temperature is 530-630° C. and a holding time is 40-60 minutes.

### Claim 13 (depends on 9)

The method according to claim 9, wherein the oil casing further comprises REM in percentage by mass: 0.07%-0.75%, preferably 0.10%-0.75%.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the REM comprises one or both of La and Ce, and contents of La and Ce in percentage by mass satisfy the following inequality: 0.07%≤La+Ce≤0.35%, preferably 0.15%≤La+Ce≤0.35%.

### Claim 15 (depends on 9)

The method according to claim 9, wherein a Cr content is 3.0-7.0%, preferably 3.0-5.0%; and/or a Cu content is 1.5%-3.5%.

### Claim 16 (depends on 9)

The method according to claim 9, wherein the oil casing further comprises the following chemical elements in percentage by mass: Si: 0.1%-1.0%, Mn: 0.10%-2.5%, Ni: 0.5%-3.5%, Mo: 0.1%-3.5%, Nb: 0.02%-0.15%, V: 0.01%-0.20%, Al: 0.01%-0.08%, B: 0.0010%-0.008%.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the oil casing satisfies one or more of the following:
Mn: 0.5-2.5%;
Ni: 1.0-3.5%;
Mo: 1.0-3.5%; and
V: 0.06-0.20%.

### Claim 18 (depends on 9)

The method according to claim 9, wherein the oil casing has an average corrosion rate of <0.0250 mm/a and a local corrosion rate of <0.0450 mm/a measured according to ASTM G111-97 (2013) standard.

### Claim 19 (depends on 9)

The method according to claim 9, wherein the oil casing has a yield strength of ≥758 MPa, preferably ≥800 MPa, a full-sized impact energy at 0° C. of ≥80 J, preferably ≥95 J; and/or, a microstructure of tempered sorbite.