# US 2026/0062780 A1 · Ultra high strength and high ductility steel sheet having excellent yield ratio and manufacturing method for same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0062780 A1
- Document ID: US20260062780A1
- Status: Published application
- Kind: A1
- Application number: 19/386,214
- Filed: 2025-11-11
- Published: 2026-03-05
- Earliest claimed: 2018-09-04
- Assignees: Posco
- Applicants: Posco Co., Ltd
- Inventors: Joo-Hyun RYU; Kyoo-Young LEE; Sea-Woong LEE
- Web page: https://patentgrep.com/patent/US20260062780A1

## CPC

- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/50: with titanium or zirconium
- B32B 15/013: {one layer being formed of an iron alloy or steel, another layer being formed of a metal other than iron or aluminium}
- C21D 1/26: Methods of annealing
- C21D 6/00: Heat treatment of ferrous alloys
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0247: characterised by the heat treatment
- C21D 9/46: for sheet metals
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/14: containing titanium or zirconium
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C23C 2/02: Pretreatment of the material to be coated, e.g. for coating on selected surface areas (C23C2/30 takes precedence)
- C23C 2/0224: {Two or more thermal pretreatments}
- C23C 2/06: Zinc or cadmium or alloys based thereon
- C23C 2/28: Thermal after-treatment, e.g. treatment in oil bath
- C21D 2211/001: Austenite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C21D 2221/00: Treating localised areas of an article
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Provided is a method for manufacturing an ultra high-strength and high-ductility steel sheet having an excellent yield ratio. The method includes: heating a slab in a temperature range of 1050 to 1300° C.; finish hot rolling the heated slab in a temperature range of 800° C. to 1000° C.; winding the hot-rolled steel sheet in a temperature range of 50° C. to 750° C.; cold rolling the wound hot-rolled steel sheet at a reduction rate of 15% or higher after pickling; and annealing the cold-rolled steel sheet in a temperature range of 600° C. to 720° C. for 10 sec to 3,600 sec, or annealing in a temperature range of higher than 720° C. and 900° C. or lower for 10 sec to 3,600 sec and cooling, followed by a second annealing in a temperature range of 480° C. to 700° C. for 10 sec to 3,600 sec.

## Claims

### Claim 1

A method for manufacturing an ultra high-strength and high-ductility steel sheet having an excellent yield ratio, comprising:
heating a slab comprising, by wt % 0.1% to 0.3% of carbon (C), 2% or less of silicon (Si), 6-10% of manganese (Mn), 0.05% or less of phosphorus (P), 0.02% or less of sulfur(S), 0.02% or less of nitrogen (N), 0.5% or less (excluding 0%) of aluminum (Al), and a balance Fe and inevitable impurities, and further comprising one or more selected from the group consisting of 0.1% or less of titanium (Ti), 0.1% or less of niobium (Nb), 0.2% or less of vanadium (V), and 0.5% or less of molybdenum (Mo), in a temperature range of 1050° C. to 1300° C.;
preparing a hot-rolled steel sheet by finish hot rolling the heated slab in a temperature range of 800° C. to 1000° C.;
winding the hot-rolled steel sheet in a temperature range of 50° C. to 750° C.;
preparing a cold-rolled steel sheet by cold rolling the wound hot-rolled steel sheet at a reduction rate of 15% or higher after pickling; and
selectively annealing the cold-rolled steel sheet under any one of a first annealing condition and a second annealing condition,
wherein the first annealing condition involves annealing the cold-rolled steel sheet in a temperature range of 600° C. to 720° C. for 10 sec to 3,600 sec, and
the second annealing condition involves first annealing in a temperature range of higher than 720° C. and 900° C. or lower for 10 sec to 3,600 sec and cooling, followed by second annealing in a temperature range of 480° C. to 700° C. for 10 sec to 3,600 sec.

### Claim 2 (depends on 1)

The method of claim 1, wherein the slab further comprises one or more selected from the group consisting of nickel (Ni): 0.1 wt % or less, copper (Cu): 0.5 wt % or less and chromium (Cr): 0.1 wt % or less.