# US 2026/0062766 A1 · Method for recovering valuable metals

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0062766 A1
- Document ID: US20260062766A1
- Status: Published application
- Kind: A1
- Application number: 19/107,059
- Filed: 2023-08-10
- Published: 2026-03-05
- Earliest claimed: 2022-09-01
- Assignees: Sumitomo Metal Mining Co., Ltd.
- Applicants: Sumitomo Metal Mining Co., Ltd.
- Inventors: Toshihiko Nagakura; Takayuki Yabe
- Web page: https://patentgrep.com/patent/US20260062766A1

## CPC

- C22B 1/02: Roasting processes (C22B1/16 takes precedence)
- C22B 5/10: by solid carbonaceous reducing agents
- C22B 7/001: {Dry processes}
- C22B 7/007: {by acid leaching}
- C22B 15/0071: {containing sulfur}
- C22B 23/043: {Sulfurated acids or salts thereof}
- C22B 23/0461: {by chemical methods}
- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- Y02P 10/20: Recycling
- Y02W 30/84: Recycling of batteries or fuel cells
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

To provide a method of recovering, at low cost, valuable metals from waste lithium-ion batteries by a dry smelting process. The present invention is a method of recovering valuable metals from waste lithium-ion batteries, the method comprising: an oxidation roasting step S3 in which oxidation roasting is implemented on a raw material containing waste lithium-ion batteries; and a reduction step S4 in which the obtained oxidation-roasted matter is reduced in the presence of carbon. In the oxidation roasting step S3, an oxidant of 1.5 times or more the chemical equivalent of carbon within the raw material to be treated is introduced, and the oxidation roasting is carried out at a processing temperature selected in a range of 600° C. to 900° C., so that the carbon grade of the obtained oxidation-roasted matter will be less than 1.0 mass %.

## Claims

### Claim 1

A method for recovering valuable metals from waste lithium-ion batteries, the method comprising:
an oxidative roasting step of carrying out an oxidative roasting treatment on a raw material containing the waste lithium-ion batteries, and
a reduction step of reducing an obtained oxidatively roasted material in presence of carbon,
a carbon grade of the obtained oxidatively roasted material being less than 1.0 mass % by introducing an oxidant in an amount of 1.5 times or more chemical equivalent of carbon in the raw material to be treated, and carrying out the oxidative roasting treatment at a treatment temperature selected in a range of 600° C. or higher and 900° C. or lower in the oxidative roasting step.

### Claim 2 (depends on 1)

The method for recovering valuable metals according to claim 1,
wherein in the reduction step, the oxidatively roasted material is reduced and melted in presence of carbon to obtain a molten material containing a slag and an alloy containing valuable metals.

### Claim 3 (depends on 1)

The method for recovering valuable metals according to claim 1,
wherein a carbon grade of the raw material containing waste lithium-ion batteries is 26 mass % or less, and
in the oxidative roasting step, an amount of the oxidant introduced is 2.0 times or more and 3.0 times or less chemical equivalent of carbon in the raw material to be treated, and a treatment time of the oxidative roasting treatment is two hours or longer and shorter than 3 hours.

### Claim 4 (depends on 2)

The method for recovering valuable metals according to claim 2,
wherein a carbon grade of the raw material containing waste lithium-ion batteries is 26 mass % or less, and
in the oxidative roasting step, an amount of the oxidant introduced is 2.0 times or more and 3.0 times or less chemical equivalent of carbon in the raw material to be treated, and a treatment time of the oxidative roasting treatment is two hours or longer and shorter than 3 hours.