# US 2026/0062587 A1 · Solvent-free polyurethane slurry and preparation method thereof, and environmental-friendly resin-coated protective gloves and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0062587 A1
- Document ID: US20260062587A1
- Status: Published application
- Kind: A1
- Application number: 18/817,392
- Filed: 2024-08-28
- Published: 2026-03-05
- Earliest claimed: 2024-08-28
- Assignees: WonderGrip(CHINA)CO., Ltd.
- Applicants: WonderGrip(CHINA)CO., Ltd.
- Inventors: Guoda Dai; Menglu Dai; Genkai Watanabe; Wei Wen
- Web page: https://patentgrep.com/patent/US20260062587A1

## CPC

- C09D 175/04: Polyurethanes
- A41D 19/0006: {made of several layers of material}
- A41D 19/015: Protective gloves {(A41D19/0055 takes precedence)}
- C08G 18/18: containing secondary or tertiary amines or salts thereof
- C08G 18/3206: {aliphatic}
- C08G 18/4829: {Polyethers containing at least three hydroxy groups (C08G18/4833 - C08G18/5096 take precedence)}
- C08G 18/4845: {containing oxypropylene or higher oxyalkylene end groups}
- C08G 18/672: {Esters of acrylic or alkyl acrylic acid having only one group containing active hydrogen}
- C08G 18/7671: {containing only one alkylene bisphenyl group}
- C08G 18/797: {containing carbodiimide and/or uretone-imine groups}
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- A41D: OUTERWEAR; PROTECTIVE GARMENTS; ACCESSORIES
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

Provided are a solvent-free polyurethane (PU) slurry and a preparation method thereof. Also provided are environmental-friendly resin-coated protective gloves and a preparation method thereof. The solvent-free PU slurry includes a component A and a component B, with a mass ratio of the component A to the component B ranging from 100:67 to 100:93.

## Claims

### Claim 1

A solvent-free polyurethane (PU) slurry, comprising:
a component A; and
a component B;
wherein a mass ratio of the component A to the component B ranges from 100:67 to 100:93;
wherein the component A comprises the following raw materials in parts by mass: 67 parts to 93 parts of a polyoxypropylene tetraol, 7 parts to 24 parts of a hydroxy acrylate, 0.3 parts to 5 parts of an alcohol chain extender, 0.7 parts to 7 parts of a photoinitiator, 0.03 parts to 0.7 parts of a delayed-action catalyst, and 0.03 parts to 0.8 parts of a foam stabilizer; and
wherein the component B comprises the following raw materials in parts by mass: 21 parts to 43 parts of a polyoxypropylene diol, 12 parts to 25 parts of a double-bond-containing terminal hydroxyl polymer, 45 parts to 61 parts of a polyisocyanate, and 0.008 parts to 0.05 parts of a polymerization inhibitor.

### Claim 2 (depends on 1)

The solvent-free PU slurry according to claim 1, wherein the polyoxypropylene tetraol has a number average molecular weight of 800 to 3,000.

### Claim 3 (depends on 1)

The solvent-free PU slurry according to claim 1, wherein the hydroxy acrylate comprises at least one member selected from the group consisting of hydroxyethyl acrylate, hydroxypropyl acrylate, hydroxyethyl methacrylate (HEMA), hydroxypropyl methacrylate (HPMA), trimethylolpropane diacrylate (TMPDA), and pentaerythritol triacrylate (PETA).

### Claim 4 (depends on 1)

The solvent-free PU slurry according to claim 1, wherein the polyoxypropylene diol has a number average molecular weight of 1,000 to 3,000.

### Claim 5 (depends on 1)

A resin-coated protective glove produced from the solvent-free PU slurry according to claim 1.

### Claim 6 (depends on 5)

The resin-coated protective glove according to claim 5, wherein the polyoxypropylene tetraol has a number average molecular weight of 800 to 3,000.

### Claim 7 (depends on 5)

The resin-coated protective glove according to claim 5, wherein the hydroxy acrylate comprises at least one member selected from the group consisting of hydroxyethyl acrylate, hydroxypropyl acrylate, hydroxyethyl methacrylate (HEMA), hydroxypropyl methacrylate (HPMA), trimethylolpropane diacrylate (TMPDA), and pentaerythritol triacrylate (PETA).

### Claim 8 (depends on 5)

The resin-coated protective glove according to claim 5, wherein the polyoxypropylene diol has a number average molecular weight of 1,000 to 3,000.

### Claim 9

A method for preparing a solvent-free PU slurry, the method comprising:
mixing a polyoxypropylene tetraol, a hydroxy acrylate, and an alcohol chain extender to obtain a first mixture;
subjecting the first mixture to first heating stirring and cooling in sequence;
adding a foam stabilizer to a resulting cooled product to obtain a second mixture;
subjecting the second mixture to second heating stirring to obtain a mixture system;
mixing the mixture system with a photoinitiator and a delayed-action catalyst to obtain a component A;
mixing a polyisocyanate and a polymerization inhibitor to obtain a third mixture;
subjecting the third mixture to third heating stirring;
adding a polyoxypropylene diol and a double-bond-containing terminal hydroxyl polymer to the third mixture;
subjecting a resulting product to heating reaction and vacuum defoamation in sequence to obtain a component B; and
mixing the component A and the component B to obtain the solvent-free PU slurry;
wherein a mass ratio of the component A to the component B ranges from 100:67 to 100:93;
wherein the component A comprises the following raw materials in parts by mass: 67 parts to 93 parts of the polyoxypropylene tetraol, 7 parts to 24 parts of the hydroxy acrylate, 0.3 parts to 5 parts of the alcohol chain extender, 0.7 parts to 7 parts of the photoinitiator, 0.03 parts to 0.7 parts of the delayed-action catalyst, and 0.03 parts to 0.8 parts of the foam stabilizer; and
wherein the component B comprises the following raw materials in parts by mass: 21 parts to 43 parts of the polyoxypropylene diol, 12 parts to 25 parts of the double-bond-containing terminal hydroxyl polymer, 45 parts to 61 parts of the polyisocyanate, and 0.008 parts to 0.05 parts of the polymerization inhibitor.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the polyoxypropylene tetraol has a number average molecular weight of 800 to 3,000.

### Claim 11 (depends on 9)

The method according to claim 9, wherein the hydroxy acrylate comprises at least one member selected from the group consisting of hydroxyethyl acrylate, hydroxypropyl acrylate, hydroxyethyl methacrylate (HEMA), hydroxypropyl methacrylate (HPMA), trimethylolpropane diacrylate (TMPDA), and pentaerythritol triacrylate (PETA).

### Claim 12 (depends on 9)

The method according to claim 9, wherein the polyoxypropylene diol has a number average molecular weight of 1,000 to 3,000.

### Claim 13

A method for making a resin-coated protective glove, the method comprising:
preparing a solvent-free polyurethane (PU) slurry that comprises a component A and a component B, wherein a mass ratio of the component A to the component B ranges from 100; 67 to 100; 93;
preheating a hand model covered with a glove core;
coating an anti-penetration agent on a surface of the glove core;
subjecting a resulting coated glove core to impregnating with the solvent-free PU slurry, ultraviolet (UV)-curing, and drying in sequence; and
then subjecting a resulting dried product to a post-treatment to obtain the resin-coated protective glove;
wherein the component A comprises the following raw materials in parts by mass: 67 parts to 93 parts of a polyoxypropylene tetraol, 7 parts to 24 parts of a hydroxy acrylate, 0.3 parts to 5 parts of an alcohol chain extender, 0.7 parts to 7 parts of a photoinitiator, 0.03 parts to 0.7 parts of a delayed-action catalyst, and 0.03 parts to 0.8 parts of a foam stabilizer; and
wherein the component B comprises the following raw materials in parts by mass: 21 parts to 43 parts of a polyoxypropylene diol, 12 parts to 25 parts of a double-bond-containing terminal hydroxyl polymer, 45 parts to 61 parts of a polyisocyanate, and 0.008 parts to 0.05 parts of a polymerization inhibitor.

### Claim 14 (depends on 13)

The method according to claim 13, wherein preparing the solvent-free PU slurry comprises:
mixing the polyoxypropylene tetraol, the hydroxy acrylate, and the alcohol chain extender to obtain a first mixture, and subjecting the first mixture to first heating stirring and cooling in sequence, and adding the foam stabilizer to a resulting cooled product to obtain a second mixture, and subjecting the second mixture to second heating stirring to obtain a mixture system;
mixing the mixture system with the photoinitiator and the delayed-action catalyst to obtain the component A;
mixing the polyisocyanate and the polymerization inhibitor to obtain a third mixture, and subjecting the third mixture to third heating stirring, and adding the polyoxypropylene diol and the double-bond-containing terminal hydroxyl polymer to the third mixture;
subjecting a resulting product to heating reaction and vacuum defoamation in sequence to obtain the component B; and
mixing the component A and the component B to obtain the solvent-free PU slurry.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the polyoxypropylene tetraol has a number average molecular weight of 800 to 3,000.

### Claim 16 (depends on 14)

The method according to claim 14, wherein the hydroxy acrylate comprises at least one member selected from the group consisting of hydroxyethyl acrylate, hydroxypropyl acrylate, hydroxyethyl methacrylate (HEMA), hydroxypropyl methacrylate (HPMA), trimethylolpropane diacrylate (TMPDA), and pentaerythritol triacrylate (PETA).

### Claim 17 (depends on 14)

The method according to claim 14, wherein the polyoxypropylene diol has a number average molecular weight of 1,000 to 3,000.

### Claim 18 (depends on 13)

The method according to claim 13, wherein the polyoxypropylene tetraol has a number average molecular weight of 800 to 3,000.

### Claim 19 (depends on 13)

The method according to claim 13, wherein the hydroxy acrylate comprises at least one member selected from the group consisting of hydroxyethyl acrylate, hydroxypropyl acrylate, hydroxyethyl methacrylate (HEMA), hydroxypropyl methacrylate (HPMA), trimethylolpropane diacrylate (TMPDA), and pentaerythritol triacrylate (PETA).

### Claim 20 (depends on 13)

The method according to claim 13, wherein the polyoxypropylene diol has a number average molecular weight of 1,000 to 3,000.