# US 2026/0062522 A1 · Ionomer dispersant for making aqueous polyolefin dispersions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0062522 A1
- Document ID: US20260062522A1
- Status: Published application
- Kind: A1
- Application number: 19/105,247
- Filed: 2023-08-22
- Published: 2026-03-05
- Earliest claimed: 2022-08-22
- Assignees: Dow Global Technologies LLC
- Applicants: Dow Global Technologies LLC
- Inventors: Hari Katepalli; David L. Malotky; Alexander Williamson; Joshua Enokida; Leslie O'Leary
- Web page: https://patentgrep.com/patent/US20260062522A1

## CPC

- C08J 3/05: from solid polymers
- C08L 23/142: {at least partially crystalline copolymers of propene with other olefins}
- C08J 3/203: {Solid polymers with solid and/or liquid additives}
- C08K 3/22: of metals
- C08F 210/02: Ethene
- C08J 2323/12: Polypropene
- C08J 2423/08: Copolymers of ethene (C08J2423/16 takes precedence)
- C08K 2003/262: {Alkali metal carbonates}
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

Methods for producing an aqueous polyolefin dispersion comprise providing a partially neutralized ionomer dispersant, which is an ethylene acid copolymer comprising the polymerized reaction product of 70 to 85 wt. % ethylene and 15 to 30 wt. % carboxylic acid containing comonomer, based on the total weight of monomers present in the ethylene acid copolymer, of which 0.01 to 30 mole % of the acid units are neutralized by alkali metal cations based on the total weight of monomers present in the ethylene acid copolymer. The methods further comprise melt blending the partially neutralized ionomer dispersant and polyolefin to produce a polymer melt blend, emulsifying the polymer melt blend in the presence of water and additional base to produce an emulsion, wherein the additional base further neutralizes a fraction or all of the remaining acid units, and diluting the emulsion with additional water to produce the aqueous polyolefin dispersion.

## Claims

### Claim 1

A method of producing an aqueous polyolefin dispersion comprising:
providing a partially neutralized ionomer dispersant, which comprises an ethylene acid copolymer wherein the ethylene acid copolymer comprises the polymerized reaction product of 70 to 85 wt. % ethylene and 15 to 30 wt. % carboxylic acid containing comonomer, based on the total weight of monomers present in the ethylene acid copolymer, wherein 0.01 to 30 mole % of total acid units of the ethylene acid copolymer are neutralized by alkali metal cations;
melt blending the partially neutralized ionomer dispersant and one or more polyolefins to produce a polymer melt blend;
emulsifying the polymer melt blend in the presence of water and additional base to produce an emulsion, wherein the additional base further neutralizes a fraction or all of the remaining acid units of the partially neutralized ionomer; and
diluting the emulsion with additional water to produce the aqueous polyolefin dispersion.

### Claim 2 (depends on 1)

The method of claim 1, wherein the carboxylic acid containing comonomer comprises methacrylic acid, acrylic acid, or combinations thereof.

### Claim 3 (depends on 1)

The method of claim 1, wherein melt blending and emulsifying occurs at a temperature from 100 to 250° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the aqueous polyolefin dispersion comprises 30 to 60 wt. % total solids.

### Claim 5 (depends on 4)

The method of claim 4, wherein the total solids have an average particle size of less than or equal to 2 μm.

### Claim 6 (depends on 1)

The method of claim 1, wherein the alkali metal comprises sodium.

### Claim 7 (depends on 1)

The method of claim 1, wherein the additional base comprises KOH.

### Claim 8 (depends on 1)

The method of claim 1, wherein the melt index (I2) of the partially neutralized ionomer dispersant is between 35 to 750 g/10 min, or between 60 and 250 g/10 min as determined according to ASTM D1238 (at 190° C. 2.16 kg).

### Claim 9 (depends on 1)

The method of claim 1, wherein the melt index (I2) of the ethylene acid copolymer prior to neutralization is between 100 and 1000 g/10 min, or between 200 to 400 g/10 min as determined according to ASTM D1238 (at 190° C., 2.16 kg).

### Claim 10 (depends on 1)

The method of claim 1, wherein the partially neutralized ionomer dispersant has from 0.1 mole % to 30 mole %, from 1 mole % to 30 mole %, from 2 mole % to 30 mole %, from 2 to 20 mole %, or from 5 to 20 mole % of total acid units neutralized by alkali metal cations.

### Claim 11 (depends on 1)

The method of claim 1, wherein the polyolefin comprises ethylene/alpha-olefin copolymer having a melt index (I2) of 0.1 to 100.0 g/10 min as determined according to ASTM D1238 (at 190° C. 2.16 kg).

### Claim 12 (depends on 1)

The method of claim 1, wherein the polyolefin comprises propylene/ethylene copolymer having a melt flow rate of 0.5 to 75 g/10 min as determined according to ASTM D-1238, Procedure B (condition 230° C./2.16 kg).

### Claim 13 (depends on 1)

The method of any of claim 1, wherein the polyolefin is selected from the group consisting of polyethylene or polypropylene.

### Claim 14 (depends on 1)

An aqueous polyolefin dispersion produced from the method of claim 1.

### Claim 15 (depends on 14)

A coated article produced from the aqueous polyolefin dispersion of claim 14.