# US 2026/0062340 A1 · Front-loaded stress profiles for high-stress applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0062340 A1
- Document ID: US20260062340A1
- Status: Published application
- Kind: A1
- Application number: 19/311,122
- Filed: 2025-08-27
- Published: 2026-03-05
- Earliest claimed: 2024-08-30
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Venkatesh BOTU; Timothy Michael GROSS; Qiao LI; Rostislav Vatchev ROUSSEV; Ljerka UKRAINCZYK
- Web page: https://patentgrep.com/patent/US20260062340A1

## CPC

- C03C 3/091: containing aluminium
- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 3/083: containing aluminium oxide or an iron compound
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 4/00: Compositions for glass with special properties
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 2201/32: containing aluminium (C03C2201/36 takes precedence)
- C03C 2201/50: containing alkali metals
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

Glass articles having high surface compressive stress (CS) and high CS-integrated area are provided. Methods of making such articles include chemical ion exchange processes.

## Claims

### Claim 1

A glass article comprising:
opposing first and second surfaces defining a body of the article having a thickness (t);
a stress profile of the body comprising:
a spike region extending from the first surface to a knee located at a depth of layer (DOL);
a peak compressive stress (CSmax) of the spike region being greater than or equal to 1150 MPa;
a tail region extending from the knee to a center of the glass article having a central tension (CT) and including a depth of compression (DOC);
a compressive stress integral at a depth of 5 micrometers that is greater than or equal to 4.75 MPa·millimeter; and
the compressive stress integral at a depth of 8 micrometers that is greater than or equal to 6.7 MPa·millimeter.

### Claim 2 (depends on 1)

The glass article of claim 1, wherein the t is in a range of 0.30 millimeters to 1.5 millimeters.

### Claim 3 (depends on 1)

The glass article of claim 1, wherein the DOC is greater than or equal to 0.020·t.

### Claim 4 (depends on 1)

The glass article of claim 1, including one or more of the following:
the compressive stress integral at a depth of 12 micrometers is greater than or equal to 8.0 MPa·millimeter; and
the compressive stress integral at a depth of 16 micrometers is greater than or equal to 8.3 MPa·millimeter.

### Claim 5 (depends on 1)

The glass article of claim 1, wherein the peak compressive stress (CSmax) of the spike region is greater than or equal to 1200 MPa, 1250 MPa, 1300 MPa, or 1350 MPa.

### Claim 6 (depends on 1)

The glass article of claim 1, wherein the compressive stress integral at a depth of 5 micrometers is greater than or equal to 5 MPa·millimeter.

### Claim 7 (depends on 1)

The glass article of claim 1 comprising an alkali aluminosilicate central composition having a sodium oxide content in a range of greater than or equal to 4.0 mol % to less than or equal to 15.0 mol % Na2O.

### Claim 8 (depends on 1)

The glass article of claim 1 comprising an alkali aluminosilicate central composition having a Young's modulus that is greater than or equal to 76 GPa or greater than or equal to 80 GPa; and/or a facture toughness of greater than or equal to 0.78; and/or a Na2O/Li2O molar ratio in a range of greater than or equal to 1.5 to less than or equal to 2.1.

### Claim 9

A glass article comprising:
opposing first and second surfaces defining a body of the article having a thickness (t) of greater than or equal to 0.70 millimeters to less than or equal to 1.3 millimeters;
a stress profile of the body comprising:
a spike region extending from the first surface to a knee located at a depth of layer (DOL);
a peak compressive stress (CSmax) of the spike region being greater than or equal to 1000 MPa;
a tail region extending from the knee to a center of the glass article having a central tension (CT) and including a depth of compression (DOC); and
a compressive stress integral at a depth of 5 micrometers that is greater than or equal to 4.75 MPa·millimeter; and
the compressive stress integral at a depth of 8 micrometers that is greater than or equal to 7.0 MPa·millimeter.

### Claim 10 (depends on 9)

The glass article of claim 9 including one or more of the following:
the compressive stress integral at a depth of 12 micrometers is greater than or equal to 10.9 MPa·millimeter;
the compressive stress integral at a depth of 16 micrometers is greater than or equal to 13.1 MPa·millimeter;
the compressive stress integral at a depth of 20 micrometers is greater than or equal to 14.1 MPa·millimeter; and
the compressive stress integral at a depth of 25 micrometers is greater than or equal to 14.9 MPa·millimeter.

### Claim 11 (depends on 9)

The glass article of claim 9 comprising a 3D configuration.

### Claim 12 (depends on 9)

The glass article of claim 9, wherein the peak compressive stress (CSmax) of the spike region is greater than or equal to 1100 MPa or 1150 MPa.

### Claim 13 (depends on 9)

The glass article of claim 9 comprising an alkali aluminosilicate central composition.

### Claim 14 (depends on 13)

The glass article of claim 13, wherein the alkali aluminosilicate central composition has a Young's modulus that is greater than or equal to 76 GPa or greater than or equal to 80 GPa; and/or a facture toughness of greater than or equal to 0.78; and/or a Na2O/Li2O molar ratio in a range of greater than or equal to 1.5 to less than or equal to 2.1.

### Claim 15 (depends on 13)

The glass article of claim 13, wherein the alkali aluminosilicate central composition comprises:
about 50 mol % to about 69 mol % SiO2;
about 12.5 mol % to about 25 mol % Al2O3;
about 0 mol % to about 8 mol % B2O3;
about 11.0 mol % to about 19.0 mol % Na2O; and
about 0.5 mol % to about 10 mol % Li2O.

### Claim 16 (depends on 9)

The glass article of claim 9 comprising the compressive stress integral at a depth of 30 micrometers of greater than or equal to 16 MPa·millimeter, or 17 MPa millimeter.

### Claim 17 (depends on 9)

The glass article of claim 9, wherein the DOC is greater than or equal to 20 and optionally is less than 30 micrometers.

### Claim 18 (depends on 9)

The glass article of claim 9, wherein the DOC is greater than or equal to 30 micrometers.

### Claim 19 (depends on 1)

A consumer electronic product comprising:
a housing having a front surface, a back surface, and side surfaces;
electrical components provided at least partially within the housing, the electrical components including at least a controller, a memory, and a display, the display being provided at or adjacent the front surface of the housing; and
the glass article of claim 1 disposed over the display.