# US 2026/0062339 A1 · Glass, method for producing glass, member for semiconductor production apparatus, and semiconductor production apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0062339 A1
- Document ID: US20260062339A1
- Status: Published application
- Kind: A1
- Application number: 19/307,146
- Filed: 2025-08-22
- Published: 2026-03-05
- Earliest claimed: 2024-08-28
- Assignees: AGC Inc.
- Applicants: AGC Inc.
- Inventors: Kazuki KANEHARA; Tomonori OGAWA
- Web page: https://patentgrep.com/patent/US20260062339A1

## CPC

- C03C 3/085: containing an oxide of a divalent metal
- C03C 3/078: containing an oxide of a divalent metal, e.g. an oxide of zinc
- C03C 3/089: containing boron
- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 4/20: for chemical resistant glass
- H01J 37/32477: {characterised by the means for protecting vessels or internal parts, e.g. coatings}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

A glass including: silicon; magnesium; strontium; and barium, in which the glass has, in mol % based on oxides, a content of SiO2 of 48.0 mol % or more, a content of Al2O3 of 20.0 mol % or less, a content of MgO of 0.1 mol % or more, a content of SrO of 0.1 mol % or more, a content of BaO of 0.1 mol % or more, and a content of R2O of 22.0 mol % or more, provided that R2 indicates an alkaline earth metal element, and the glass is substantially free of CaO, substantially free of TiO2, and substantially free of R12O, provided that R1 indicates an alkali metal element.

## Claims

### Claim 1

A glass comprising:
silicon;
magnesium;
strontium; and
barium, wherein
the glass has, in mol % based on oxides, a content of SiO2 of 48.0 mol % or more, a content of Al2O3 of 20.0 mol % or less, a content of MgO of 0.1 mol % or more, a content of SrO of 0.1 mol % or more, a content of BaO of 0.1 mol % or more, and a content of R2O of 22.0 mol % or more, provided that R2 indicates an alkaline earth metal element, and
the glass is substantially free of CaO, substantially free of TiO2, and substantially free of R12O, provided that R1 indicates an alkali metal element.

### Claim 2 (depends on 1)

The glass according to claim 1, wherein the content of Al2O3 is 13.5 mol % or less.

### Claim 3 (depends on 1)

The glass according to claim 1, which is substantially free of Al2O3.

### Claim 4 (depends on 1)

The glass according to claim 1, wherein the content of BaO is 4.0 mol % to 14.0 mol %.

### Claim 5 (depends on 1)

The glass according to claim 1, wherein
the content of Al2O3 is 13.5 mol % or less, and
the content of BaO is 4.0 mol % to 14.0 mol %.

### Claim 6 (depends on 1)

The glass according to claim 1, which is a glass block.

### Claim 7 (depends on 1)

The glass according to claim 1, which is a disk-shaped glass block.

### Claim 8 (depends on 1)

The glass according to claim 1, which is an annular glass block.

### Claim 9 (depends on 1)

The glass according to claim 1, which is for use as a member for a semiconductor production apparatus to be mounted on a semiconductor production apparatus.

### Claim 10 (depends on 9)

The glass according to claim 9, wherein the member for a semiconductor production apparatus is an edge ring, a shield ring, a focus ring, a shower plate, an electrostatic chuck, a susceptor, an injector, an inspection window, a top plate, or a side wall to be mounted on the semiconductor production apparatus.

### Claim 11 (depends on 1)

A method for producing the glass according to claim 1, the method comprising:
melting a glass raw material by heating at a melting temperature of 1,400° C. to 1,800° C.; and
cooling the obtained molten glass to a cooling stop temperature of 500° C. to 700° C. at a cooling rate of 100° C./min to 1,500° C./min.

### Claim 12 (depends on 1)

A member for a semiconductor production apparatus comprising:
the glass according to claim 1.

### Claim 13 (depends on 12)

The member for a semiconductor production apparatus according to claim 12, which is an edge ring, a shield ring, a focus ring, a shower plate, an electrostatic chuck, a susceptor, an injector, an inspection window, a top plate, or a side wall to be mounted on a semiconductor production apparatus.

### Claim 14 (depends on 12)

A semiconductor production apparatus comprising:
the member for a semiconductor production apparatus according to claim 12.

### Claim 15 (depends on 13)

A semiconductor production apparatus comprising:
the member for a semiconductor production apparatus according to claim 13.