# US 2026/0062313 A1 · Nickel-containing hydroxide, cathode active material with nickel-containing hydroxide as precursor, and method for producing nickel-containing hydroxide

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0062313 A1
- Document ID: US20260062313A1
- Status: Published application
- Kind: A1
- Application number: 19/311,803
- Filed: 2025-08-27
- Published: 2026-03-05
- Earliest claimed: 2024-08-28
- Assignees: Tanaka Chemical Corporation
- Applicants: Tanaka Chemical Corporation
- Inventors: Yudai YASUNO
- Web page: https://patentgrep.com/patent/US20260062313A1

## CPC

- C01G 53/05: Hydroxides; Oxyhydroxides
- C01G 53/50: of the type (MnO2)n-, e.g. Li(NixMn1-x)O2 or Li(MyNixMn1-x-y)O2
- C01G 53/82: Compounds containing nickel, with or without oxygen or hydrogen, and containing two or more other elements
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2006/12: Surface area
- C01P 2006/40: Electric properties
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided is a nickel-containing hydroxide as a precursor of a cathode active material for a non-aqueous electrolyte secondary battery, wherein the nickel-containing hydroxide is secondary particles formed by agglomeration of a plurality of primary particles, and the primary particles have an average area of 0.035 μm2 or more.

## Claims

### Claim 1

A nickel-containing hydroxide as a precursor of a cathode active material for a non-aqueous electrolyte secondary battery, wherein the nickel-containing hydroxide is secondary particles formed by agglomeration of a plurality of primary particles, and the primary particles have an average area of 0.035 μm2 or more.

### Claim 2 (depends on 1)

The nickel-containing hydroxide according to claim 1, wherein the primary particles have an average area of 0.100 μm2 or less.

### Claim 3 (depends on 1)

The nickel-containing hydroxide according to claim 1, wherein the primary particles have an average area of 0.039 μm2 or more and 0.080 μm2 or less.

### Claim 4 (depends on 1)

The nickel-containing hydroxide according to claim 1, wherein the nickel-containing hydroxide comprises 80 mol % or more of nickel (Ni) relative to a total amount of metals in the nickel-containing hydroxide.

### Claim 5 (depends on 4)

The nickel-containing hydroxide according to claim 4, wherein the nickel-containing hydroxide is a composite hydroxide comprising nickel (Ni) and at least one metal selected from the group consisting of cobalt (Co) and manganese (Mn).

### Claim 6 (depends on 4)

The nickel-containing hydroxide according to claim 4, wherein the nickel-containing hydroxide is a composite hydroxide in which a molar ratio among nickel (Ni): cobalt (Co): manganese (Mn): an additive element M is represented by (1-x-y-z):x:y:z (0≤x≤0.15, 0≤y≤0.15, 0≤z≤0.05, and M is one or more additive elements selected from the group consisting of Al, Fe, Ti, Mg, Ca, Sr, Ba, V, Nb, Cr, Mo, W, Ru, Cu, Zn, B, Ga, Si, Sn, P, Bi, and Zr).

### Claim 7 (depends on 1)

A cathode active material for a non-aqueous electrolyte secondary battery, wherein the cathode active material is formed by calcining the nickel-containing hydroxide according to claim 1 with a lithium compound.

### Claim 8

A method for producing a nickel-containing hydroxide as a precursor of a cathode active material for a non-aqueous electrolyte secondary battery, wherein the nickel-containing hydroxide is secondary particles formed by agglomeration of a plurality of primary particles, the method comprising:
obtaining the nickel-containing hydroxide by a crystallization reaction by continuously supplying a metal-containing aqueous solution containing nickel, a complexing agent, and an alkaline aqueous solution to a reaction tank, and
continuously extracting a slurry containing the nickel-containing hydroxide from the reaction tank,
wherein a flow rate of the metal-containing aqueous solution containing nickel supplied to the reaction tank is 0.25 m/s or less.

### Claim 9 (depends on 8)

The method for producing a nickel-containing hydroxide according to claim 8, wherein the flow rate of the metal-containing aqueous solution containing nickel supplied to the reaction tank is 0.01 m/s or more.

### Claim 10 (depends on 8)

The method for producing a nickel-containing hydroxide according to claim 8, wherein the nickel-containing hydroxide extracted from the reaction tank is washed with an alkaline aqueous solution and is then subjected to solid-liquid separation.