# US 2026/0061513 A1 · Composite material, its preparation and use

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0061513 A1
- Document ID: US20260061513A1
- Status: Published application
- Kind: A1
- Application number: 19/274,917
- Filed: 2025-07-21
- Published: 2026-03-05
- Earliest claimed: 2024-08-28
- Assignees: City University of Hong Kong
- Applicants: City University of Hong Kong
- Inventors: Yong Yang; Yun Teng; Wenqing ZHU; Hao Gong
- Web page: https://patentgrep.com/patent/US20260061513A1

## CPC

- B23K 20/023: {Thermo-compression bonding}
- C22F 1/08: of copper or alloys based thereon
- B23K 2103/12: Copper or alloys thereof
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

A composite material for bonding copper to copper includes a copper-based heterogeneous nanostructure, wherein the copper-based heterogeneous nanostructure includes a nanocrystalline copper and dispersions of copper oxide. Also addressed are the method of preparing and use of the composite material.

## Claims

### Claim 1

A composite material for bonding copper to copper comprising a copper-based heterogeneous nanostructure, wherein the copper-based heterogeneous nanostructure comprises a nanocrystalline copper and dispersions of copper oxide.

### Claim 2 (depends on 1)

The composite material as claimed in claim 1, wherein the nanocrystalline copper is interspersed with the dispersions of copper oxide.

### Claim 3 (depends on 1)

The composite material as claimed in claim 1, wherein the nanocrystalline copper and the dispersions of copper oxide have a volume ratio of about 8:2.

### Claim 4 (depends on 1)

The composite material as claimed in claim 1, wherein the nanocrystalline copper and the dispersions of copper oxide have an atomic percentage ratio of about 90%:10%.

### Claim 5 (depends on 1)

The composite material as claimed in claim 1, wherein the heterogeneous nanostructure has an average grain size of about 16 nm.

### Claim 6 (depends on 1)

The composite material as claimed in claim 1, wherein the heterogeneous nanostructure includes at least one type of material defect of crystallography derived from lattice structures of the nanocrystalline copper and the dispersions of copper oxide.

### Claim 7 (depends on 6)

The composite material as claimed in claim 6, wherein the at least one type of material defect of crystallography comprises twin boundary and stacking faults.

### Claim 8 (depends on 6)

The composite material as claimed in claim 6, wherein the nanocrystalline copper has a lattice structure of hexagonal close packing symmetry.

### Claim 9 (depends on 6)

The composite material as claimed in claim 6, wherein the dispersions of copper oxide are dispersions of copper (I) oxide having a mixed lattice structure of body-centered cubic symmetry and face-centered cubic symmetry.

### Claim 10 (depends on 1)

The composite material as claimed in claim 1 is in form of a membrane.

### Claim 11 (depends on 10)

The composite material as claimed in claim 10, wherein the membrane has a thickness ranging from about 35 nm to about 50 nm.

### Claim 12 (depends on 10)

The composite material as claimed in claim 10, wherein the membrane has a lateral size of ≥1 cm.

### Claim 13 (depends on 10)

The composite material as claimed in claim 10 having at least one of the following mechanical characteristics: a yield strength of about 850 MPa to about 1050 MPa; a ductility of about 37% to about 43%; an elastic modulus of about 32 GPa to about 38 GPa; and an elastic strain limit of about 2.4% to about 3.0%.

### Claim 14 (depends on 1)

The composite material as claimed in claim 1 is adapted to be disposed between a first and a second copper surfaces for bonding under a condition of a temperature of about 200° C. to about 300° C., a pressure of 10 MPa and in a vacuum of 2×10−2 Pa, for about 3 min to about 300 min.

### Claim 15 (depends on 14)

The composite material as claimed in claim 14, wherein at least one of the first and the second copper surfaces is a patterned copper surface.

### Claim 16 (depends on 14)

The composite material as claimed in claim 14 bonds the first and the second copper surfaces with an internal shear strength, wherein the internal shear strength is up to about 73 MPa at room temperature.

### Claim 17 (depends on 16)

The composite material as claimed in claim 16, wherein the internal shear strength is about 35 times greater than that of a copper-copper bond without the composite material.

### Claim 18 (depends on 1)

A method of preparing the composite material as claimed in claim 1 comprising the steps of:
(a) depositing a layer of Cu onto a water-absorbing substrate by ion beam sputtering or electron beam evaporation;
(b) immersing the deposited water absorbing substrate of (a) into water for absorption for a predetermined of time;
(c) separating the composite material from the deposited water-absorbing substrate.

### Claim 19 (depends on 18)

The method as claimed in claim 18, wherein the water-absorbing substrate in step (a) comprises a composite substrate in dehydrated form.

### Claim 20 (depends on 19)

The method as claimed in claim 19, wherein the composite substrate in dehydrated form is prepared by the step of spin-coating a layer of hydrogel onto a base substrate, followed by dehydrating the spin-coated layer of hydrogel.

### Claim 21 (depends on 20)

The method as claimed in claim 20, wherein the layer of hydrogel comprises poly(vinyl alcohol) (PVA).

### Claim 22 (depends on 20)

The method as claimed in claim 20, wherein the base substrate comprises glass or polyimide (PI).

### Claim 23 (depends on 20)

The method as claimed in claim 20, wherein the step of spin-coating of the layer of hydrogel comprises spin-coating a PVA solution onto a glass plate to form a PVA-glass composite substrate.

### Claim 24 (depends on 23)

The method as claimed in claim 23, wherein the spin-coating is carried out at about 1000 to about 3000 rpm for about 30 to about 300 seconds.

### Claim 25 (depends on 23)

The method as claimed in claim 23, wherein the PVA solution has a concentration of about 8 wt. % to about 11 wt. %.

### Claim 26 (depends on 23)

The method as claimed in claim 23, wherein the PVA-glass composite substrate is dehydrated at about 60° C. to about 90° C. for about 1 to about 24 hours.

### Claim 27 (depends on 18)

The method as claimed in claim 18, wherein the electron beam evaporation is carried out under a pressure of less than 6×10−4 Pa at a nominal deposition rate of about 1 Å/s.

### Claim 28 (depends on 18)

The method as claimed in claim 18, wherein the ion beam sputtering is carried out under a stable deposition rate.

### Claim 29 (depends on 18)

The method as claimed in claim 18, wherein the deposited water-absorbing substrate of (a) is immersed into water for about 120 seconds to about 600 seconds.

### Claim 30 (depends on 1)

A method of fabricating a joined body comprising the step of:
(a) disposing one or more layer of the composite material as claimed in claim 1 between a first copper surface and a second copper surface, to form a pre-joined body;
(b) annealing the pre-joined body in step (a) for bonding the first and the second copper surfaces through the one or more layer of the composite material;
wherein the first and the second copper surfaces in step (a) are non-planarized surfaces.

### Claim 31 (depends on 30)

The method as claimed in claim 30 further comprising the step of applying a pressure of about 10 N to about 100 N to the pre-joined body in step (a) to facilitate contact of the first copper surface, the composite material and the second copper surface.

### Claim 32 (depends on 30)

The method as claimed in claim 30, wherein step (b) is carried out under a condition of a temperature of about 200° C. to about 300° C., a pressure of 10 MPa and in a vacuum of 2×10−2 Pa, for about 3 min to about 300 min.

### Claim 33 (depends on 30)

The method as claimed in claim 30, wherein at least one of the first and the second copper surfaces is a layer of copper deposited on a base substrate comprising Si wafer.

### Claim 34 (depends on 33)

The method as claimed in claim 33, wherein the layer of copper partially covers the base substrate.

### Claim 35 (depends on 33)

The method as claimed in claim 33, wherein the layer of copper fully covers the base substrate.

### Claim 36 (depends on 30)

The method as claimed in claim 30, wherein each of the first and the second copper surfaces is a layer of copper deposited on a base substrate comprising Si wafer.

### Claim 37 (depends on 33)

The method as claimed in claim 33, wherein the layer of copper is deposited on the based substrate by magnetron sputtering.