# US 2026/0061410 A1 · Method for making a benzimidazole

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0061410 A1
- Document ID: US20260061410A1
- Status: Published application
- Kind: A1
- Application number: 19/383,003
- Filed: 2025-11-07
- Published: 2026-03-05
- Earliest claimed: 2023-06-02
- Assignees: King Fahd University of Petroleum and Minerals
- Applicants: King Fahd University of Petroleum and Minerals
- Inventors: Aasif HELAL; Mohammed Ahmed SANHOOB
- Web page: https://patentgrep.com/patent/US20260061410A1

## CPC

- B01J 35/393: {Metal or metal oxide crystallite size}
- B01J 21/18: Carbon
- B01J 23/75: Cobalt
- B01J 23/755: Nickel
- B01J 35/23: in a colloidal state
- B01J 35/394: {Metal dispersion value, e.g. percentage or fraction}
- B01J 35/615: {100-500 m2/g}
- B01J 37/0236: {Drying, e.g. preparing a suspension, adding a soluble salt and drying}
- B01J 37/031: {Precipitation}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/086: {Decomposition of an organometallic compound, a metal complex or a metal salt of a carboxylic acid}
- B01J 37/16: Reducing
- C07C 1/12: from carbon dioxide with hydrogen
- C07D 235/08: Radicals containing only hydrogen and carbon atoms
- C07C 2521/18: Carbon
- C07C 2523/75: Cobalt
- C07C 2523/755: Nickel
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- C07D: HETEROCYCLIC COMPOUNDS (macromolecular compounds C08)

## Abstract

A method of making a bimetallic nanoalloy composite includes mixing and dissolving a nickel salt, a cobalt salt, and an aromatic carboxylic acid in a first solvent to form a first mixture; mixing acetic acid with the first mixture and heating at a temperature of 150 to 200 degrees Celsius (° C.) form a second mixture; washing the second mixture with at least one organic solvent and drying to form a bimetallic metal-organic framework (CoNiBTC); heating the CoNiBTC at a temperature of 600 to 900° C. under a nitrogen stream to form a pyrolyzed composite; and cooling the pyrolyzed composite and exposing to a gas mixture to form the bimetallic nanoalloy composite. A method of making a benzimidazole compound. A method of making methane from CO2.

## Claims

### Claim 1

(canceled)

### Claim 2 (depends on 13)

The method of claim 13, wherein the cobalt nanoparticles are present in the bimetallic nanoalloy composite at a concentration of 20 to 50% by weight based on the total weight of the bimetallic nanoalloy composite.

### Claim 3 (depends on 13)

The method of claim 13, wherein the nickel nanoparticles are present in the bimetallic nanoalloy composite at a concentration of 10 to 30% by weight based on the total weight of the bimetallic nanoalloy composite.

### Claim 4 (depends on 13)

The method of claim 13, wherein the bimetallic nanoalloy composite is in the form of particles having a surface area of 150 to 210 square meters per gram (m2/g).

### Claim 5 (depends on 13)

The method of claim 13, wherein the lattice structure of the bimetallic nanoalloy composite has an average interplanar spacing of 0.05 to 0.5 nm.

### Claim 6 (depends on 13)

The method of claim 13, wherein the nickel salt comprises nickel sulfate, nickel acetate, nickel chloride, nickel nitrate, nickel carbonate, nickel phosphate and nickel oxalate, and/or a hydrate thereof.

### Claim 7 (depends on 13)

The method of claim 13, wherein the cobalt salt comprises cobalt sulfate, cobalt acetate, cobalt citrate, cobalt iodide, cobalt chloride, cobalt perchlorate, cobalt nitrate, cobalt phosphate, cobalt triflate, cobalt bis(trifluoromethanesulfonyl)imide, cobalt tetrafluoroborate, cobalt bromide, and/or a hydrate thereof.

### Claim 8 (depends on 13)

The method of claim 13, wherein the aromatic carboxylic acid comprises at least one of trimesic acid, trimellitic acid, trimellitic anhydride, and pyromellitic acid anhydride.

### Claim 9 (depends on 13)

The method of claim 13, wherein the solvent is an amide solvent selected from the group consisting of N-methyl-2-pyrrolidone, N,N-dimethylacetamide, N,N-dimethylformamide, and 1,3-dimethyl-2-imidazolidinone.

### Claim 10 (depends on 13)

The method of claim 13, wherein a molar ratio of the nickel salt to the cobalt salt is in a range of 1:10 to 10:1, and wherein a molar ratio of the aromatic carboxylic acid to the combined amount of nickel and cobalt salt in the first mixture is in a range of 1:5 to 5:1.

### Claim 11 (depends on 13)

The method of claim 13, wherein the bimetallic metal-organic framework (CoNiBTC) is in the form of particles having a surface area of 650 to 750 m2/g.

### Claim 12 (depends on 13)

The method of claim 13, wherein the gas mixture comprises an oxygen gas and a nitrogen gas, and wherein a flow rate ratio of the oxygen gas to the nitrogen gas is in a range of 1:1 to 1:10.

### Claim 13

A method of making a benzimidazole compound, comprising:
contacting a phenylenediamine compound with a bimetallic nanoalloy composite in the presence of CO2 and H2, and heating under a pressure of 20 to 40 bar to form the benzimidazole compound having a structure of formula (I)
wherein R is selected from the group consisting of hydrogen, an optionally substituted alkyl, an optionally substituted cycloalkyl, an optionally substituted alkoxy, a hydroxyl group, a halogen group, a nitro group, and a cyano group;
wherein the bimetallic nanoalloy composite is prepared by:
mixing and dissolving a nickel salt, a cobalt salt and an aromatic carboxylic acid in a first solvent to form a first mixture;
mixing acetic acid with the first mixture and heating at a temperature of 150 to 200 degrees Celsius (° C.) form a second mixture;
washing the second mixture with at least one organic solvent and drying to form a bimetallic metal-organic framework (CoNiBTC);
heating the CoNiBTC at a temperature of 600 to 900° C. under a nitrogen stream to form a pyrolyzed composite;
cooling the pyrolyzed composite and exposing to a gas mixture to form the bimetallic nanoalloy composite, wherein the bimetallic nanoalloy composite is in the form of bimetallic nanoalloy composite particles comprising cobalt nanoparticles, nickel nanoparticles and porous carbon layers;
wherein the cobalt nanoparticles present in the bimetallic nanoalloy composite have an average particle size of 5 to 50 nanometers (nm);
wherein the nickel nanoparticles present in the bimetallic nanoalloy composite have an average particle size of 5 to 50 nm; and
wherein the nanoparticles of cobalt and nickel are embedded in the porous carbon layers of the bimetallic nanoalloy composite, and are uniformly distributed throughout the bimetallic nanoalloy composite.

### Claim 14 (depends on 13)

The method of claim 13, wherein the heating is performed at a temperature in a range of 30 to 150° C.

### Claim 15 (depends on 13)

The method of claim 13, wherein the bimetallic nanoalloy composite has a concentration of 50 to 200 milligrams per millimole (mg/mmol) based on a total molar amount of the phenylenediamine compound.

### Claim 16 (depends on 13)

The method of claim 13, wherein the benzimidazole compound is at least one selected from the group consisting of benzimidazole, 5-chloro-benzoimidazole, 5-methyl-benzoimidazole, and 5-nitro-benzoimidazole.

### Claim at position 17

17-20. (canceled)