# US 2026/0055251 A1 · Method for preparing hydrophobic melamine resin foam, and its products and applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0055251 A1
- Document ID: US20260055251A1
- Status: Published application
- Kind: A1
- Application number: 18/813,039
- Filed: 2024-08-23
- Published: 2026-02-26
- Earliest claimed: 2024-08-23
- Assignees: FoamTech (Zhejiang) New Materials Co., Ltd
- Applicants: FoamTech (Zhejiang) New Materials Co., Ltd
- Inventors: Yangyang Li; Xuezi Fan
- Web page: https://patentgrep.com/patent/US20260055251A1

## CPC

- C08J 9/42: with macromolecular compounds
- B01J 20/262: {obtained otherwise than by reactions only involving carbon to carbon unsaturated bonds, e.g. obtained by polycondensation (macromolecular compounds obtained otherwise than by reactions only involving unsaturated carbon-to-carbon bonds per se C08G)}
- B01J 20/267: {Cross-linked polymers}
- B01J 20/28045: {Honeycomb or cellular structures; Solid foams or sponges}
- B01J 20/3071: {Washing or leaching}
- B01J 20/3078: {Thermal treatment, e.g. calcining or pyrolizing}
- B01J 20/3212: {consisting of a polymer obtained by reactions otherwise than involving only carbon to carbon unsaturated bonds}
- B01J 20/3221: {the chemical bond being an ionic interaction}
- B01J 20/3236: {containing metal, other than zeolites, e.g. oxides, hydroxides, sulphides or salts}
- B01J 20/3272: {Polymers obtained by reactions otherwise than involving only carbon to carbon unsaturated bonds}
- B01J 20/3282: {Crosslinked polymers}
- B01J 20/3285: {Coating or impregnation layers comprising different type of functional groups or interactions, e.g. different ligands in various parts of the sorbent, mixed mode, dual zone, bimodal, multimodal, ionic or hydrophobic, cationic or anionic, hydrophilic or hydrophobic}
- C02F 1/288: {using composite sorbents, e.g. coated, impregnated, multi-layered}
- C08G 73/0644: {Poly(1,3,5)triazines}
- C02F 1/285: {using synthetic organic sorbents}
- C02F 2101/32: Hydrocarbons, e.g. oil
- C08J 2379/04: Polycondensates having nitrogen-containing heterocyclic rings in the main chain; Polyhydrazides; Polyamide acids or similar polyimide precursors
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

The invention relates to the field of functional materials technology, specifically to a preparation method, product, and application of hydrophobic melamine resin foam. The preparation method of hydrophobic melamine resin foam includes the following steps: Vacuum-impregnate the melamine resin foam with a solution of poly(dimethyl diallyl ammonium chloride). Subsequently, immerse the cationic-coated melamine resin foam in a sodium polyacrylate solution. Next, immerse the anionic-coated melamine resin foam in a titanium dioxide mixed solution for cross-linking. After cross-linking, immerse the melamine resin foam in a solution of tridecafluoro-octyl triethoxysilane. After impregnation, dry the foam to obtain hydrophobic melamine resin foam. The preparation method of the invention is simple, cost-effective, and easy to scale up for industrial applications. The hydrophobic melamine resin foam prepared using this method can achieve a hydrophobic contact angle of up to 150° and exhibits excellent oil absorption performance.

## Claims

### Claim 1

A method for preparing hydrophobic melamine resin foam, comprising the following steps: step 1: vacuum-impregnate melamine resin foam in a solution of poly(dimethyl diallyl ammonium chloride) to obtain melamine resin foam coated with a cationic membrane; step 2: immerse the cationic-coated melamine resin foam in a solution of sodium polyacrylate to obtain melamine resin foam coated with an anionic membrane; step 3: immerse the anionic-coated melamine resin foam in a titanium dioxide mixed solution for cross-linking to obtain cross-linked melamine resin foam; step 4: immerse the cross-linked melamine resin foam in a solution of tridecafluoro-octyl triethoxysilane, then dry the foam after impregnation to obtain the hydrophobic melamine resin foam.

### Claim 2 (depends on 1)

The preparation method of hydrophobic melamine resin foam, as claimed in claim 1, wherein in step 1, the poly(dimethyl diallyl ammonium chloride) solution has a concentration of 5 mol/L; the vacuum impregnation time is 8-10 minutes; and the process further includes a washing step after vacuum impregnation.

### Claim 3 (depends on 1)

The preparation method of hydrophobic melamine resin foam as claimed in claim 1, wherein in step 2, the sodium polyacrylate solution has a concentration of 5 mol/L; the impregnation time is 8-10 minutes at atmospheric pressure; and the process further includes a washing step after impregnation.

### Claim 4 (depends on 1)

The preparation method of hydrophobic melamine resin foam as claimed in claim 1, wherein in step 3, the titanium dioxide mixed solution is a mixed aqueous solution of nano-titanium dioxide and sodium carboxymethyl cellulose; the concentration of nano-titanium dioxide in the mixed solution is 2-4 mg/mL; and the concentration of sodium carboxymethyl cellulose in the mixed solution is 3-7 mg/mL.

### Claim 5 (depends on 1)

The preparation method of hydrophobic melamine resin foam as claimed in claim 1, wherein in step 3, the cross-linking temperature is 20-30° ;. the cross-linking time is 1 hour; and the process further includes a washing step after cross-linking.

### Claim 6 (depends on 1)

The preparation method of hydrophobic melamine resin foam as claimed in claim 1, wherein in step 4, the tridecafluoro-octyl triethoxysilane solution is prepared by adding tridecafluoro-octyl triethoxysilane to ethanol; the mass concentration of the tridecafluoro-octyl triethoxysilane solution is 5%-10%; the impregnation time of the cross-linked melamine resin foam in the tridecafluoro-octyl triethoxysilane solution is 8-10 minutes; and the process further includes a drying step at 40-60° C. for 6-8 hours after impregnation.

### Claim 7 (depends on 1)

A hydrophobic melamine resin foam obtained by the preparation method of claim 1.

### Claim 8 (depends on 7)

An application of the hydrophobic melamine resin foam in treating oil-containing wastewater as claimed in claim 7.