# US 2026/0054352 A1 · Cutting Disk With Diamonds In Metal Sinter Matrix

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0054352 A1
- Document ID: US20260054352A1
- Status: Published application
- Kind: A1
- Application number: 19/103,621
- Filed: 2023-01-31
- Published: 2026-02-26
- Earliest claimed: 2022-08-16
- Applicants: Klingspor AG
- Inventors: Stefan Neubach; Oleksandr Filatov
- Web page: https://patentgrep.com/patent/US20260054352A1

## CPC

- B24D 3/06: metallic {or mixture of metals with ceramic materials, e.g. hard metals, "cermets", cements}
- B28D 1/121: {Circular saw blades}
- B24D 5/123: {having different cutting segments}
- C04B 35/117: Composites
- B24D: TOOLS FOR GRINDING, BUFFING OR SHARPENING (abrading-bodies specially designed for tumbling apparatus, e.g. abrading-balls B24B31/14; honing tools B24B33/08; lapping tools B24B37/11)
- B28D: WORKING STONE OR STONE-LIKE MATERIALS
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

A cutting wheel includes a core wheel made of a metallic material and cutting segments disposed at the circumference of the core wheel and each having a sintered metal matrix in which diamonds are embedded. Additionally, aluminum oxide particles are embedded in the sintered metal matrix of each of the cutting segments. The aluminum oxide particles are shaped in such a manner that they each have a surface area/volume (A/V) ratio greater than 5.

## Claims

### Claim 1

A cutting wheel comprising a core wheel made of a metallic material and cutting segments disposed at the circumference of the core wheel and each having a sintered metal matrix in which diamonds are embedded, aluminum oxide particles being embedded in the sintered metal matrix of each of the cutting segments, wherein the aluminum oxide particles are shaped in such a manner that they each have a surface area/volume (A/V) ratio greater than 5.

### Claim 2 (depends on 1)

The cutting wheel according to claim 1, wherein the aluminum oxide particles are each rod-shaped.

### Claim 3 (depends on 1)

The cutting wheel according to claim 1, wherein the content of the aluminum oxide particles in the sintered metal matrix is 1 to 30 wt. %.

### Claim 4 (depends on 1)

The cutting wheel according to claim 1, wherein the aluminum oxide particles are made of sintered corundum.

### Claim 5 (depends on 1)

The cutting wheel according to claim 1, wherein the sintered metal matrix comprises 8 to 75 wt. % iron, nickel, tin and/or cobalt.

### Claim 6 (depends on 1)

The cutting wheel according to claim 1, wherein the sintered metal matrix comprises 5 to 40 wt. % copper and/or copper-based alloy.

### Claim 7 (depends on 1)

The cutting wheel according to claim 1, wherein the sintered metal matrix comprises 0.1 to 40 wt. % hard materials and/or hard-material alloy.

### Claim 8 (depends on 1)

The cutting wheel according to claim 1, wherein the sintered metal matrix comprises 0.5 to 15 wt. % iron phosphide.

### Claim 9 (depends on 1)

The cutting wheel according to claim 1, wherein the aluminum oxide particles are disposed regularly and/or in patterns in the sintered metal matrix.