# US 2026/0048387 A1 · Hydrocracking catalyst comprising hierarchical zeolite y and mesoporous nano-sized zeolite beta composite

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0048387 A1
- Document ID: US20260048387A1
- Status: Published application
- Kind: A1
- Application number: 18/804,970
- Filed: 2024-08-14
- Published: 2026-02-19
- Earliest claimed: 2024-08-14
- Assignees: Saudi Arabian Oil Company
- Applicants: Saudi Arabian Oil Company
- Inventors: Lianhui Ding; Faisal Alotaibi; Mazin Tamimi; Mohammad Aljishi; Batool Altaher; Eman Albaher
- Web page: https://patentgrep.com/patent/US20260048387A1

## CPC

- B01J 29/80: Mixtures of different zeolites
- C10G 47/02: characterised by the catalyst used
- B01J 21/04: Alumina
- B01J 29/084: {Y-type faujasite}
- B01J 29/146: {Y-type faujasite}
- B01J 29/166: {Y-type faujasite}
- B01J 29/7615: {Zeolite Beta}
- B01J 29/7815: {Zeolite Beta}
- B01J 35/615: {100-500 m2/g}
- B01J 35/633: {less than 0.5 ml/g}
- B01J 35/635: {0.5-1.0 ml/g}
- B01J 35/647: {2-50 nm}
- B01J 37/0018: {Addition of a binding agent or of material, later completely removed among others as result of heat treatment, leaching or washing,(e.g. forming of pores; protective layer, desintegrating by heat)}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/06: Washing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C10G 11/05: Crystalline alumino-silicates, e.g. molecular sieves
- C10G 47/16: Crystalline alumino-silicate carriers
- C10G 47/20: the catalyst containing other metals or compounds thereof
- B01J 2029/062: {Mixtures of different aluminosilicates}
- B01J 2229/20: to introduce other elements in the catalyst composition comprising the molecular sieve, but not specially in or on the molecular sieve itself
- B01J 2229/42: Addition of matrix or binder particles
- C10G 2400/20: C2-C4 olefins
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES

## Abstract

A catalyst comprising a zeolite beta and a hierarchical zeolite Y. The zeolite beta comprises a plurality of micropores having a pore size of less than 2 nm and a plurality of mesopores having a pores size of greater than or equal to 2 nm to less than or equal to 50 nm. A volume of mesopores is greater than or equal to 35% of a total pore volume of the zeolite beta and an average particle size of the zeolite beta is less than or equal to 100 nm.

## Claims

### Claim 1

A catalyst, the catalyst comprising:
zeolite beta; and
hierarchical zeolite Y;
wherein:
the zeolite beta comprises a plurality of micropores having a pore size of less than 2 nm and a plurality of mesopores having a pore size of greater than or equal to 2 nm to less than or equal to 50 nm;
a volume of mesopores is greater than or equal to 35% of a total pore volume of the zeolite beta; and
an average particle size of the zeolite beta is less than or equal to 100 nm.

### Claim 2 (depends on 1)

The catalyst of claim 1, wherein a weight ratio of the zeolite beta and the hierarchical zeolite Y is from 0.2 to 5.

### Claim 3 (depends on 1)

The catalyst of claim 1, wherein the catalyst further comprises a support material.

### Claim 4 (depends on 1)

The catalyst of claim 1, wherein:
The catalyst comprises one or more metals, one or more metal oxides, or combinations thereof, chosen from tungsten atoms, molybdenum atoms, nickel atoms, tungsten oxide, molybdenum oxide, nickel oxide, or combinations thereof.

### Claim 5 (depends on 1)

The catalyst of claim 1, wherein the catalyst comprises:
from 2 wt. % to 50 wt. % of the zeolite beta;
from 2 wt. % to 50 wt. % of the hierarchical zeolite Y;
from 4 wt. % to 6 wt. % NiO; and
from 20 wt. % to 80 wt. % Al2O3.

### Claim 6 (depends on 1)

The catalyst of claim 1, wherein the catalyst comprises:
from 10 wt. % to 60 wt. % of the zeolite beta and the hierarchical zeolite Y;
from 4 wt. % to 6 wt. % NiO; and
from 20 wt. % to 80 wt. % Al2O3.

### Claim 7 (depends on 1)

The catalyst of claim 1, wherein the catalyst comprises 20 wt. % to 26 wt. % WO3.

### Claim 8 (depends on 1)

The catalyst of claim 1, wherein the catalyst comprises 14 wt. % to 16 wt. % MoO3.

### Claim 9 (depends on 1)

The catalyst of claim 1, wherein the hierarchical zeolite Y has an average silica to alumina molar ratio of less than or equal to 80.

### Claim 10

A method of making a catalyst comprising:
forming a composite comprising hierarchical zeolite Y and zeolite beta;
extruding the composite to form a plurality of extrudates; and
heating the extrudates;
wherein:
the zeolite beta comprises a plurality of micropores having a pore size of less than 2 nm and a plurality of mesopores having a pore size of greater than or equal to 2 nm to less than or equal to 50 nm;
a volume of mesopores is greater than or equal to 35% of a total pore volume of the zeolite beta; and
an average particle size of the zeolite beta is less than or equal to 100 nm.

### Claim 11 (depends on 10)

The method of claim 10, further comprising, prior to the forming of the composite, adding water to the zeolite beta at a weight ratio of water to zeolite beta of 0.5 to 2.

### Claim 12 (depends on 10)

The method of claim 10, wherein forming the composite comprises:
mixing the zeolite beta and the hierarchical zeolite Y to form a zeolite mixture; and
heating the zeolite mixture at a temperature from 100° C. to 200° C. for a duration from 4 to 8 hours, or
hydrothermally treating the zeolite mixture at a temperature from 500° C. to 550° C. for a duration from 1 to 4 hours.

### Claim 13 (depends on 10)

The method of claim 10, wherein forming the composite comprises:
mixing the zeolite beta and the hierarchical zeolite Y to form a zeolite mixture; and
combing the zeolite mixture and a support material.

### Claim 14 (depends on 10)

The method of claim 10, wherein forming the composite comprises:
mixing the zeolite beta and the hierarchical zeolite Y to form a zeolite mixture; and
combing the zeolite mixture, a support material, and one or more metals, one or more metal oxides, or combinations thereof, chosen from tungsten atoms, molybdenum atoms, nickel atoms, tungsten oxide, molybdenum oxide, nickel oxide, or combinations thereof.

### Claim 15 (depends on 10)

The method of claim 10, wherein heating of the extrudates further comprises:
drying and calcinating at a temperature greater than or equal to 500° C. for a duration of at least 4 hours.

### Claim 16 (depends on 10)

The method of claim 10, wherein the method further comprises, after the heating of the extrudates, contacting the extrudates to a metal solution comprising one or more metals, one or more metal oxides, or combinations thereof, chosen from tungsten atoms, molybdenum atoms, nickel atoms, tungsten oxide, molybdenum oxide, nickel oxide, or combinations thereof.

### Claim 17 (depends on 16)

The method of claim 16, wherein the metal solution comprises nickel nitrate hexahydrate.

### Claim 18 (depends on 16)

The method of claim 16, wherein the metal solution comprises ammonium metatungstate.

### Claim 19

A process for upgrading a heavy oil, the process comprising:
contacting the heavy oil with a catalyst, wherein the contacting hydrocracks the heavy oil to produce an updated product stream;
the catalyst comprises zeolite beta, and
hierarchical zeolite Y;
wherein:
the zeolite beta comprises a plurality of micropores having a pore size of less than 2 nm and a plurality of mesopores having a pore size of greater than or equal to 2 nm to less than or equal to 50 nm;
a volume of mesopores is greater than or equal to 35% of a total pore volume of the zeolite beta; and
an average particle size of the zeolite beta is less than or equal to 100 nm.

### Claim 20 (depends on 19)

The process of claim 19, wherein the heavy oil and catalyst are contacted in a reactor, and a temperature of the reactor during the contacting is greater than or equal to 335° C.

### Claim 21 (depends on 19)

The process of claim 19, wherein the heavy oil is a crude oil comprising an API gravity of 25 to 30.

### Claim 22 (depends on 19)

The process of claim 19, wherein the updated product stream comprises greater than 47 wt. % ethylene, propylene, and butene.

### Claim 23 (depends on 19)

The process of claim 19, wherein hydrogen consumption is less than 4.75 wt. %.

### Claim 24 (depends on 19)

The process of claim 19, wherein the updated product stream comprises a sulfur concentration less than or equal to 16.9 wppm.

### Claim 25 (depends on 19)

The process of claim 19, wherein the updated product stream comprises a nitrogen concentration less than or equal to 3.7 wppm.

### Claim 26 (depends on 19)

The process of claim 19, wherein the updated product stream has a density less than or equal to 0.7999 g/ml.