# US 2026/0048371 A1 · Slurry homogenization process and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0048371 A1
- Document ID: US20260048371A1
- Status: Published application
- Kind: A1
- Application number: 19/367,813
- Filed: 2025-10-23
- Published: 2026-02-19
- Earliest claimed: 2023-04-27
- Assignees: Eve Power Co., Ltd.
- Applicants: Eve Power Co., Ltd.
- Inventors: Wenjun WANG; Yongmao LIU; Fei ZHANG
- Web page: https://patentgrep.com/patent/US20260048371A1

## CPC

- B01F 35/714: {for feeding predetermined amounts (B01F35/88 takes precedence)}
- H01M 4/1397: of electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- B01F 25/50: Circulation mixers, e.g. wherein at least part of the mixture is discharged from and reintroduced into a receptacle
- B01F 35/71775: {using helical screws}
- B01F 23/565: {by introducing liquids in solid material, e.g. to obtain slurries}
- B01F 2215/0477: Numerical time values
- B01F 2215/0481: Numerical speed values
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/623: {fluorinated polymers}
- H01M 4/625: {Carbon or graphite}
- Y02E 60/10: Energy storage using batteries
- B01F: MIXING, e.g. DISSOLVING, EMULSIFYING OR DISPERSING (mixing paints B44D3/06)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A slurry homogenization process and a use thereof, including the following steps: performing a first pre-mixing operation on a main material, a first conductive agent, and a binder to obtain a first mixture; adding the first mixture into a first solvent, and sequentially performing a second pre-mixing operation and a first dispersing operation to obtain a second mixture; and adding a conductive slurry into the second mixture, sequentially performing a third pre-mixing operation and a second dispersing operation to obtain a third mixture, and performing a defoaming and cooling operation on the third mixture to obtain a homogenized slurry.

## Claims

### Claim 1

A slurry homogenization process, comprising the following steps:
performing a first pre-mixing operation on a main material, a first conductive agent, and a binder to obtain a first mixture;
adding the first mixture into a first solvent, and sequentially performing a second pre-mixing operation and a first dispersing operation to obtain a second mixture; and
adding a conductive slurry into the second mixture, sequentially performing a third pre-mixing operation and a second dispersing operation to obtain a third mixture, and performing a defoaming and cooling operation on the third mixture to obtain a homogenized slurry.

### Claim 2 (depends on 1)

The slurry homogenization process according to claim 1, wherein based on a mass percent of the first mixture being 100%, a feeding sequence of the main material, the first conductive agent, and the binder is as follows: sequentially adding 40% to 60% of the main material, the first conductive agent, the binder, and 40% to 60% of the main material;
wherein the first conductive agent accounts for 0.2% to 5% by mass of the first mixture; and
the binder accounts for 1.3% to 6% by mass of the first mixture.

### Claim 3 (depends on 1)

The slurry homogenization process according to claim 1, wherein the main material comprises lithium iron phosphate, the first conductive agent comprises super P (SP), and the binder comprises polyvinylidene fluoride (PVDF).

### Claim 4 (depends on 1)

The slurry homogenization process according to claim 1, wherein the first pre-mixing operation is performed in a pre-mixing chamber; and
wherein the first pre-mixing operation is performed for a period of time ranging from 5 minutes to 30 minutes.

### Claim 5 (depends on 1)

The slurry homogenization process according to claim 1, wherein the first solvent comprises N-methylpyrrolidone (NMP).

### Claim 6 (depends on 1)

The slurry homogenization process according to claim 1, wherein a mass ratio of the first solvent to the first mixture is 1:(1.2 to 5).

### Claim 7 (depends on 1)

The slurry homogenization process according to claim 1, wherein before the step of adding the first mixture into a first solvent, the first solvent is circulated between a circulating tank and a pulping machine; and
wherein a flow rate of the first solvent for circulating between the pulping machine and the circulating tank is set between 50% and 65% of a pulping productivity of the pulping machine.

### Claim 8 (depends on 1)

The slurry homogenization process according to claim 1, wherein the second pre-mixing operation is performed in a circulating tank and a pulping machine;
wherein a linear velocity of the circulating tank in the second pre-mixing operation ranges from 18 m/s to 30 m/s;
a linear velocity of the pulping machine in the second pre-mixing operation ranges from 18 m/s to 30 m/s; and
in the second pre-mixing operation, a flow rate of the second mixture for circulating and dispersing between the pulping machine and the circulating tank is set between 50% and 65% of a pulping productivity of the pulping machine.

### Claim 9 (depends on 1)

The slurry homogenization process according to claim 1, wherein the second pre-mixing operation is performed for a period of time ranging from 15 minutes to 40 minutes.

### Claim 10 (depends on 1)

The slurry homogenization process according to claim 1, wherein the first dispersing operation is performed in a circulating tank and a pulping machine;
wherein a linear velocity of the circulating tank in the first dispersing operation ranges from 18 m/s to 30 m/s;
a linear velocity of the pulping machine in the first dispersing operation ranges from 18 m/s to 30 m/s; and
in the first dispersing operation, a flow rate of the second mixture for circulating and dispersing between the pulping machine and the circulating tank is set between 50% and 65% of a pulping productivity of the pulping machine.

### Claim 11 (depends on 1)

The slurry homogenization process according to claim 1, wherein the first dispersing operation is performed for a period of time ranging from 15 minutes to 30 minutes.

### Claim 12 (depends on 1)

The slurry homogenization process according to claim 1, wherein the conductive slurry accounts for 5% to 20% by mass of the homogenized slurry.

### Claim 13 (depends on 1)

The slurry homogenization process according to claim 1, wherein based on a mass percent of the conductive slurry being 100%, the conductive slurry comprises 4% to 6% of a second conductive agent, 1% to 2% of a dispersant, and a second solvent;
wherein the second conductive agent comprises carbon nanotubes, and the second solvent comprises N-methylpyrrolidone (NMP).

### Claim 14 (depends on 1)

The slurry homogenization process according to claim 1, wherein the third pre-mixing operation is performed in a circulating tank; and
wherein a linear velocity of the circulating tank in the third pre-mixing operation ranges from 18 m/s to 30 m/s.

### Claim 15 (depends on 1)

The slurry homogenization process according to claim 1, wherein the third pre-mixing operation is performed for a period of time ranging from 5 minutes to 15 minutes.

### Claim 16 (depends on 1)

The slurry homogenization process according to claim 1, wherein the second dispersing operation is performed in a pulping machine and a circulating tank;
wherein a condition for starting the second dispersing operation is as follows: a flow rate of the third mixture achieves stable during circulation between the pulping machine and the circulating tank; and
in the second dispersing operation, a flow rate of the third mixture for circulating and dispersing between the pulping machine and the circulating tank is set between 50% and 65% of a pulping productivity of the pulping machine.

### Claim 17 (depends on 16)

The slurry homogenization process according to claim 16, wherein a linear velocity of the pulping machine in the second dispersing operation ranges from 18 m/s to 30 m/s; and
wherein a linear velocity of the circulating tank in the second dispersing operation ranges from 18 m/s to 30 m/s.

### Claim 18 (depends on 1)

The slurry homogenization process according to claim 1, wherein the second dispersing operation is performed for a period time ranging from 15 minutes to 30 minutes.

### Claim 19 (depends on 1)

The slurry homogenization process according to claim 1, wherein the step of performing a defoaming and cooling operation is treated for a period time ranging from 15 minutes to 30 minutes.

### Claim 20

A use of a slurry homogenization process in the field of lithium-ion batteries, wherein the slurry homogenization process comprises the following steps:
performing a first pre-mixing operation on a main material, a first conductive agent, and a binder to obtain a first mixture;
adding the first mixture into a first solvent, and sequentially performing a second pre-mixing operation and a first dispersing operation to obtain a second mixture; and
adding a conductive slurry into the second mixture, sequentially performing a third pre-mixing operation and a second dispersing operation to obtain a third mixture, and performing a defoaming and cooling operation on the third mixture to obtain a homogenized slurry.