# US 2026/0043446 A1 · Method of refurbishing a steel-shell brake drum

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0043446 A1
- Document ID: US20260043446A1
- Status: Published application
- Kind: A1
- Application number: 19/293,657
- Filed: 2025-08-07
- Published: 2026-02-12
- Earliest claimed: 2024-08-08
- Assignees: Wheelnz LLC
- Applicants: Wheelnz LLC
- Inventors: Omar J. Fakhoury; John A. Schneider
- Web page: https://patentgrep.com/patent/US20260043446A1

## CPC

- F16D 65/0043: {Brake maintenance and assembly, tools therefor}
- B22D 13/04: of shallow solid or hollow bodies, e.g. wheels or rings, in moulds rotating around their axis of symmetry
- B22D 13/107: {Means for feeding molten metal}
- B22D 19/00: Casting in, on, or around objects which form part of the product (B22D23/04 takes precedence; alumino-thermic welding B23K23/00; coating by casting molten material on the substrate C23C6/00)
- B22D 19/10: Repairing defective or damaged objects by metal casting procedures (by other procedures B23P6/04; ingot mould B22D7/06; B22D19/06 takes precedence)
- F16D 51/00: Brakes with outwardly-movable braking members co-operating with the inner surface of a drum or the like (similar clutches F16D13/14)
- F16D 65/10: Drums for externally- or internally-engaging brakes
- B22D 19/08: for building-up linings or coverings, e.g. of anti-frictional metal
- F16D 2069/0491: {Tools, machines, processes}
- F16D 2200/0008: Ferro
- F16D 2200/0013: Cast iron
- F16D 2250/0007: Casting
- F16D 2250/0046: Coating
- F16D: COUPLINGS FOR TRANSMITTING ROTATION; CLUTCHES; BRAKES
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)

## Abstract

A method of refurbishing a steel-shell brake drum that includes superheating a worn-out brake drum until the worn-out brake drum is glowing hot. The worn-out brake drum includes a steel shell and a worn-out, gray-iron layer bonded to an inside surface of the steel shell. The method further includes centrifugal casting additional molten iron to the gray-iron layer to increase the radial thickness of the gray-iron layer.

## Claims

### Claim 1

A method of refurbishing a steel-shell brake drum, the method comprising:
superheating a worn-out brake drum until the worn-out brake drum is glowing hot, the worn-out brake drum comprising a steel shell and a gray-iron layer bonded to an inside surface of the steel shell, the gray-iron layer being worn out, the steel shell having an open end of the steel shell; and
centrifugal casting additional molten iron to the gray-iron layer to increase a radial thickness of the gray-iron layer to a rebuilt inner diameter of the gray-iron layer, the result being subsequently referred to in these claims as a phase-one brake drum.

### Claim 2 (depends on 1)

The method of claim 1, further comprising determining a structural integrity of the worn-out brake drum prior to superheating.

### Claim 3 (depends on 1)

The method of claim 1, further comprising removing rust, debris, and contaminants from the worn-out brake drum prior to superheating.

### Claim 4 (depends on 1)

The method of claim 1, further comprising machining one or more circumferential grooves in the gray-iron layer prior to superheating.

### Claim 5 (depends on 1)

The method of claim 1, in which the operation of centrifugal casting comprises:
orienting the worn-out brake drum so that the open end of the steel shell is horizontal;
spinning the superheated, horizontal, worn-out brake drum; and
introducing, under a centrifugal force created by the spinning, additional molten iron to the gray-iron layer to increase the radial thickness of the gray-iron layer to the rebuilt inner diameter of the gray-iron layer.

### Claim 6 (depends on 1)

The method of claim 1, further comprising, after centrifugal casting:
cooling the phase-one brake drum; and
machining the rebuilt inner diameter of the gray-iron layer of the phase-one brake drum to a final inner diameter of the gray-iron layer, the result being subsequently referred to in these claims as a phase-two brake drum.

### Claim 7 (depends on 6)

The method of claim 6, further comprising painting the phase-two brake drum.

### Claim 8 (depends on 1)

The method of claim 1, further comprising affixing a splash dam to the open end of the steel shell prior to superheating, the splash dam comprising a flat, annular plate, an inner diameter of the splash dam being less than the rebuilt inner diameter of the gray-iron layer.

### Claim 9 (depends on 8)

The method of claim 8, further comprising, after centrifugal casting:
cooling the phase-one brake drum;
removing the splash dam from the phase-one brake drum; and
machining the rebuilt inner diameter of the gray-iron layer of the phase-one brake drum to a final inner diameter of the gray-iron layer, the result being subsequently referred to in these claims as a phase-two brake drum.

### Claim 10 (depends on 9)

The method of claim 9, further comprising painting the phase-two brake drum.

### Claim 11

A method of refurbishing a worn-out brake drum, the worn-out brake drum comprising a steel shell and a gray-iron layer bonded to an inside surface of the steel shell, the gray-iron layer being worn out, the steel shell having an open end of the steel shell, the method comprising:
machining one or more circumferential grooves in the gray-iron layer;
affixing a splash dam to the open end of the steel shell, the splash dam comprising a flat, annular plate,
superheating the worn-out brake drum until the worn-out brake drum is glowing hot;
orienting the worn-out brake drum so that the open end of the steel shell is horizontal;
spinning the superheated, horizontal, worn-out brake drum;
introducing, under a centrifugal force created by the spinning, additional molten iron to the gray-iron layer to increase a radial thickness of the gray-iron layer to a rebuilt inner diameter of the gray-iron layer, the result being subsequently referred to in these claims as a phase-one brake drum, an inner diameter of the splash dam being less than the rebuilt inner diameter of the gray-iron layer;
removing the splash dam from the phase-one brake drum; and
machining the rebuilt inner diameter of the gray-iron layer of the phase-one brake drum to a final inner diameter of the gray-iron layer, the result being subsequently referred to in these claims as a phase-two brake drum.

### Claim 12 (depends on 11)

The method of claim 11, further comprising determining a structural integrity of the worn-out brake drum prior to superheating.

### Claim 13 (depends on 11)

The method of claim 11, further comprising removing rust, debris, and contaminants from the worn-out brake drum prior to superheating.

### Claim 14 (depends on 11)

The method of claim 11, further comprising painting the phase-two brake drum.