# US 2026/0043155 A1 · Method for making perovskite electrodes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0043155 A1
- Document ID: US20260043155A1
- Status: Published application
- Kind: A1
- Application number: 19/365,820
- Filed: 2025-10-22
- Published: 2026-02-12
- Earliest claimed: 2023-04-20
- Assignees: King Fahd University of Petroleum and Minerals
- Applicants: King Fahd University of Petroleum and Minerals
- Inventors: Mohamed Jaffer Sadiq MOHAMED; Muhammad Ashraf GONDAL
- Web page: https://patentgrep.com/patent/US20260043155A1

## CPC

- C25B 11/0773: {of the perovskite type}
- C25B 1/04: by electrolysis of water
- C25B 11/052: Electrodes comprising one or more electrocatalytic coatings on a substrate
- C25B 11/065: Carbon
- C25B 11/067: Inorganic compound e.g. ITO, silica or titania
- C25B 11/075: consisting of a single catalytic element or catalytic compound
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)

## Abstract

An electrode includes a transparent substrate, and a layer of a nanostructured material at least partially covering a surface of the transparent substrate. The nanostructured material includes defective perovskite nanostructures (DPNSs) in the form of nanoplates having an average particle size in a range of 10 to 100 nanometers (nm), an interplanar spacing d(101) of the (101) plane in a range of 0.3 to 0.4 nm, and an interplanar spacing d(104) of the (104) plane in a range of 0.2 to 0.3 nm. A method of making the electrode.

## Claims

### Claim 1

(canceled)

### Claim 2 (depends on 10)

The method of claim 10, wherein the transparent substrate is a glass substrate, and wherein the glass substrate is at least one selected from the group consisting of a fluorine doped tin oxide (FTO) glass substrate, a tin doped indium oxide (ITO) glass substrate, an aluminum doped zinc oxide (AZO) glass substrate, a niobium doped titanium dioxide (NTO) glass substrate, an indium doped cadmium oxide (ICO) glass substrate, an indium doped zinc oxide (IZO) glass substrate, a fluorine doped zinc oxide (FZO) glass substrate, a gallium doped zinc oxide (GZO) glass substrate, an antimony doped tin oxide (ATO) glass substrate, a phosphorus doped tin oxide (PTO) glass substrate, a zinc antimonate glass substrate, a zinc oxide glass substrate, a ruthenium oxide glass substrate, a rhenium oxide glass substrate, a silver oxide glass substrate, and a nickel oxide glass substrate.

### Claim 3 (depends on 10)

The method of claim 10, wherein the transparent substrate is a glassy carbon substrate.

### Claim 4 (depends on 10)

The method of claim 10, wherein the nanostructured material has a formula ATiO3-x, wherein:
A is at least one metal selected from the group consisting of Ba, Co, Ni, Pb, Zn, Sr, and La, and 0<x<3.

### Claim 5 (depends on 10)

The method of claim 10, wherein the nanostructured material has a formula CoTiO3-x, wherein 0<x<3.

### Claim 6 (depends on 10)

The method of claim 10, wherein the electrode has an overpotential of 0.2 to 0.5 volts (V) in an acidic medium at a current density of 5 to 20 milliamperes per square centimeter (mA/cm2).

### Claim 7 (depends on 10)

The method of claim 10, wherein the electrode has a double layer capacitance of 200 to 280 microfarads per square centimeter (μF/cm2) in an acidic medium at an overpotential of 0.352 VRHE.

### Claim 8 (depends on 10)

The method of claim 10, wherein the electrode has an active surface area of 4 to 10 square centimeters (cm2) in an acidic medium at an overpotential of 0.352 VRHE.

### Claim 9 (depends on 10)

The method of claim 10, wherein the electrode has a Tafel slope of 80 to 110 millivolts per decade (mV/decade) in an acidic medium at a scan rate of 5 to 20 millivolts per second (mV/s).

### Claim 10

A method of making an electrode, comprising:
preparing a nanostructured material having defective perovskite nanostructures by:
mixing a titanium salt, an alkaline earth metal base and water to form a precipitate in a first mixture;
removing the precipitate from the first mixture, drying, and calcining at a temperature of at least 600° C. to form a TiO2 nanocomposite;
mixing the TiO2 nanocomposite and a borohydride reducing agent to form a second mixture;
calcining the second mixture at a temperature of at least 600° C. to form a defective nanocomposite of formula TiO2-x;
wherein 0<x<2;
mixing and sonicating the defective nanocomposite, a cobalt salt, and a solvent to form a suspension;
generating a pulsed laser using a laser device and projecting the pulsed laser onto the suspension to form an ablated nanocomposite in the suspension;
removing the ablated nanocomposite from the second suspension, washing, and drying to form a nanostructured material precursor; and
calcining the nanostructured material precursor at a temperature of at least 600° C. to form the nanostructured material,
disposing the nanostructured material on a transparent substrate to form the electrode;
wherein a layer of the nanostructured material at least partially covers a surface of the transparent substrate; and
wherein the nanostructured material comprises defective perovskite nanostructures (DPNSs) in the form of nanoplates having an average particle size in a range of 10 to 100 nanometers (nm), an interplanar spacing d(101) of the (101) plane in a range of 0.3 to 0.4 nm, and an interplanar spacing d(104) of the (104) plane in a range of 0.2 to 0.3 nm, as determined by X-ray diffraction.

### Claim 11 (depends on 10)

The method of claim 10, wherein the titanium salt comprises titanium tetrachloride, titanium trichloride, titanium potassium fluoride, titanium potassium oxalate, titanium sulfate, titanium tetra iodide, and/or its hydrate.

### Claim 12 (depends on 10)

The method of claim 10, wherein the alkaline earth metal base comprises an alkaline earth metal carbonate, and an alkaline earth metal hydroxide.

### Claim 13 (depends on 10)

The method of claim 10, wherein the cobalt salt comprises cobalt sulfate, cobalt acetate, cobalt citrate, cobalt iodide, cobalt chloride, cobalt perchlorate, cobalt nitrate, cobalt phosphate, cobalt triflate, cobalt bis(trifluoromethanesulfonyl)imide, cobalt tetrafluoroborate, cobalt bromide, and/or its hydrate.

### Claim 14 (depends on 10)

The method of claim 10, wherein the solvent is at least one selected from the group consisting of a ketone solvent, an ester solvent, an alcohol solvent, an amide solvent and an ether solvent, and wherein the alcohol solvent comprises ethylene glycol.

### Claim 15 (depends on 10)

The method of claim 10, wherein the pulsed laser has a wavelength of 500 to 560 nm, and a pulse energy of 300 to 400 millijoules (mJ).

### Claim 16 (depends on 10)

The method of claim 10, further comprising:
coating the transparent substrate by:
mixing the nanostructured material, a sulfonated polymer and a solvent mixture to form a third mixture;
sonicating the third mixture to form a coating composition; and
drop casting the coating composition onto a surface of the transparent substrate and drying to form the electrode having the layer of the nanostructured material at least partially covered on the surface of the transparent substrate.

### Claim 17 (depends on 16)

The method of claim 16, wherein the sulfonated polymer comprises at least one of Nafion, sulfonated poly(ether ether ketone) (SPEEK), sulfonated polyimide, sulfonated poly(phenylene oxide) (PPO), sulfonated poly(arylene ether sulfone), and sulfonated poly(4-phenoxybenzoyl-1,4-phenylene).

### Claim 18 (depends on 16)

The method of claim 16, wherein the solvent mixture comprises an alcohol solvent and an ester solvent, and wherein a volume ratio of the alcohol solvent and the ester solvent is in a range of 1:50 to 1:10.

### Claim at position 19

-20. (canceled)