# US 2026/0043124 A1 · Fabrication of scandium-containing targets

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0043124 A1
- Document ID: US20260043124A1
- Status: Published application
- Kind: A1
- Application number: 19/295,610
- Filed: 2025-08-09
- Published: 2026-02-12
- Earliest claimed: 2024-08-09
- Applicants: SRL Holding Company Pty Ltd
- Inventors: Timothy James Langan; Paul George Sanders
- Web page: https://patentgrep.com/patent/US20260043124A1

## CPC

- C23C 14/3414: {Metallurgical or chemical aspects of target preparation, e.g. casting, powder metallurgy}
- B22F 7/008: {characterised by the composition}
- B22F 7/08: with one or more parts not made from powder {(B22F7/062 takes precedence)}
- B22F 10/28: Powder bed fusion, e.g. selective laser melting [SLM] or electron beam melting [EBM]
- C22C 1/0416: {Aluminium-based alloys}
- C22C 1/047: comprising intermetallic compounds {(C22C1/0441 takes precedence)}
- C23C 14/0641: {Nitrides (C23C14/0617 takes precedence)}
- B22F 2201/01: Reducing atmosphere
- B22F 2201/10: Inert gases
- B22F 2201/20: Use of vacuum
- B22F 2301/052: Aluminium
- B33Y 10/00: Processes of additive manufacturing
- B33Y 70/00: Materials specially adapted for additive manufacturing
- B33Y 80/00: Products made by additive manufacturing
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING

## Abstract

Aluminum-scandium sputter targets with controlled compositions and refined microstructures are disclosed. The composition and microstructure of the Al—Sc target may be controlled to deposit AlScN structures with optimal Sc levels. Refining microstructure reduces variations in parameters required for sputter deposition of Al—Sc structures. The fabrication process may utilize a localized heat source such as a laser, electron beam, electric arc, or the like to build the target layer-by-layer from powder feed stock.

## Claims

### Claim 1

A method of making an aluminum-scandium sputter target comprising:
depositing a first powder layer comprising Al—Sc particles onto a substrate;
heating the particles of the first powder layer to form a first Al—Sc alloy layer and rapidly cooling the first Al—Sc alloy layer;
depositing at least one additional powder layer comprising Al—Sc particles onto the first Al—Sc alloy layer; and
heating the particles of the at least one additional powder layer to form at least one additional Al—Sc alloy layer and rapidly cooling the at least one additional Al—Sc alloy layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the steps of heating the particles of the first powder layer and heating the particles of the at least one additional powder layer are performed at a heating temperature of at least 1,400° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the steps of heating the particles of the first powder layer and heating the particles of the at least one additional powder layer are performed with a laser, e-beam or electric arc.

### Claim 4 (depends on 1)

The method of claim 1, wherein the steps of rapidly cooling the first Al—Sc alloy layer and rapidly cooling the at least one additional Al—Sc alloy layer are performed at a cooling rate of at least 103° C./second.

### Claim 5 (depends on 4)

The method of claim 4, wherein the cooling rate is from 105° C./second to 107° C./second.

### Claim 6 (depends on 1)

The method of claim 1, wherein the method comprises a powder bed fusion additive manufacturing process.

### Claim 7 (depends on 1)

The method of claim 1, wherein the method is performed in an atmosphere comprising a vacuum, inert gas, or a reducing gas that reacts with oxygen.

### Claim 8 (depends on 1)

The method of claim 1, wherein the substrate comprises a target backing plate.

### Claim 9 (depends on 8)

The method of claim 8, wherein the first powder layer is deposited directly on the target backing plate.

### Claim 10 (depends on 8)

The method of claim 8, wherein the first powder layer is deposited on an intermediate bonding layer at least partially covering the target backing plate.

### Claim 11 (depends on 10)

The method of claim 10, wherein the bonding layer is uniform through a thickness of the bonding layer.

### Claim 12 (depends on 10)

The method of claim 10, wherein the bonding layer is non-uniform through a thickness of the bonding layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein the non-uniform bonding layer is graded through the thickness of the bonding layer.

### Claim 14 (depends on 10)

The method of claim 10, wherein the bonding layer is additively manufactured on the target backing plate.

### Claim 15 (depends on 1)

The method of claim 1, wherein the Al—Sc particles have particle sizes of from 10 to 50 microns.

### Claim 16 (depends on 1)

The method of claim 1, wherein the Al—Sc alloy layers comprise a single phase.

### Claim 17 (depends on 1)

The method of claim 1, wherein the Al—Sc alloy layers comprise a metastable phase that is substantially free of Al3Sc, Al2Sc, AlSc and AlSc2 intermetallics.

### Claim 18 (depends on 1)

The method of claim 1, wherein the Al—Sc alloy layers comprise from 40 to 90 atomic percent Al and from 10 to 60 atomic percent Sc.

### Claim 19 (depends on 1)

The method of claim 1, wherein the Al—Sc alloy layers comprise from 50 to 80 atomic percent Al and from 20 to 50 atomic percent Sc.

### Claim 20 (depends on 1)

An aluminum-scandium sputter target produced by the method of claim 1.

### Claim 21

An aluminum-scandium sputter target comprising an Al—Sc alloy comprising a metastable phase that is substantially free of Al3Sc, Al2Sc, AlSc and AlSc2 intermetallics.

### Claim 22 (depends on 1)

A method of sputter depositing aluminum scandium nitride on a substrate comprising generating Al—Sc alloy vapor from an Al—Sc alloy target in a nitrogen containing atmosphere to produce AlScN, and depositing the AlScN on a substrate, wherein the Al—Sc alloy target has been produced by the method of claim 1.

### Claim 23

A method of sputter depositing aluminum scandium nitride on a substrate comprising generating Al—Sc alloy vapor from an Al—Sc alloy target in a nitrogen containing atmosphere to produce AlScN, and depositing the AlScN on a substrate, wherein the Al—Sc alloy comprises a metastable phase that is substantially free of Al3Sc, Al2Sc, AlSc and AlSc2 intermetallics.