# US 2026/0042674 A1 · Method for making activated carbon material for supercapacitor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0042674 A1
- Document ID: US20260042674A1
- Status: Published application
- Kind: A1
- Application number: 18/913,475
- Filed: 2024-10-11
- Published: 2026-02-12
- Earliest claimed: 2024-08-06
- Assignees: CPC Corporation, Taiwan
- Applicants: Cpc Corporation, Taiwan
- Inventors: Yan-Shi CHEN
- Web page: https://patentgrep.com/patent/US20260042674A1

## CPC

- C01B 32/318: characterised by the starting materials
- C01B 32/33: from distillation residues of coal or petroleum; from petroleum acid sludge
- C01B 32/342: characterised by non-gaseous activating agents
- C01B 32/348: Metallic compounds
- C01B 32/378: Purification
- H01G 11/44: Raw materials therefor, e.g. resins or coal
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/14: Pore volume
- C01P 2006/16: Pore diameter
- C01P 2006/40: Electric properties
- H01G 11/34: characterised by carbonisation or activation of carbon
- Y02E 60/13: Energy storage using capacitors
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for making an activated carbon material for a supercapacitor includes: heating a heavy hydrocarbon oil at 2 atm to 3 atm and 480° C. to 580° C. for at least 4 hours such that the heavy hydrocarbon oil undergoes a coking reaction to form a soft carbon precursor containing a mesophase structure of greater than 50 vol % and having a quinoline-insoluble content from 78 wt % to 98 wt % and a toluene-insoluble content from 88 wt % to 100 wt %; mixing the soft carbon precursor and an activator to obtain a mixture; heating the mixture to obtain a first carbonaceous component containing an activated carbon and a residual of the activator; removing the residual of the activator to obtain a second carbonaceous component; grinding and sizing the second carbonaceous component to obtain a third carbonaceous component; and heating the third carbonaceous component to obtain the activated carbon material.

## Claims

### Claim 1

A method for making an activated carbon material for a supercapacitor, comprising the steps of:
(A) heating a heavy hydrocarbon oil at a pressure ranging from 2 atm to 3 atm and a temperature ranging from 480° C. to 580° C. for at least 4 hours such that the heavy hydrocarbon oil undergoes a coking reaction to form a soft carbon precursor, the soft carbon precursor containing a mesophase structure of greater than 50 vol % based on 100 vol % of the soft carbon precursor, and having a quinoline-insoluble content ranging from 78 wt % to 98 wt % and a toluene-insoluble content ranging from 88 wt % to 100 wt %;
(B) mixing the soft carbon precursor and an activator so as to obtain a mixture;
(C) heating the mixture such that the mixture undergoes an activation reaction and a carbonization reaction to obtain a first carbonaceous component containing an activated carbon and a residual of the activator;
(D) removing the residual of the activator from the first carbonaceous component so as to obtain a second carbonaceous component;
(E) grinding and sizing the second carbonaceous component so as to obtain a third carbonaceous component; and
(F) heating the third carbonaceous component so as to obtain the activated carbon material for the supercapacitor.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein in step (B), a weight ratio of the soft carbon precursor to the activator ranges from 0.125 to 0.25.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein in step (C), the mixture is heated to a temperature ranging from 700° C. to 900° C. at a heating rate ranging from 1° C./min to 10° C./min under nitrogen atmosphere.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein in step (F), the third carbonaceous component is heated to a temperature of less than 1000° C. at a heating rate ranging from 1° C./min to 10° C./min under nitrogen atmosphere.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein in step (F), the activated carbon material has a plurality of micropores and a plurality of mesopores, a diameter of each of the plurality of mesopores being greater than a diameter of each of the plurality of micropores, and a ratio of a total volume of the plurality of micropores to a total volume of the plurality of mesopores ranging from 0.45 to 7.5.

### Claim 6 (depends on 1)

The method as claimed in claim 1, wherein in step (B), the activator is potassium hydroxide.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein in step (D), the residual of the activator is removed by subjecting the first carbonaceous component to an acid washing treatment, a water washing treatment and a drying treatment.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein in step (E), a portion of the third carbonaceous component has a D50 particle size ranging from 8 μm to 12 μm, a D10 particle size ranging from 2 μm to 6 μm, and a D90 particle size ranging from 14 μm to 20 μm.