# US 2026/0040848 A1 · Method for forming a high-k metal oxide

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0040848 A1
- Document ID: US20260040848A1
- Status: Published application
- Kind: A1
- Application number: 19/031,877
- Filed: 2025-01-18
- Published: 2026-02-05
- Earliest claimed: 2024-08-02
- Assignees: Pentapro Materials Inc.
- Applicants: Pentapro Materials Inc.
- Inventors: Wen-Che Kuo; Wen-Lian Lee; Pi-Chun Juan; Pak-Man Yiu
- Web page: https://patentgrep.com/patent/US20260040848A1

## CPC

- H10P 14/69392: {the material containing hafnium, e.g. HfO2}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/668: {the materials being characterised by the deposition precursor materials}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention provides a method for forming a high-k metal oxide. By using a small amount of a precursor mainly composed of trisilyl amine (TSA, chemical formula: N(SiH3)3) to generate silicon dioxide (SiO2), and incorporating it into a high-k metal oxide with an organometallic compound as its precursor, a high-performance high-k metal oxide with a good interface layer to the substrate is formed. This approach effectively prevents leakage in a metal-insulator-semiconductor (MIS) structure and achieves a transistor gate oxide layer with high dielectric constant, low leakage current, high breakdown voltage, and high reliability, while also lowering production costs.

## Claims

### Claim 1

A method for forming a metal oxide dielectric layer, comprising:
providing a substrate;
placing the substrate into a sealed chamber;
forming a silicon-doped metal oxide dielectric layer on the substrate;
performing a rapid thermal anneal on the substrate such that a silicon dioxide interfacial layer is formed between the substrate and the metal oxide dielectric layer;
wherein the silicon doping employs trisilyl amine (chemical formula N(SiH3)3) as a reaction precursor.

### Claim 2 (depends on 1)

The method for forming a metal oxide dielectric layer according to claim 1, wherein the silicon-doped metal oxide dielectric layer is formed by doping an organometallic precursor with trisilyl amine and then introducing it into an environment containing an active oxygen source to react.

### Claim 3 (depends on 1)

The method for forming a metal oxide dielectric layer according to claim 1, wherein the silicon-doped metal oxide dielectric layer is formed by an atomic layer deposition process comprising alternating cycles of depositing silicon dioxide using trisilyl amine as the precursor and depositing a metal oxide using an organometallic precursor.

### Claim 4 (depends on 1)

The method for forming a metal oxide dielectric layer according to claim 1, wherein the metal oxide dielectric layer is a metal oxide or nitride.

### Claim 5 (depends on 1)

The method for forming a metal oxide dielectric layer according to claim 1, wherein the metal oxide dielectric layer is selected from the group consisting of hafnium dioxide, zirconium dioxide, lanthanum oxide, and aluminum oxide.

### Claim 6 (depends on 2)

The method for forming a metal oxide dielectric layer according to claim 2, wherein is the organometallic precursor tetrakis(ethylmethylamino)hafnium or tetrakis(dimethylamido)hafnium to form a hafnium dioxide metal oxide dielectric layer.

### Claim 7 (depends on 1)

The method for forming a metal oxide dielectric layer according to claim 1, wherein the silicon doping concentration is between 0.1% and 10%.

### Claim 8 (depends on 1)

The method for forming a metal oxide dielectric layer according to claim 1, wherein forming the silicon-doped metal oxide dielectric layer on the substrate further comprises:
introducing an active oxygen source into the sealed chamber; and
heating the substrate to a temperature between 100° C. and 450° C.

### Claim 9 (depends on 1)

The method for forming a metal oxide dielectric layer according to claim 1, wherein the rapid thermal anneal temperature is between 300° C. and 1100° C.

### Claim 10 (depends on 6)

The method for forming a metal oxide dielectric layer according to claim 6, wherein the hafnium dioxide has an orthorhombic or tetragonal crystal structure.

### Claim 11 (depends on 8)

The method for forming a metal oxide dielectric layer according to claim 8, wherein the active oxygen source is selected from the group consisting of ozone, neutral oxygen atoms, and oxygen ions.

### Claim 12 (depends on 1)

The method for forming a metal oxide dielectric layer according to claim 1, wherein the substrate is selected from the group consisting of silicon, silicon carbide, and compound semiconductors.