# US 2026/0040723 A1 · Photovoltaic cell, method for producing the same and photovoltaic module

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0040723 A1
- Document ID: US20260040723A1
- Status: Published application
- Kind: A1
- Application number: 19/356,017
- Filed: 2025-10-10
- Published: 2026-02-05
- Earliest claimed: 2023-02-21
- Assignees: Zhejiang Jinko Solar Co., Ltd.; Jinko Solar Co., Ltd.
- Applicants: Zhejiang Jinko Solar Co., Ltd.; Jinko Solar Co., Ltd.
- Inventors: Jingsheng JIN; Guangming LIAO; Nannan YANG
- Web page: https://patentgrep.com/patent/US20260040723A1

## CPC

- H10F 77/219: {Arrangements for electrodes of back-contact photovoltaic cells}
- H10F 10/146: {Back-junction photovoltaic cells, e.g. having interdigitated base-emitter regions on the back side}
- H10F 10/165: the heterojunctions being Group IV-IV heterojunctions, e.g. Si/Ge, SiGe/Si or Si/SiC photovoltaic cells
- H10F 71/131: {Recrystallisation; Crystallization of amorphous or microcrystalline semiconductors}
- H10F 77/311: {for photovoltaic cells}
- H10F 77/315: {the coatings being antireflective or having enhancing optical properties}
- H10F 77/703: {of the semiconductor bodies, e.g. textured active layers}
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed is a method for producing a photovoltaic cell. The method includes providing a silicon wafer, forming a tunneling oxide layer on a first side of the silicon wafer, forming an amorphous silicon layer having alternatingly arranged P-type amorphous silicon and N-type amorphous silicon on a side of the tunneling oxide layer away from the silicon wafer, forming a protective layer on a side of the amorphous silicon layer away from the silicon wafer, performing laser processing on the protective layer and the amorphous silicon layer to form grooves, subjecting the silicon wafer to further processing to increase depths of the grooves, removing the protective layer, and subjecting the silicon wafer to high temperature processing to convert the amorphous silicon layer into a polycrystalline silicon layer.

## Claims

### Claim 1

A method for producing a photovoltaic cell, comprising:
providing a silicon wafer, the silicon wafer having a first side;
forming a tunneling oxide layer on the first side of the silicon wafer;
forming an amorphous silicon layer having alternatingly arranged P-type amorphous silicon and N-type amorphous silicon on a side of the tunneling oxide layer away from the silicon wafer;
forming a protective layer on a side of the amorphous silicon layer away from the silicon wafer;
performing laser processing on the protective layer and the amorphous silicon layer, to form grooves;
subjecting the silicon wafer to further processing, wherein depths of the grooves are increased during the further processing;
removing the protective layer; and
subjecting the silicon wafer to high temperature processing, to convert the amorphous silicon layer into a polycrystalline silicon layer.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the grooves are configured to extend through the amorphous silicon layer and the tunneling oxide layer and into the silicon wafer, after the further processing.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the silicon wafer has a second side opposite to the first side; the method comprises: forming a textured structure on the second side of the silicon wafer during the further processing.

### Claim 4 (depends on 1)

The method according to claim 1, wherein after subjecting the silicon wafer to the high temperature processing, to convert the amorphous silicon layer into the polycrystalline silicon layer, the method further includes:
simultaneously forming a passivation layer on the first side and a second side of the silicon wafer; and
forming an electrode on the first side of the silicon wafer.

### Claim 5 (depends on 1)

The method according to claim 1, wherein after the further processing, the depths of the grooves are greater than a total thickness of the polysilicon layer and the tunneling oxide layer.

### Claim 6 (depends on 3)

The method according to claim 3, wherein subjecting the silicon wafer to the further processing by using a tank-type device, and by using potassium hydroxide, additives, and deionized water, wherein a concentration of the potassium hydroxide ranges from 1% to 1.5%, and a concentration of the additives ranges from 0.5% to 1%.

### Claim 7 (depends on 1)

The method according to claim 1, wherein removing the protective layer includes: using a tank-type device, and removing the protective layer by using a hydrogen fluoride solution, wherein a concentration of the hydrogen fluoride ranges from 10% to 20%.

### Claim 8 (depends on 1)

The method according to claim 1, wherein during the high temperature processing, a temperature of the high temperature processing ranges from 850° C. to 950° C.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the silicon wafer has a thickness ranging from 80 μm to 180 μm.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the silicon wafer has a length ranging from 156 mm to 220 mm.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the silicon wafer as provided is a clean silicon wafer on which impurities have been removed from a surface.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the silicon wafer has a surface that is not exposed to sunlight on the first side.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the tunneling oxide layer has a thickness ranging from 1 nm to 1.5 nm.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the protective layer has a thickness greater than or equal to 2 nm.

### Claim 15 (depends on 1)

The method according to claim 1, wherein during the laser processing, a laser wavelength ranges from 300 nm to 1000 nm, a size of a laser spot ranges from 50 μm to 120 μm, laser energy ranges from 2 W to 15 W, and an overlapping area of adjacent light spots ranges from 10% to 30%.

### Claim 16 (depends on 1)

The method according to claim 1, wherein a distance between adjacent grooves ranges from 100 μm to 500 μm.

### Claim 17 (depends on 1)

The method according to claim 1, wherein the grooves have widths ranging from 100 μm to 300 μm.

### Claim 18 (depends on 1)

The method according to claim 1, wherein the grooves are configured to separate the P-type amorphous silicon and the N-type amorphous silicon respectively.

### Claim 19 (depends on 4)

The method according to claim 4, wherein the electrode extends into the polysilicon silicon layer by a depth ranging from 10 nm to 100 nm.

### Claim 20 (depends on 4)

The method according to claim 4, the passivation layer is of two layers or three layers.