# US 2026/0040458 A1 · Thin, stretchable and flexible printed circuit and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0040458 A1
- Document ID: US20260040458A1
- Status: Published application
- Kind: A1
- Application number: 19/027,657
- Filed: 2025-01-17
- Published: 2026-02-05
- Earliest claimed: 2024-07-31
- Assignees: Mflex (Yancheng) Co., Ltd.
- Applicants: Mflex (Yancheng) Co., Ltd.
- Inventors: JIE ZHANG; ZONGMIN HU; JIANCHENG CAO
- Web page: https://patentgrep.com/patent/US20260040458A1

## CPC

- H05K 1/0283: {Stretchable printed circuits}
- H05K 3/007: {Manufacture or processing of a substrate for a printed circuit board supported by a temporary or sacrificial carrier (H05K1/187, H05K3/20 and H05K3/4682 take precedence)}
- H05K 1/02: Details
- H05K 1/0277: {Bendability or stretchability details (H05K1/038, H05K3/4691 take precedence)}
- H05K 1/0393: {Flexible materials (H05K1/038 takes precedence; specific organic compositions are classified in H05K1/0313 and subgroups)}
- H05K 3/0044: {Mechanical working of the substrate, e.g. drilling or punching (H05K3/0008 takes precedence)}
- H05K 2201/05: Flexible printed circuits [FPCs]
- H05K 2201/09009: Substrate related
- H05K 2201/09263: Meander
- H05K 2203/0147: Carriers and holders
- H05K 2203/0228: Cutting, sawing, milling or shearing
- H05K 2203/10: Using electric, magnetic and electromagnetic fields; Using laser light
- H05K 2203/1194: Thermal treatment leading to a different chemical state of a material, e.g. annealing for stress-relief, aging
- H05K 2203/1377: Protective layers
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

Disclosed are a thin, stretchable and flexible printed circuit and a manufacturing method therefor. The manufacturing method comprise: attaching an adhesion-reducing carrier film to a first side of a flexible circuit board provided with a circuit layer and two protective films, wherein the adhesion-reducing carrier film has a large first preset adhesive force; and attaching a first elastomer composite film, and then performing an adhesion-reducing operation on the adhesion-reducing carrier film to allow the adhesion-reducing carrier film to have a small second preset adhesive force. The elastomer composite film is formed by two polymer films with different melting points. The invention can increase the product yield in mass production based on the adhesion-reducing carrier film and can wrap a serpentine circuit by means of the elasticity of a composite structure of the polymer films to realize thin and light design and miniaturization.

## Claims

### Claim 1

A manufacturing method for a thin, stretchable and flexible printed circuit, comprising:
a step of providing a flexible circuit board provided with a circuit layer and two protective films, and attaching an adhesion-reducing carrier film to a first side of the flexible circuit board to form a first circuit board, wherein the two protective layers are located on two sides of the circuit layer respectively, and the adhesion-reducing carrier film has a first preset adhesive force;
a step of performing contour cutting, from a second side of the first circuit board, on the two protective films in the first circuit board to form a serpentine circuit by the circuit layer and the two protective films subjected to the contour cutting, and stripping scrap from the cut first circuit board to form a second circuit board, wherein the serpentine circuit has at least one stretching direction;
a step of providing a first elastomer composite film, attaching the first elastomer composite film to a second side of the second circuit board, and performing an adhesion-reducing operation on the adhesion-reducing carrier film on a first side of the second circuit board to allow the adhesion-reducing carrier film to have a second preset adhesive force to form a third circuit board, wherein the second preset adhesive force is less than the first preset adhesive force; and
a step of stripping the adhesion-reducing carrier film from the third circuit board to form a target circuit.

### Claim 2 (depends on 1)

The manufacturing method according to claim 1, wherein the adhesion-reducing carrier film is any one of a UV adhesion-reducing film and a thermal adhesion-reducing film.

### Claim 3 (depends on 2)

The manufacturing method according to claim 2, wherein in a case where the adhesion-reducing carrier film is the UV adhesion-reducing film, performing an adhesion-reducing operation on the adhesion-reducing carrier film on a first side of the second circuit board comprises:
performing UV exposure on the adhesion-reducing carrier film on the first side of the second circuit board;
in a case where adhesion-reducing carrier film is the thermal adhesion-reducing film, performing an adhesion-reducing operation on the adhesion-reducing carrier film on a first side of the second circuit board comprises:
heating the adhesion-reducing carrier film on the first side of the second circuit board.

### Claim 4 (depends on 1)

The manufacturing method according to claim 1, wherein the first preset adhesive force is greater than 500 gf/inch, and the second preset adhesive force is less than 100 gf/inch.

### Claim 5 (depends on 1)

The manufacturing method according to claim 1, wherein the first elastomer composite film comprises a first polymer film with a first melting point and a second polymer film with a second melting point, and the second polymer film is arranged on a side of the first polymer film; wherein, the first melting point is lower than the second melting point.

### Claim 6 (depends on 5)

The manufacturing method according to claim 5, wherein the step of providing a first elastomer composite film, attaching the first elastomer composite film to a second side of the second circuit board, and performing an adhesion-reducing operation on the adhesion-reducing carrier film on a first side of the second circuit board to allow the adhesion-reducing carrier film to have a second preset adhesive force to form a third circuit board comprises:
performing the adhesion-reducing operation on the adhesion-reducing carrier film on the first side of the second circuit board to allow the adhesion-reducing carrier film to have the second preset adhesive force;
providing the first elastomer composite film; and
attaching a side, provided with the first polymer film, of the first elastomer composite film to the second side of the second circuit board subjected to the adhesion-reducing operation to form the third circuit board.

### Claim 7 (depends on 5)

The manufacturing method according to claim 5, wherein the step of providing a first elastomer composite film, attaching the first elastomer composite film to a second side of the second circuit board, and performing an adhesion-reducing operation on the adhesion-reducing carrier film on a first side of the second circuit board to allow the adhesion-reducing carrier film to have a second preset adhesive force to form a third circuit board comprises:
providing the first elastomer composite film;
attaching a side, provided with the first polymer film, of the first elastomer composite film to the second side of the second circuit board; and
performing the adhesion-reducing operation on the adhesion-reducing carrier film on the first side of the second circuit board to allow the adhesion-reducing carrier film to have the second preset adhesive force to form the third circuit board.

### Claim 8 (depends on 5)

The manufacturing method according to claim 5, wherein after the step of stripping the adhesion-reducing carrier film from the third circuit board, the manufacturing method further comprises:
a step of providing a second elastomer composite film identical with the first elastomer composite film; and
a step of attaching a side, provided with the first polymer film, of the second elastomer composite film to a first side of the third circuit board formed after the adhesion-reducing carrier film is stripped.

### Claim 9 (depends on 5)

The manufacturing method according to claim 5, wherein a difference between the second melting point and the first melting point ranges from 20° C. to 100° C.

### Claim 10 (depends on 5)

The manufacturing method according to claim 5, wherein a difference between the second melting point and the first melting point ranges from 30° C. to 60° C.

### Claim 11 (depends on 5)

The manufacturing method according to claim 5, wherein a thickness of the first polymer film ranges from 30 μm to 100 μm, and/or, a thickness of the second polymer film ranges from 25 μm to 150 μm.

### Claim 12 (depends on 1)

The manufacturing method according to claim 1, wherein the serpentine circuit comprises:
a substrate layer;
at least one wire layer, laminated on one or two sides of the substrate layer; and
the two protective films subjected to the contour cutting, respectively adhered to outermost said wire layers or the substrate layer by means of adhesive layers.

### Claim 13 (depends on 12)

The manufacturing method according to claim 12, wherein one or more wires are configured in each said wire layer.

### Claim 14 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13)

A thin, stretchable and flexible printed circuit, being manufactured by the manufacturing method according to any one of claims 1-13.