# US 2026/0040443 A1 · Use of inorganic thin non-woven dielectrics in printed circuit boards

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0040443 A1
- Document ID: US20260040443A1
- Status: Published application
- Kind: A1
- Application number: 19/350,791
- Filed: 2025-10-06
- Published: 2026-02-05
- Earliest claimed: 2023-04-04
- Assignees: Advanced Chip and Circuit Materials, Inc.
- Applicants: Advanced Chip and Circuit Materials, Inc.
- Inventors: Tarun Amla; Keshav Amla; Jyoti Amla
- Web page: https://patentgrep.com/patent/US20260040443A1

## CPC

- H05K 1/0366: {reinforced, e.g. by fibres, fabrics (H05K1/036 takes precedence)}
- H05K 1/024: {Dielectric details, e.g. changing the dielectric material around a transmission line}
- H05K 1/0373: {containing additives, e.g. fillers (H05K1/036 takes precedence)}
- H05K 2201/0293: Non-woven fibrous reinforcement
- H05K 2201/068: wherein the coefficient of thermal expansion is important
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

Dielectric materials including non-woven inorganic fabrics impregnated with a low-density resin are disclosed. The dielectric materials may have a thickness in a range of about 5 to about 125 microns for use in printed circuit boards.

## Claims

### Claim at position 1

1-16. (canceled)

### Claim 17

A method of making a dielectric material layer, comprising:
providing a non-woven, inorganic fabric reinforcement;
impregnating the reinforcement with a crosslinked thermosetting polymer resin;
drying the impregnated reinforcement; and
pressing the dried impregnated reinforcement to form a dielectric material layer having a thickness of less than about 125 microns.

### Claim 18 (depends on 17)

The method of claim 17, wherein the non-woven, inorganic fabric reinforcement has a thickness of less than about 220 microns.

### Claim 19 (depends on 17)

The method of claim 17, wherein the non-woven, inorganic fabric reinforcement is E-glass, S-2 Glass, R Glass, or ECR Glass, Quartz, L-glass, NE Glass, or D Glass.

### Claim 20 (depends on 17)

The method of claim 17, wherein the density of the resin is less than about 1.6 g/cc.

### Claim 21 (depends on 17)

The method of claim 17, wherein the density of the resin is less than about 1.2 g/cc.

### Claim 22 (depends on 17)

The method of claim 17, wherein the density of the resin is less than about 1.05 g/cc.

### Claim 23 (depends on 17)

The method of claim 17, further comprising controlling a thickness of the impregnated reinforcement prior to drying with a squeeze roll, slot die, doctor blade or gravure.

### Claim 24 (depends on 17)

The method of claim 17, further comprising supporting the dielectric material layer with a foil, release, or carrier film.

### Claim 25

(canceled)

### Claim 26 (depends on 17)

The method of claim 17, wherein the dielectric material layer has a thickness of less than about 100 microns.

### Claim 27 (depends on 26)

The method of claim 26, wherein the dielectric material layer has a thickness of less than about 50 microns.

### Claim 28 (depends on 27)

The method of claim 27, wherein the dielectric material layer has a thickness of less than about 25 microns.

### Claim 29 (depends on 17)

The method of claim 17, wherein the crosslinked thermosetting polymer resin is characterized by a dissipation factor (DF) of less than about 0.010.

### Claim 30 (depends on 17)

The method of claim 17, wherein the crosslinked thermosetting polymer resin further comprises at least one of a flame retardant, a curing agent, a hardener, a filler, and an additive.

### Claim 31 (depends on 17)

The method of claim 17, wherein the crosslinked thermosetting polymer resin is substantially halogen-free.

### Claim 32 (depends on 17)

The method of claim 17, wherein the crosslinked thermosetting polymer resin is a polyphenylene ether (PPE) and/or polyphenylene oxide (PPO) based crosslinked thermosetting polymer resin.

### Claim 33 (depends on 17)

The method of claim 17, wherein the dielectric material layer is characterized by a thickness reduction of at least 25% relative to a thickness of the non-woven, inorganic fabric reinforcement prior to lamination.

### Claim 34 (depends on 17)

The method of claim 17, wherein the dielectric material layer is characterized by a glass transition temperature (Tg) of greater than about 150° C.

### Claim 35 (depends on 17)

The method of claim 17, wherein the dielectric material layer is characterized by a coefficient of thermal expansion (CTE) of less than about 35 ppm in either of the planar directions over a temperature range of about 50° C. to about 220° C.

### Claim 36 (depends on 17)

The method of claim 17, wherein the dielectric material layer is characterized by a tensile modulus in the planar directions of less than about 5 GPa.

### Claim 37 (depends on 17)

The method of claim 17, wherein the dielectric material layer is characterized by a dielectric constant (DK) of less than about 3.5.

### Claim 38 (depends on 37)

The method of claim 37, wherein the dielectric material layer is characterized by a dielectric constant (DK) of less than about 3.0.

### Claim 39 (depends on 38)

The method of claim 38, wherein the dielectric material layer is characterized by a dielectric constant (DK) of less than about 2.8.