# US 2026/0036653 A1 · Preparation method of cross-shaped high-temperature three-dimensional hall sensor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0036653 A1
- Document ID: US20260036653A1
- Status: Published application
- Kind: A1
- Application number: 19/351,505
- Filed: 2025-10-07
- Published: 2026-02-05
- Earliest claimed: 2022-12-09
- Assignees: Dalian University of Technology
- Applicants: Dalian University of Technology
- Inventors: Huolin HUANG; Kaiming Ma
- Web page: https://patentgrep.com/patent/US20260036653A1

## CPC

- G01R 33/07: Hall effect devices
- G01R 33/0052: {Manufacturing aspects; Manufacturing of single devices, i.e. of semiconductor magnetic sensor chips (devices based on galvano-magnetic effect or the like H10N50/85)}
- G01R 33/0076: {Protection, e.g. with housings against stray fields}
- G01R 33/0206: {Three-component magnetometers}
- G01R: MEASURING ELECTRIC VARIABLES; MEASURING MAGNETIC VARIABLES (indicating correct tuning of resonant circuits H03J3/12)

## Abstract

A cross-shaped high-temperature three-dimensional Hall sensor includes the X column, the Y column and the Z column all made of third-generation semiconductor materials. The X column, the Y column and the Z column are vertically connected to each other. An electrode C1 and an electrode C2 are respectively arranged at two ends of the Z column. An electrode C3 and an electrode C4 are respectively arranged at two sides of the Y column. An electrode C5 and an electrode C6 are respectively arranged at two sides of the X column. The current description uses the excellent high temperature performance of the third generation semiconductor to make the sensor work in the high temperature environment, the new structure greatly reduces the volume compared with the other device packaging combined Hall sensor, and makes the sensor work in very narrow space.

## Claims

### Claim 1

A method for preparing a cross-shaped high-temperature three-dimensional Hall sensor, wherein the steps are following:
S1, material preparation: preparing third-generation semiconductor materials, cleaning the materials using acetone, ethanol, deionized water, and hydrochloric acid to remove impurities on the surface of the materials;
S2, structural etching: after developing the third-generation semiconductor materials by photolithography, using inductively coupled plasma etching equipment to etch the third-generation semiconductor materials, to etch both sides to the same depth, and preserve the electron-active region;
S3, device isolation: after photolithography development, using plasma etching or ion implantation to form isolation in the device area;
S4, electrode fabrication: after photolithography development, depositing composite metal by using an electron beam evaporation system, and using rapid thermal annealing to form ohmic contacts on the surface of the third-generation semiconductor materials;
S5, surface passivation: depositing a dielectric layer for device passivation by using any one of electron beam evaporation, magnetron sputtering, plasma-enhanced chemical vapor deposition, or atomic layer deposition;
S6, window opening: after photolithography, etching openings in the passivation layer at the electrode locations using any of magnetron sputtering, electron beam evaporation, or thermal evaporation methods to deposit metal at the electrode locations, and to create solder pads and lead wires.

### Claim 2 (depends on 1)

The method for preparing the cross-shaped high-temperature three-dimensional Hall sensor according to claim 1, wherein, in the step S1:
preparing SiC material with an electron concentration of 1e15˜1e18 cm−3, performing hydrogen etching on the material to smooth the surface, cleaning the substrate by using acetone, ethanol, deionized water to remove organic substances, using hydrochloric acid to remove oxides and metals from the surface, then rinsing with deionized water and drying with high-purity nitrogen,
or,
preparing GaN material with an electron concentration of 1e16˜1e18 cm−3, cleaning the substrate by using acetone, ethanol, deionized water to remove organic substances, using hydrochloric acid to remove oxides and metals from the surface, then rinsing with deionized water and drying with high-purity nitrogen.

### Claim 3 (depends on 2)

The method for preparing a cross-shaped high-temperature three-dimensional Hall sensor according to claim 2, wherein, in the step S4:
after photolithography development, using an electron beam evaporation system to deposit Ni/Ti/Al metal on the SiC surface, subsequently, using rapid thermal annealing in a nitrogen environment to form ohmic contacts reserving a 2˜5 μm margin around the electrode,
or,
after photolithography development, using an electron beam evaporation system to deposit Ti/Al metal on the GaN surface, subsequently, using rapid thermal annealing in a nitrogen environment to form ohmic contacts reserving a 2˜5 μm margin around the electrode.

### Claim 4 (depends on 3)

The method for preparing a cross-shaped high-temperature three-dimensional Hall sensor according to claim 3, wherein, in the step S5:
using plasma-enhanced chemical vapor deposition to deposit a SiO2 passivation layer to weaken the influence of the environment on device characteristics;
or,
using plasma-enhanced chemical vapor deposition to deposit a Si3N4 passivation layer to weaken the influence of the environment on device characteristics.