# US 2026/0035835 A1 · Methods for selectively depositing a boron doped silicon germanium layer on a surface of a substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0035835 A1
- Document ID: US20260035835A1
- Status: Published application
- Kind: A1
- Application number: 19/281,879
- Filed: 2025-07-28
- Published: 2026-02-05
- Earliest claimed: 2024-07-31
- Assignees: ASM IP Holding B.V.
- Applicants: ASM IP Holding B.V.
- Inventors: Daniel Casey; Rami Khazaka; Patricio Eduardo Romero
- Web page: https://patentgrep.com/patent/US20260035835A1

## CPC

- C30B 31/08: the diffusion materials being a compound of the elements to be diffused
- C30B 25/04: Pattern deposit, e.g. by using masks
- C30B 29/06: Silicon
- C30B 29/08: Germanium
- C30B 31/185: {Pattern diffusion, e.g. by using masks}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

Methods for selectively depositing a boron doped silicon germanium layer on a substrate disposed within a reaction chamber are disclosed. The methods disclosed include selectively depositing the boron doped silicon germanium layers by an epitaxial deposition process employing a silicon precursor, a germanium halide precursor, and a boron halide dopant precursor.

## Claims

### Claim 1

A method of selectively depositing a boron doped silicon germanium layer on a substrate disposed within a reaction chamber, the method comprising:
heating the substrate to a deposition temperature; and
depositing the boron doped silicon germanium layer on a surface of the substrate by a selective epitaxial deposition process comprising:
introducing a silicon precursor into the reaction chamber, the silicon precursor having a general formula of the form SinXmH2n+2−m, with X being selected from Cl, Br, and I, with n being an integer from at least 2 to at most 4, and with m being an integer from at least 1 to at most 2n+2−m;
introducing a germanium halide precursor into the reaction chamber; and
introducing a boron halide dopant precursor into the reaction chamber, the boron halide dopant precursor having a general formula of the form BpYqH3p-q, with Y being selected from Cl, Br, and I, with p being an integer from at least 1, and q being an integer from at least 1 to at most 3p.

### Claim 2 (depends on 1)

The method of claim 1, wherein the silicon precursor, the germanium halide precursor, and the boron halide dopant precursor are co-flowed into the reaction chamber.

### Claim 3 (depends on 2)

The method of claim 2, wherein the deposition temperature is between 250° C. and 450° C.

### Claim 4 (depends on 3)

The method of claim 3, wherein the silicon precursor comprises a chlorosilane precursor selected from a group consisting of Si2Cl5H, Si2ClH5, Si2Cl2H4, and Si3Cl8.

### Claim 5 (depends on 4)

The method of claim 4, wherein the chlorosilane precursor comprises Si2Cl5H.

### Claim 6 (depends on 3)

The method of claim 3, wherein the germanium halide precursor comprises a germanium chloride precursor.

### Claim 7 (depends on 6)

The method of claim 6, wherein the germanium chloride precursor comprises at least one of GeCl3H, GeCl4, GeClH3, GeCl2H2, and Ge2ClH5.

### Claim 8 (depends on 3)

The method of claim 3, wherein the boron halide dopant precursor comprises at least one of BH2Cl, BCl2H, BCl3, and BBr3.

### Claim 9 (depends on 3)

The method of claim 3, wherein the selective epitaxial deposition process deposits the boron doped silicon germanium layer on a surface A relative to a surface B, wherein the surface A is a semiconductor surface, and the surface B is a dielectric surface.

### Claim 10 (depends on 9)

The method of claim 9, further comprising introducing an etchant into the reaction chamber.

### Claim 11

A method of forming a boron doped silicon germanium layer on a substrate, the method comprising:
heating the substrate to a deposition temperature 250° C. and 450° C.; and
contacting the substrate with a precursor gas composition, the precursor gas composition comprising:
a silicon precursor having a general formula of the form SinClmH2n+2−m, with n being an integer from at least 2 to at most 4, and with m being an integer from at least 1 to at most 2n+2−m;
a germanium halide precursor comprising one or more of GeCl3H, GeCl4, GeClH3, GeCl2H2, and Ge2ClH5; and
a boron halide dopant precursor comprising one or more of BCl3 and BBr3.

### Claim 12 (depends on 11)

The method of claim 11, wherein the precursor gas composition consists essentially of the silicon precursor, the germanium halide precursor, and the boron halide dopant precursor.

### Claim 13 (depends on 12)

The method of claim 12, wherein the silicon precursor comprises one or more of Si2Cl5H, Si2ClH5, Si2Cl2H4, and Si3Cl8.

### Claim 14 (depends on 13)

The method of claim 13, wherein the boron doped silicon germanium layer is formed by a selective epitaxial deposition process which preferentially deposits the boron doped silicon germanium layer on a surface A relative to a surface B, wherein the surface A is a silicon surface or silicon germanium surface, and the surface B is a silicon oxide surface or a silicon nitride surface.

### Claim 15 (depends on 11)

The method of claim 11, wherein the precursor gas composition further comprises an additional germanium precursor selected from a group consisting of GeH4, Ge2H6, Ge3H8, GeH6Si, GeCl4, GeCl2, and GeCl2H2.

### Claim 16 (depends on 11)

The method of claim 11, wherein the precursor gas composition further comprises an additional silicon precursor selected from a group consisting of silanes, chlorosilanes, and iodosilanes.

### Claim 17 (depends on 11)

The method of claim 11, wherein the precursor gas composition further comprises an additional boron precursor selected from a group consisting of B2H6, B2D6, BH2Cl, BCl2H, BCl3, and BBr3.

### Claim 18

A method of forming a contact layer to a silicon germanium source/drain region, the method comprising:
seating a substrate within a reaction chamber, the substrate comprising one or more silicon germanium source/drain regions;
heating the substrate to a deposition temperature between 250° C. and 450° C.; and
depositing a boron doped silicon germanium layer directly on a surface of the silicon germanium source/drain region by a selective epitaxial deposition process by co-flowing into the reaction chamber a precursor gas composition comprising:
a silicon precursor having a general formula of the form SinXmH2n+2−m, with X being selected from Cl, Br, and I, with n being an integer from at least 2 to at most 4, and with m being an integer from at least 1 to at most 2n+2−m;
a germanium halide precursor; and
a boron halide dopant precursor having a general formula of the form BpYqH3p−q, with Y being selected from Cl, Br, and I, with p being an integer from at least 1, and q being an integer from at least 1 to at most 3p.

### Claim 19 (depends on 18)

The method of claim 18, wherein the selective epitaxial deposition process deposits the boron doped silicon germanium layer on the surface of the silicon germanium source/drain region relative to a silicon oxide surface or a silicon nitride surface.

### Claim 20 (depends on 18)

The method of claim 18 wherein the deposited boron doped silicon germanium layer has both an active dopant concentration greater than 2×1021 cm−3 and a germanium content greater than 40 atomic percent (atomic-%).