# US 2026/0035496 A1 · Aqueous photo-iniferter polymerization of polyacrylonitrile and copolymers thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0035496 A1
- Document ID: US20260035496A1
- Status: Published application
- Kind: A1
- Application number: 19/277,733
- Filed: 2025-07-23
- Published: 2026-02-05
- Earliest claimed: 2024-07-23
- Assignees: The University of Southern Mississippi
- Inventors: Tristan Clemons; Evan Stacy; Charles McCormick, IV
- Web page: https://patentgrep.com/patent/US20260035496A1

## CPC

- C08F 120/44: Acrylonitrile
- C08F 2/38: Polymerisation using regulators, e.g. chain terminating agents {, e.g. telomerisation}
- C08F 2/48: by ultraviolet or visible light
- C08F 220/46: with carboxylic acids, sulfonic acids or salts thereof
- C08F 220/48: with nitrogen-containing monomers
- D01D 5/06: Wet spinning methods {(D01D5/0046 takes precedence)}
- D01D 5/28: while mixing different spinning solutions or melts during the spinning operation; Spinnerette packs therefor
- D01F 6/18: from polymers of unsaturated nitriles, e.g. polyacrylonitrile, polyvinylidene cyanide
- C08F 2438/03: Use of a di- or tri-thiocarbonylthio compound, e.g. di- or tri-thioester, di- or tri-thiocarbamate, or a xanthate as chain transfer agent, e.g . Reversible Addition Fragmentation chain Transfer [RAFT] or Macromolecular Design via Interchange of Xanthates [MADIX]
- D10B 2321/10: polymers of unsaturated nitriles, e.g. polyacrylonitrile, polyvinylidene cyanide
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES

## Abstract

A polyacrylonitrile homopolymer, wherein the homopolymer has a number average molecular weight of from about 50,000 to about 1,000,000 g/mol, as measured by gel permeation chromatography, and a polydispersity index of from about 1.0 to about 1.5. Also disclosed is a method of making a polyacrylonitrile homopolymer, comprising mixing a)-c) to form a mixture: a) an amount of an acrylonitrile monomer; b) an amount of a chain transfer agent, and c) an amount of an aqueous solution comprising one or more components selected from the group consisting of an inorganic salts, organic salts, transition metals, and one or more organic solvents; and polymerizing the mixture via photo-iniferter reversible addition-fragmentation chain transfer (PI-RAFT) polymerization.

## Claims

### Claim 1

A polyacrylonitrile homopolymer, wherein the homopolymer has a number average molecular weight of from about 50,000 to about 1,000,000 g/mol, as measured by gel permeation chromatography, and a polydispersity index of from about 1.0 to about 1.5.

### Claim 2

A method of making a polyacrylonitrile homopolymer, comprising mixing a)-c) to form a mixture:
a) an amount of an acrylonitrile monomer;
b) an amount of a chain transfer agent, and
c) an amount of an aqueous solution comprising one or more components selected from the group consisting of an inorganic salts, organic salts, transition metals, and one or more organic solvents; and
polymerizing the mixture via photo-iniferter reversible addition-fragmentation chain transfer (PI-RAFT) polymerization.

### Claim 3 (depends on 2)

The method of claim 2, wherein the aqueous solution comprises the one or more inorganic salts selected from the group consisting of zinc salts and NaSCN, or combinations thereof.

### Claim 4 (depends on 2)

The method of claim 2, wherein the homopolymer is polymerized in the mixture having a molar ratio of acrylonitrile monomer to chain transfer agent of from about 500:1 to about 50,000:1.

### Claim 5 (depends on 2)

The method of claim 2, wherein the homopolymer is polymerized in the mixture having a molarity of the acrylonitrile monomer (mol) to the mixture (liter) of from about 0.5 mol/L to about 10 mol/L.

### Claim 6 (depends on 2)

The method of claim 2, wherein the step of polymerizing is carried out for a period of 1 hour to about 120 hours.

### Claim 7 (depends on 2)

The method of claim 2, where the aqueous solution comprises the inorganic salt, the organic salts, the transition metals, or the one or more organic solvents in an amount of from about 20 wt. % to about 80 wt. %, based on a total weight of the aqueous solution.

### Claim 8 (depends on 2)

The method of claim 2, wherein the polymerization step is carried out at a temperature of from about −25° C.-80° C.

### Claim 9 (depends on 2)

The method of claim 2, wherein the polymerization step comprises exposing the mixture to UV light irradiation.

### Claim 10 (depends on 2)

The method of claim 2, wherein the chain transfer agent is 4-(((2-carboxyethyl)thio)carbonothioyl)thio)-cyanopentanoic acid (CCPA).

### Claim 11 (depends on 2)

A polyacrylonitrile homopolymer composition formed by the method of claim 2.

### Claim 12

A polymer formed by mixing a)-d) to form a mixture:
a) an amount of an acrylonitrile monomer;
b) an amount of a comonomer, wherein the comonomer is nucleophilic;
c) an amount of a chain transfer agent; and
d) an amount of an aqueous solution comprising one or more components selected from the group consisting of inorganic salts, organic salts, transition metals, and one or more organic solvents; and
polymerizing the mixture by photo-iniferter reversible addition-fragmentation chain transfer (PI-RAFT) polymerization to form the polymer.

### Claim 13 (depends on 12)

The polymer of claim 12, wherein the comonomer is selected from the group consisting of phthalic anhydride vinyl, N-isopropylacrylamide, ethylenesulfonic acid, α-nitryl acrylic acid, α-amino acrylic acid, methyl acrylate, methyl methacrylate, acrylamide, acrylic acid, methacrylic acid, vinyl phosphoric acid, maleic anhydride, methacrylamide, 2-acrylamido-2-methyl-1-propane sulfonic acid, itaconic acid, N-isopropylacrylamide, N-vinyl formamide, N-phenylacrylateamide, N-(acryloyloxy)phthalimide, and 4-vinylphenylboronic acid.

### Claim 14 (depends on 12)

A fiber comprising the polymer of claim 12.

### Claim 15 (depends on 12)

A method of making a fiber, comprising spinning an aqueous solution comprising the polymer of claim 12, using a spinning process for forming the fiber.

### Claim 16 (depends on 15)

The method of claim 15, wherein the aqueous polymer solution has a viscosity of from about 100 Pa·s to about 1000 Pa·s, at a shear rate of 1 s−1 and a spinning temperature of 30-60° C., the aqueous polymer solution comprises 10 wt. % to 30 wt. % of the polymer, based on the total weight of the aqueous polymer solution, and the aqueous polymer solution comprises water, an organic polymer solution, a solvent, or combinations thereof.

### Claim 17 (depends on 16)

The method of claim 16, wherein the organic polymer solution comprises dimethyl sulfoxide (DMSO), dimethylformamide (DMF), dimethylacetamide (DMAc), and/or ethylene carbonate (EC).

### Claim 18 (depends on 16)

The method of claim 16, wherein the aqueous polymer solution has a viscosity of from about 100 Pa·s to about 200 Pa·s, at a shear rate of 1 s−1 at a spinning temperature of 50° C., and the aqueous polymer solution comprises 20 wt. % of the polymer, based on the total weight of the aqueous polymer solution.

### Claim 19 (depends on 18)

The method of claim 18, wherein the spinning is carried out with a multifilament wet jet spinning line.