# US 2026/0035309 A1 · Soluble ceramic shell/core and preparation method and application

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0035309 A1
- Document ID: US20260035309A1
- Status: Published application
- Kind: A1
- Application number: 19/356,032
- Filed: 2025-10-10
- Published: 2026-02-05
- Earliest claimed: 2025-01-07
- Assignees: Huazhong University of Science and Technology
- Applicants: Huazhong University of Science and Technology
- Inventors: Wenming Jiang; Ziwei Peng; Xiaopeng Yu; Qingqing Li; Linghui Yu; Taoxiong Guo; Li Yang; Zitian Fan
- Web page: https://patentgrep.com/patent/US20260035309A1

## CPC

- C04B 35/6261: {Milling}
- B33Y 10/00: Processes of additive manufacturing
- B33Y 80/00: Products made by additive manufacturing
- C04B 35/057: based on calcium oxide
- C04B 35/6263: {characterised by their solids loadings, i.e. the percentage of solids}
- C04B 35/62655: {Drying, e.g. freeze-drying, spray-drying, microwave or supercritical drying}
- C04B 35/6269: {Curing of mixtures}
- C04B 35/632: Organic additives
- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- C04B 35/6264: {Mixing media, e.g. organic solvents}
- C04B 2235/3208: Calcium oxide or oxide-forming salts thereof, e.g. lime
- C04B 2235/3225: Yttrium oxide or oxide-forming salts thereof
- C04B 2235/3244: Zirconium oxides, zirconates, hafnium oxides, hafnates, or oxide-forming salts thereof
- C04B 2235/6026: Computer aided shaping, e.g. rapid prototyping
- C04B 2235/606: Drying
- C04B 2235/616: Liquid infiltration of green bodies or pre-forms
- C04B 2235/6562: Heating rate
- C04B 2235/6567: Treatment time
- C04B 2235/6587: Influencing the atmosphere by vaporising a solid material, e.g. by using a burying of sacrificial powder
- C04B 2235/661: Multi-step sintering
- C04B 2235/80: Phases present in the sintered or melt-cast ceramic products other than the main phase
- C04B 2235/9623: Ceramic setters properties
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING

## Abstract

The present disclosure proposes a soluble ceramic shell/core and a preparation method and an application, and belongs to the technical field related to rapid casting. The preparation method includes the following steps: step S1: performing ball milling and drying on a raw material containing calcium oxide and a modifying solution to obtain a modified calcium oxide powder; step S2: printing the modified calcium oxide powder into a ceramic shell/core primary blank, and performing heat curing, infiltration and drying to obtain a ceramic shell/core blank; and step S3: sintering the ceramic shell/core blank to obtain the soluble ceramic shell/core. The present disclosure prepares the ceramic shell/core by a 3DP molding process, which is simple in procedure and short in production cycle, and does not need support, wherein solubility of the calcium oxide, after casting, makes it easier for a casting to be de-shelled. In addition, the raw material during a sintering process cannot be decomposed, which reduces shrinkage during the sintering process and can meet requirements for molding a large and complex structural ceramic shell/core.

## Claims

### Claim 1

A preparation method of a soluble ceramic shell/core, comprising the following steps:
step S1: performing ball milling and drying on a raw material containing calcium oxide and a modifying solution, and performing sieving to obtain a modified calcium oxide powder;
step S2: printing the modified calcium oxide powder into a ceramic shell/core primary blank, and performing heat curing, infiltration and drying to obtain a ceramic shell/core blank; and
step S3: sintering the ceramic shell/core blank to obtain the soluble ceramic shell/core; wherein
in the step S1, the modifying solution comprises a modifier and a modifying solvent;
the modifier is selected from at least one of ethyl bromide, bromobenzene, a silane coupling agent, stearic acid, or n-octadecyltrichlorosilane;
the modifying solvent is selected from at least one of methanol, ethanol, glycerol, or acetone;
by mass, the amount of the modifier is 1-10 parts, and the amount of the modifying solvent is 99-90 parts;
in the step S1, by mass, the amount of the calcium oxide is 30-70 parts, and the amount of the modifying solution is 70-30 parts;
in the step S1, time of the ball milling is 6 h-12 h;
in the ball milling, a diameter of a milling ball is 0.8 mm-2 mm;
in the ball milling, a mass fraction of the milling ball is 5%-15% that of the raw material;
a temperature of the drying is 50° C.-100° C., and time of the drying is 6 h-24 h; and
in the sieving after the drying, a mesh count of a sieve is 100 mesh-500 mesh.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein in the step S2, a temperature of the heat curing is 150° C.-180° C., and time of the heat curing is 2 h-5 h;
a temperature of the drying is 50° C.-90° C., and time of the drying is 8 h-24 h;
time of the infiltration is 30 s-3 min; and
in the step S2, an infiltration liquid used in the infiltration is selected from at least one of a nano-SiO2 ethanol dispersion, a nano-ZrO2 ethanol dispersion, or a nano-YiO2 ethanol dispersion.

### Claim 3 (depends on 1)

The preparation method according to claim 1, wherein in the step S2, a layer height of the printing is 0.05 mm-0.20 mm; and
an adhesive for the printing is phenolic resin, and saturation of the adhesive is 70%-140%.

### Claim 4 (depends on 1)

The preparation method according to claim 1, wherein in the step S3, the sintering comprises first sintering and second sintering;
a temperature of the first sintering is 600° C.-800° C., and time of the first sintering is 1 h-3 h;
a temperature of the second sintering is 1300° C.-1500° C., and time of the second sintering is 2 h-3 h; and
a heating rate of the sintering is 1° C./min−5° C./min.

### Claim 5 (depends on 1, 2, 3, 4)

A soluble ceramic shell/core prepared and obtained by the preparation method according to any one of claims 1-4.

### Claim 6 (depends on 5)

An application of the soluble ceramic shell/core according to claim 5 in a cast structural member, wherein a material of the cast structural member is selected from at least one of cast iron, cast steel, an aluminum alloy, a titanium alloy, or a magnesium alloy.