# US 2026/0028690 A1 · Steel board for polar marine engineering and preparation method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0028690 A1
- Document ID: US20260028690A1
- Status: Published application
- Kind: A1
- Application number: 19/349,735
- Filed: 2025-10-03
- Published: 2026-01-29
- Earliest claimed: 2020-08-17
- Assignees: Shadong Iron and Steel Co., Ltd
- Applicants: Laiwu Steel Yinshan Section Co., Ltd.
- Inventors: Heng MA; Zhongxue WANG; Tengfei WANG; Yuexiang WANG; Zhengxu SUN; Qingpu ZHANG; Kang HE; Pei ZHANG; Xuaoxin HUO
- Web page: https://patentgrep.com/patent/US20260028690A1

## CPC

- C21D 9/0081: {for slabs; for billets}
- C21C 5/30: Regulating or controlling the blowing
- C21C 7/0006: {Adding metallic additives}
- C21C 7/0056: {using cored wires}
- C21C 7/06: Deoxidising, e.g. killing
- C21C 7/064: Dephosphorising; Desulfurising
- C21C 7/10: Handling in a vacuum
- C21D 1/02: Hardening articles or materials formed by forging or rolling, with no further heating beyond that required for the formation
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0263: {following hot rolling}
- C21D 9/46: for sheet metals
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- Y02P 10/20: Recycling
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C21C: PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for preparing a steel board for polar marine engineering is provided. Components of the steel board in terms of mass percentage comprise: C: 0.06-0.09%, Si: 0.20-0.35%, Mn: 1.48-1.63%, Nb: 0.020%-0.035%, Ti: 0.010%-0.020%, V: 0.020%-0.035%, Ni. 0.08%-0.17%, Als: 0.015%-0.040%, P: ≤0.013%, S: ≤0.005%, N: ≤0.006%, B: ≤0.005%, the rest are Fe and unavoidable impurities; and CEV≤0.39%, Pcm≤0.20%, wherein: CEV=C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15, and Pcm=C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B≤0.20%. The method includes primary refining of molten steel and scrap to obtain a primary molten steel, then refining the primary molten steel and casting to obtain a cast billet, then slowly cooling the cast billet. The method further includes heating the cast billet after the slow cooling to obtain a hot cast billet, rolling the hot cast billet to obtain the steel board, and cooling the steel board to obtain the steel board for polar marine engineering.

## Claims

### Claim 1

A method for preparing a steel board for polar marine engineering, components of the steel board in terms of mass percentage comprising: C: 0.06-0.09%, Si: 0.20-0.35%, Mn: 1.48-1.63%, Nb: 0.020%-0.035%, Ti: 0.010%-0.020%, V: 0.020%-0.035%, Ni. 0.08%-0.17%, Als: 0.015%-0.040%, P: ≤0.013%, S: ≤0.005%, N: ≤0.006%, B: ≤0.005%, the rest are Fe and unavoidable impurities; and CEV≤0.39%, Pcm≤0.20%, wherein: CEV=C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15, and Pcm=C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B≤0.20%, the method comprising:
primary refining of molten steel and scrap to obtain a primary molten steel, then refining the primary molten steel and casting to obtain a cast billet, then slowly cooling the cast billet;
heating the cast billet after the slow cooling to obtain a hot cast billet;
rolling the hot cast billet to obtain the steel board; and
cooling the steel board to obtain the steel board for polar marine engineering.

### Claim 2 (depends on 1)

The method for preparing the steel board for polar marine engineering according to claim 1, wherein, the primary refining is carried out under top-bottom combined blowing converter conditions, the molten steel is desulfurized using KR pretreatment, with the molten steel containing ≤0.015 wt. % sulfur after desulfurization.

### Claim 3 (depends on 1)

The method for preparing the steel board for polar marine engineering according to claim 1, wherein
the refining is LF+RH refining.

### Claim 4 (depends on 1)

The method for preparing the steel board for polar marine engineering according to claim 1, wherein
during the casting, the whole process is protected casting, a liquidus temperature is 1515-1525° C., superheat is required to be not more than 17° C., a light press down technique is used at a solidification end of the cast billet in a sector section, and the cast billet is slowly cooled in a pit and stack for not less than 60 hours.

### Claim 5 (depends on 1)

The method for preparing the steel board for polar marine engineering according to claim 1, wherein
during the heating, the heating rate is greater than 10 mins/cm and a uniform heat time is not less than 40 mins; after heating of the cast billet, the hot cast billet is subjected to high pressure water phosphorus removal.

### Claim 6 (depends on 1)

The method of preparing the steel board for polar marine engineering according to claim 1, wherein the rolling includes a two-stage controlled rolling of roughing rolling and finishing rolling, the roughing rolling being a recrystallization zone rolling and the finishing rolling being an unrecrystallized zone rolling.

### Claim 7 (depends on 1)

The method for preparing the steel board for polar marine engineering according to claim 1, wherein the cooling includes air cooling when a thickness of the steel board is 6-14 mm.

### Claim 8 (depends on 1)

The method for preparing the steel board for polar marine engineering according to claim 1, wherein, the primary refining is carried out under top-bottom combined blowing converter conditions; prior to the primary refining, the molten steel is desulfurized using KR pretreatment, with the molten steel containing ≤0.015 wt. % sulfur after desulfurization,
the scrap/(molten steel+scrap)≤8 wt. %, and nickel plate is added with the scrap,
the primary refining is carried out using a double slag process, with a final slag alkalinity of a second slag-making smelting controlled at R=3.0-4.0, with a single catch carbon, with slag material added 3-4 mins before an end of the primary refining; ferro-manganese aluminum is added in a forepart of a steel tapping phase to deoxidation, and manganese metal, ferro-niobium, ferro-vanadium and ferrosilicon alloy are added when the primary molten steel is out to one-fourth steel tapping to three quarters of a time to add finished.

### Claim 9 (depends on 1)

The method for preparing the steel board for polar marine engineering according to claim 1, wherein
the refining is LF+RH refining, and includes bottom-blowing argon adopted in the whole process for stirring, aluminum particles, calcium carbide are used for deoxidation, a top slag before leaving a station is yellow-white slag or white slag, the yellow-white slag or the white slag holding time is not less than 10 mins, a titanium line is fed at the end of the refining, a final slag alkalinity amount is controlled above 2.5,
during the LF refining, a composition is fine-tuned using metallic manganese, ferrosilicon, ferro-niobium and ferro-vanadium alloys, and
in the RH refining, a degassing time is not less than 5 mins and a calcium-aluminum line is fed for calcification, soft blowing is carried out before leaving the station, and the soft blowing time is not less than 12 mins.

### Claim 10 (depends on 1)

The method of preparing the steel board for polar marine engineering according to claim 1, wherein the rolling includes a two-stage controlled rolling of roughing rolling and finishing rolling, the roughing rolling being a recrystallization zone rolling and the finishing rolling being an unrecrystallized zone rolling, and an opening rolling temperature of the finishing rolling is 860 to 960° C. and a final rolling temperature of the finishing rolling is 820-840° C.

### Claim 11 (depends on 1)

The method for preparing the steel board for polar marine engineering according to claim 1, wherein the cooling includes air cooling when a thickness of the steel board is 6-14 mm, and when the thickness of the steel board is 14-40 mm, the cooling is ACC water cooling with an inlet water temperature of 770-780° C. and an outlet water temperature of 600-650° C., after water cooling, the steel board is straightened.

### Claim 12 (depends on 2)

The method for preparing the steel board for polar marine engineering according to claim 2, wherein
during the heating, the heating rate is greater than 10 mins/cm and a uniform heat time is not less than 40 mins; after heating of the cast billet, the hot cast billet is subjected to high pressure water phosphorus removal.

### Claim 13 (depends on 2)

The method of preparing steel board for polar marine engineering according to claim 2, wherein the rolling includes a two-stage controlled rolling of roughing rolling and finishing rolling, the roughing rolling being a recrystallization zone rolling and the finishing rolling being an unrecrystallized zone rolling.

### Claim 14 (depends on 2)

The method for preparing steel board for polar marine engineering according to claim 2, wherein the cooling includes air cooling when a thickness of the steel board is 6-14 mm.