# US 2026/0028688 A1 · Fired pellets for reduction and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0028688 A1
- Document ID: US20260028688A1
- Status: Published application
- Kind: A1
- Application number: 18/994,444
- Filed: 2022-08-01
- Published: 2026-01-29
- Earliest claimed: 2022-08-01
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Kenta TAKEHARA; Tetsuya YAMAMOTO; Takahide HIGUCHI; Yuji IWAMI; Shohei FUJIWARA; Yuya MORITA; Kenya HORITA; Toshiyuki HIROSAWA; Daisuke IGAWA
- Web page: https://patentgrep.com/patent/US20260028688A1

## CPC

- C21B 13/0086: {Conditioning, transformation of reduced iron ores}
- C22B 1/243: inorganic
- C21B 13/0046: {making metallised agglomerates or iron oxide}
- C21B 13/008: {Use of special additives or fluxing agents}
- C21B 13/105: {Rotary hearth-type furnaces}
- C22B 1/2406: {pelletizing}
- C21B: MANUFACTURE OF IRON OR STEEL (preliminary treatment of ferrous ores or scrap C22B1/00)
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS

## Abstract

Fired pellets for use in a solid reduction furnace that are effective in preventing clustering by reducing the possibility of contact between low-melting-temperature slags and thus preventing the fusion therebetween, and a method for producing such fired pellets. Fired pellets for reduction, wherein the proportion of high-viscosity slag components (Al2O3+MgO+SiO2) to the total Fe (T.Fe) satisfies an expression: (Al2O3+MgO+SiO2)/T.Fe≥0.09, and a method for producing the same. In the expression, Al2O3 represents the concentration (mass %) of Al2O3 in the fired pellets, MgO represents the concentration (mass %) of MgO in the fired pellets, SiO2 represents the concentration (mass %) of SiO2 in the fired pellets, and T.Fe represents the concentration (mass %) of T.Fe in the fired pellets.

## Claims

### Claim 1

Fired pellets for reduction,
wherein
a proportion of high-viscosity slag components (Al2O3+MgO+SiO2) to total Fe (T.Fe) satisfies the following Expression (1):
(
Al
2
⁢
O
3
+
MgO
+
SiO
2
)
/
T
.
Fe
≥
0.09
,
(
1
)
where Al2O3 represents a concentration (mass %) of Al2O3 in the fired pellets,
MgO represents a concentration (mass %) of MgO in the fired pellets,
SiO2 represents a concentration (mass %) of SiO2 in the fired pellets, and
T.Fe represents a concentration (mass %) of T.Fe in the fired pellets.

### Claim 2

Fired pellets for reduction,
wherein
a proportion of high-viscosity slag components (Al2O3+MgO+SiO2) to total Fe (T.Fe) satisfies the following Expression (2):
(
Al
2
⁢
O
3
+
MgO
+
SiO
2
)
/
T
.
Fe
≥
0.12
,
(
2
)
where Al2O3 represents a concentration (mass %) of Al2O3 in the fired pellets,
MgO represents a concentration (mass %) of MgO in the fired pellets,
SiO2 represents a concentration (mass %) of SiO2 in the fired pellets, and
T.Fe represents a concentration (mass %) of T.Fe in the fired pellets.

### Claim 3 (depends on 1)

The fired pellets for reduction according to claim 1,
wherein a porosity is 20% or more.

### Claim 4 (depends on 1)

The fired pellets for reduction according to claim 1,
wherein a porosity is 30% or more.

### Claim 5 (depends on 1)

A method for producing the fired pellets for reduction according to claim 1, wherein
reduction and firing are performed by using an iron-containing raw material formulated to achieve an average LOI (Loss on Ignition) of 5% or more.

### Claim 6 (depends on 5)

The method for producing the fired pellets for reduction according to claim 5, wherein
the iron-containing raw material has been subjected to a crystal water removal pretreatment in advance so as to achieve an average LOI (Loss on Ignition) of 2% or less.

### Claim 7 (depends on 6)

The method for producing the fired pellets for reduction according to claim 6, wherein
the crystal water removal pretreatment comprises heating and drying using a rotary kiln and using a measurement value of a sample at the exit side of the kiln as the average LOI (Loss on Ignition) of the iron-containing raw material.

### Claim 8 (depends on 5)

The method for producing the fired pellets for reduction according to claim 5, wherein
a mixed raw material containing 4 mass % to 24 mass % M.Fe is prepared by mixing a raw material containing M.Fe, and the mixed raw material is granulated and fired.

### Claim 9 (depends on 8)

The method for producing t fired pellets for reduction according to claim 8, wherein
the raw material is reduced iron having a particle size of 3 mm or less that has been reduced in a solid reduction furnace.

### Claim 10 (depends on 9)

The method for producing the fired pellets for reduction according to claim 9, wherein
the reduced iron contains 78 mass % or more M.Fe.