# US 2026/0028128 A1 · Ice protection coating and bonding methods thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0028128 A1
- Document ID: US20260028128A1
- Status: Published application
- Kind: A1
- Application number: 19/087,725
- Filed: 2025-03-24
- Published: 2026-01-29
- Earliest claimed: 2021-03-09
- Assignees: The Boeing Company
- Applicants: The Boeing Company
- Inventors: Edward Brouwers; Andrew Nowak; Dimitrios Priftis; Michael Jared Ventuleth; Kenneth W. Young
- Web page: https://patentgrep.com/patent/US20260028128A1

## CPC

- B64D 15/00: De-icing or preventing icing on exterior surfaces of aircraft
- C09D 5/16: Antifouling paints; Underwater paints
- C09D 175/04: Polyurethanes
- C09J 163/00: Adhesives based on epoxy resins; Adhesives based on derivatives of epoxy resins
- C09K 3/18: for application to surfaces to minimize adherence of ice, mist or water thereto (rendering particulate materials free flowing, in general, e.g. making them hydrophobic B01J2/30); Thawing or antifreeze materials for application to surfaces (used in liquids for heat-transfer, heat-exchange or heat-storage or for the production of heat or cold other than by combustion, e.g. radiator liquids, C09K5/00)
- C09J 2203/35: for aeronautic or naval applications
- C09J 2301/302: the adhesive being pressure-sensitive, i.e. tacky at temperatures inferior to 30°C
- B64D: EQUIPMENT FOR FITTING IN OR TO AIRCRAFT; FLIGHT SUITS; PARACHUTES; ARRANGEMENT OR MOUNTING OF POWER PLANTS OR PROPULSION TRANSMISSIONS IN AIRCRAFT
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

A method for bonding an icephobic coating layer to an exterior surface of a substrate, the method including roughening the exterior surface of the substrate to provide a roughened substrate surface; roughening a backside surface of the icephobic coating layer to provide a roughened icephobic coating surface; placing an epoxy film adhesive layer on the roughened substrate surface to cover at least part of the exterior surface of the substrate; placing the roughened icephobic coating layer on the epoxy film adhesive layer such that the roughened icephobic coating surface is in contact with the epoxy film adhesive layer, thereby providing a layered stack; enclosing the layered stack in a vacuum bag; applying a vacuum to the vacuum bag, and heating the layered stack enclosed in the vacuum bag; cooling the layered stack; releasing the vacuum; and removing the layered stack from the vacuum bag to provide an icephobic-coated substrate.

## Claims

### Claim 1

A method for bonding an icephobic coating layer to an exterior surface of a substrate, the method comprising:
roughening the exterior surface of the substrate to provide a roughened substrate surface;
roughening a backside surface of the icephobic coating layer to provide a roughened icephobic coating surface;
placing an epoxy film adhesive layer on the roughened substrate surface to cover at least part of the exterior surface of the substrate;
placing the roughened icephobic coating layer on the epoxy film adhesive layer such that the roughened icephobic coating surface is in contact with the epoxy film adhesive layer, thereby providing a layered stack;
enclosing the layered stack in a vacuum bag;
applying a vacuum to the vacuum bag, and heating the layered stack enclosed in the vacuum bag;
cooling the layered stack;
releasing the vacuum; and
removing the layered stack from the vacuum bag to provide an icephobic-coated substrate.

### Claim 2 (depends on 1)

The method of claim 1, wherein an abrasive pad is used to roughen the exterior surface of the substrate.

### Claim 3 (depends on 1)

The method of claim 1, wherein an abrasive pad is used to roughen the backside surface of the icephobic coating layer.

### Claim 4 (depends on 3)

The method of claim 3, further comprising placing a release film layer on top of the icephobic coating layer before the step of applying the vacuum.

### Claim 5 (depends on 4)

The method of claim 4, further comprising placing a porous breather layer on a top of the release film layer before the step of applying the vacuum.

### Claim 6 (depends on 1)

The method of claim 1,
wherein the layered stack is heated in the vacuum bag at a rate of about 5° F./min until a temperature of about 245° F. is reached; and
wherein the layered stack is held at a temperature of about 245° F. for about 90 minutes.

### Claim 7 (depends on 6)

The method of claim 6, wherein the layered stack is cooled, after heating for about 90 minutes, at a rate of about 5° F./min until room temperature is reached.

### Claim 8 (depends on 1)

The method of claim 1, wherein the exterior surface comprises at least a part of an airfoil.

### Claim 9

A method for bonding an icephobic coating layer to an exterior surface of a substrate, the method comprising:
roughening the exterior surface of the substrate to provide a roughened substrate surface;
roughening a backside surface of the icephobic coating layer to provide a roughened icephobic coating layer surface;
placing a pressure sensitive adhesive film layer on the roughened icephobic coating layer surface;
placing the icephobic coating layer and the pressure sensitive adhesive film layer on the roughened substrate surface such that the pressure sensitive adhesive film layer is in contact with the roughened substrate surface, thereby providing a layered stack;
enclosing the layered stack in a vacuum bag;
applying a vacuum to the layered stack enclosed in the vacuum bag;
releasing the vacuum; and
removing the layered stack from the vacuum bag to provide an icephobic-coated substrate.

### Claim 10 (depends on 9)

The method of claim 9, wherein an abrasive pad is used to roughen the exterior surface of the substrate.

### Claim 11 (depends on 10)

The method of claim 10, wherein an abrasive pad is used to roughen the backside surface of the icephobic coating layer.

### Claim 12 (depends on 11)

The method of claim 11, further comprising applying the pressure sensitive adhesive film layer to the roughened icephobic coating layer surface using a non-stick liquid mixture comprising water, isopropanol, and soap.

### Claim 13

A method for bonding an icephobic coating layer to an exterior surface of an airfoil, the method comprising:
roughening the exterior surface of the airfoil to provide a roughened airfoil surface;
roughening a backside surface of the icephobic coating layer to provide a roughened icephobic coating surface;
placing an epoxy film adhesive layer on the roughened airfoil surface to cover at least a part of the exterior surface of the airfoil;
placing the roughened icephobic coating layer on the epoxy film adhesive layer such that the roughened icephobic coating surface is in contact with the epoxy film adhesive layer, thereby providing a layered stack;
enclosing the layered stack in a vacuum bag;
applying a vacuum to the vacuum bag, and heating the layered stack enclosed in the vacuum bag;
cooling the layered stack;
releasing the vacuum; and
removing the layered stack from the vacuum bag to provide an icephobic-coated airfoil;
wherein the icephobic coating layer comprises:
a first polymer;
a second polymer that is a fluoropolymer;
an isocyanate; and
a curative composition.

### Claim 14 (depends on 13)

The method of claim 13, wherein the fluoropolymer is a perfluoropolyether.

### Claim 15 (depends on 13)

The method of claim 13, wherein the first polymer is a polyester, a polyether, or poly(ethylene glycol).

### Claim 16 (depends on 13)

The method of claim 13, wherein the curative composition comprises a polyol, a polyamine, or a mixture thereof.

### Claim 17 (depends on 13)

The method of claim 13, wherein the icephobic coating layer further comprises one or more of a particulate filler, a pigment, a dye, a plasticizer, a flame retardant, a flattening agent, or a substrate adhesion promoter, or combinations thereof.

### Claim 18 (depends on 13)

The method of claim 13, wherein the icephobic coating layer further comprises a tin catalyst.

### Claim 19 (depends on 18)

The method of claim 18, wherein the tin catalyst is dibutyltin dilaurate.

### Claim 20 (depends on 13)

The method of claim 13, wherein the icephobic coating layer further comprises a solvent that is selected from an ester solvent, ethyl acetate, n-butyl acetate, toluene, a fluorinated solvent, 4-chlorobenzotrifluoride, 1,3-bis(trifluoromethyl)benzene, or a mixture thereof.