# US 2026/0027641 A1 · Electric resistance welded steel pipe or tube and production method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0027641 A1
- Document ID: US20260027641A1
- Status: Published application
- Kind: A1
- Application number: 18/994,849
- Filed: 2023-05-22
- Published: 2026-01-29
- Earliest claimed: 2022-09-09
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Akihide MATSUMOTO; Shinsuke IDE
- Web page: https://patentgrep.com/patent/US20260027641A1

## CPC

- B23K 11/002: {specially adapted for particular articles or work}
- C22C 38/02: containing silicon
- C21D 1/02: Hardening articles or materials formed by forging or rolling, with no further heating beyond that required for the formation
- C21D 7/10: of the whole cross-section, e.g. of concrete reinforcing bars
- C21D 8/10: during manufacturing of tubular bodies
- C21D 9/08: for tubular bodies or pipes
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/04: containing manganese
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- C22C 38/22: with molybdenum or tungsten
- C22C 38/24: with vanadium
- C22C 38/26: with niobium or tantalum
- C22C 38/28: with titanium or zirconium
- C22C 38/38: with more than 1.5% by weight of manganese
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/54: with boron
- F16L 9/17: obtained by bending a sheet longitudinally and connecting the edges
- B21C 37/08: Making tubes with welded or soldered seams {(with helically arranged seams B21C37/122)}
- B21C 37/30: Finishing tubes, e.g. sizing, burnishing
- B23K 11/0873: {of the longitudinal seam of tubes}
- B23K 2101/10: Pipe-lines
- C21D 2211/002: Bainite
- C21D 2211/005: Ferrite
- Y02P 10/20: Recycling
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- F16L: PIPES; JOINTS OR FITTINGS FOR PIPES; SUPPORTS FOR PIPES, CABLES OR PROTECTIVE TUBING; MEANS FOR THERMAL INSULATION IN GENERAL
- B21C: MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES, PROFILES OR LIKE SEMI-MANUFACTURED PRODUCTS OTHERWISE THAN BY ROLLING; AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKING WITHOUT ESSENTIALLY REMOVING MATERIAL
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided is a high-strength electric resistance welded steel pipe or tube having excellent SSC resistance. An absolute value of circumferential residual stress on a pipe or tube inner surface of the electric resistance welded steel pipe or tube is 10 MPa or more, and an absolute value of shear residual stress on the pipe or tube inner surface is 300 MPa or less. In a steel microstructure at a wall thickness center of a base metal portion of the electric resistance welded steel pipe or tube, a total volume fraction of ferrite and bainite is 90% or more and an average crystal grain size is 9.0 um or less. In a steel microstructure at a position 0.1 mm radially outward from the pipe or tube inner surface of the base metal portion, a total volume fraction of ferrite and bainite is 95% or more.

## Claims

### Claim 1

An electric resistance welded steel pipe or tube comprising a base metal portion and an electric resistance weld portion,
wherein an absolute value of circumferential residual stress on a pipe or tube inner surface of the electric resistance welded steel pipe or tube is 10 MPa or more,
an absolute value of shear residual stress on the pipe or tube inner surface is 300 MPa or less,
in a steel microstructure at a wall thickness center of the base metal portion, a total volume fraction of ferrite and bainite is 90% or more and an average crystal grain size at the wall thickness center is 9.0 μm or less, and
in a steel microstructure at a position 0.1 mm radially outward from the pipe or tube inner surface of the base metal portion, a total volume fraction of ferrite and bainite is 95% or more.

### Claim 2 (depends on 1)

The electric resistance welded steel pipe or tube according to claim 1, wherein a chemical composition of the base metal portion contains, in mass %,
C: 0.020% or more and 0.150% or less,
Si: 0.01% or more and 0.50% or less,
Mn: 0.30% or more and 2.00% or less,
P: 0.050% or less,
S: 0.0200% or less,
Al: 0.005% or more and 0.100% or less, and
N: 0.0100% or less,
with a balance consisting of Fe and inevitable impurities.

### Claim 3 (depends on 2)

The electric resistance welded steel pipe or tube according to claim 2, wherein the chemical composition further contains, in mass %, one or more selected from
Nb: 0.100% or less,
V: 0.100% or less,
Ti: 0.150% or less,
Cr: 1.00% or less,
Mo: 1.00% or less,
Cu: 1.00% or less,
Ni: 1.00% or less,
Ca: 0.0100% or less, and
B: 0.0100% or less.

### Claim 4 (depends on 1)

A production method for the electric resistance welded steel pipe or tube according to claim 1, the production method comprising:
heating a steel material to a heating temperature of 1100° C. or more and 1300° C. or less and then subjecting the steel material to hot rolling with a rolling finish temperature of 750° C. or more and 850° C. or less;
thereafter performing cooling with an average cooling rate at a sheet thickness center of 10° C./s or more and 60° C./s or less, a cooling stop temperature at the sheet thickness center of 450° C. or more and 650° C. or less, and a cooling stop temperature at a sheet surface of 250° C. or more and 500°° C. or less to obtain a hot-rolled steel sheet;
thereafter forming the hot-rolled steel sheet into a cylinder by cold roll forming and butting and electric resistance welding both circumferential ends of the cylinder together;
thereafter obtaining an electric resistance welded steel pipe or tube material using a sizing roll that satisfies the following formula (1); and
thereafter applying an internal pressure p in MPa that satisfies the following formula (2) to an inner surface of the electric resistance welded steel pipe or tube material to obtain an electric resistance welded steel pipe or tube,
(
a
⁢
diameter
⁢
in
⁢
mm
⁢
of
⁢
the
⁢
sizing
⁢
roll
)
≥
(
a
⁢
sheet
⁢
thickness
⁢
in
⁢
mm
⁢
of
⁢
the
⁢
hot
-
rolled
⁢
steel
⁢
sheet
)
/
0.02
(
1
)
X
<
p
≤
X
×
1.5
(
2
)
where X=((a wall thickness in mm of the electric resistance welded steel pipe or tube material)/(a radius in mm of the electric resistance welded steel pipe or tube material))×(a yield stress in MPa of the electric resistance welded steel pipe or tube material).

### Claim 5 (depends on 2)

A production method for the electric resistance welded steel pipe or tube according to claim 2, the production method comprising:
heating a steel material to a heating temperature of 1100° C. or more and 1300° C. or less and then subjecting the steel material to hot rolling with a rolling finish temperature of 750°° C. or more and 850° C. or less;
thereafter performing cooling with an average cooling rate at a sheet thickness center of 10° C./s or more and 60° C./s or less, a cooling stop temperature at the sheet thickness center of 450° C. or more and 650° C. or less, and a cooling stop temperature at a sheet surface of 250° C. or more and 500° C. or less to obtain a hot-rolled steel sheet;
thereafter forming the hot-rolled steel sheet into a cylinder by cold roll forming and butting and electric resistance welding both circumferential ends of the cylinder together;
thereafter obtaining an electric resistance welded steel pipe or tube material using a sizing roll that satisfies the following formula (1); and
thereafter applying an internal pressure p in MPa that satisfies the following formula (2) to an inner surface of the electric resistance welded steel pipe or tube material to obtain an electric resistance welded steel pipe or tube,
(
a
⁢
diameter
⁢
in
⁢
mm
⁢
of
⁢
the
⁢
sizing
⁢
roll
)
≥
(
a
⁢
sheet
⁢
thickness
⁢
in
⁢
mm
⁢
of
⁢
the
⁢
hot
-
rolled
⁢
steel
⁢
sheet
)
/
0.02
(
1
)
X
<
p
≤
X
×
1.5
(
2
)
where X=((a wall thickness in mm of the electric resistance welded steel pipe or tube material)/(a radius in mm of the electric resistance welded steel pipe or tube material))×(a yield stress in MPa of the electric resistance welded steel pipe or tube material).

### Claim 6 (depends on 3)

A production method for the electric resistance welded steel pipe or tube according to claim 3, the production method comprising:
heating a steel material to a heating temperature of 1100° C. or more and 1300° C. or less and then subjecting the steel material to hot rolling with a rolling finish temperature of 750° C. or more and 850° C. or less;
thereafter performing cooling with an average cooling rate at a sheet thickness center of 10° C./s or more and 60° C./s or less, a cooling stop temperature at the sheet thickness center of 450° C. or more and 650° C. or less, and a cooling stop temperature at a sheet surface of 250° C. or more and 500° C. or less to obtain a hot-rolled steel sheet;
thereafter forming the hot-rolled steel sheet into a cylinder by cold roll forming and butting and electric resistance welding both circumferential ends of the cylinder together;
thereafter obtaining an electric resistance welded steel pipe or tube material using a sizing roll that satisfies the following formula (1); and
thereafter applying an internal pressure p in MPa that satisfies the following formula (2) to an inner surface of the electric resistance welded steel pipe or tube material to obtain an electric resistance welded steel pipe or tube,
(
a
⁢
diameter
⁢
in
⁢
mm
⁢
of
⁢
the
⁢
sizing
⁢
roll
)
≥
(
a
⁢
sheet
⁢
thickness
⁢
in
⁢
mm
⁢
of
⁢
the
⁢
hot
-
rolled
⁢
steel
⁢
sheet
)
/
0.02
(
1
)
X
<
p
≤
X
×
1.5
(
2
)
where X=((a wall thickness in mm of the electric resistance welded steel pipe or tube material)/(a radius in mm of the electric resistance welded steel pipe or tube material))×(a yield stress in MPa of the electric resistance welded steel pipe or tube material).