# US 2026/0022050 A1 · Hot joining process for producing complex light-weight structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0022050 A1
- Document ID: US20260022050A1
- Status: Published application
- Kind: A1
- Application number: 18/996,372
- Filed: 2023-07-19
- Published: 2026-01-22
- Earliest claimed: 2022-07-19
- Assignees: Schott AG
- Applicants: Schott AG
- Inventors: Ralf Jedamzik; Clemens Kunisch; Hauke Esemann; Peter Daniel Hohmann; Martin Schäfer; Jürgen Vogt; Rudolf Müller
- Web page: https://patentgrep.com/patent/US20260022050A1

## CPC

- C03B 23/20: Uniting glass pieces by fusing without substantial reshaping
- C03B 23/0013: {by pressing (C03B21/04, C03B23/02, C03B23/04, C03B23/18, C03B23/26 take precedence)}
- C03B 32/02: Thermal crystallisation, e.g. for crystallising glass bodies into glass-ceramic articles {(C03B27/012 takes precedence)}
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

The invention relates to a method for producing a glass-ceramic composite object, and a glass-ceramic composite object produced from at least two starting elements. In the method, respective surfaces of at least two starting elements consisting of the precursor glass of the glass-ceramic material are pressed flat and directly against one another with the application of pressure, and at a temperature at which the ceramisation of the glass-ceramic material takes place they are joined so as to create a monolithic bond between the at least two starting elements.

## Claims

### Claim at position 1

1-14. (canceled)

### Claim 15

A process for producing a glass-ceramic composite body having a coefficient of thermal expansion CTE in a range from 0 to 50° C. of not more than 0±0.1×10−6/K, the method comprising:
providing at least two starting elements consisting of a green glass of a glass-ceramic;
arranging the at least two starting elements and contacting surfaces of the starting elements to be bonded;
two-dimensionally pressing the surfaces of the at least two starting elements to be bonded to one another under the action of pressure; and
creating a monolithic bond between the at least two starting elements by heating, under the action of pressure, the at least two starting elements pressed to one another to a temperature Tx at which ceramization of the green glass to the glass-ceramic takes place.

### Claim 16 (depends on 15)

The process of claim 15, wherein the surfaces of the at least two starting elements to be bonded are provided with a flatness of less than 300 μm and/or greater than 20 μm.

### Claim 17 (depends on 15)

The process of claim 15, further comprising the step of controlled geometric deformation of at least one of the at least two starting elements at a temperature between Tg and Tg+Ts by sagging into a target shape.

### Claim 18 (depends on 15)

The process of claim 15, further comprising the step of processing at least one of the at least two starting elements by water-jet cutting, CNC processing and/or sandblasting.

### Claim 19 (depends on 15)

The process of claim 15, wherein at least one of the at least two starting elements has a surface interrupted by cavities and/or at least one of the at least two starting elements has a plate- or disk-shaped form.

### Claim 20 (depends on 15)

The process of claim 15, wherein the pressure is generated by at least one added weight in a two-dimensional arrangement on or above at least one of the at least two starting elements and/or wherein the pressure is generated by a vacuum on the green glass structure.

### Claim 21 (depends on 15)

The process of claim 15, wherein at least one of the at least two starting elements has a diameter and/or an edge length of at least 400 mm.

### Claim 22 (depends on 1)

A monolithic composite body which has a coefficient of thermal expansion CTE in the range from 0 to 50° C. of not more than 0±0.1×10−6/K, and which is produced by the process of claim 1.

### Claim 23 (depends on 22)

The composite body of claim 22, having a diameter or an edge length of at least 400 mm.

### Claim 24 (depends on 22)

The composite body of claim 22, wherein at least one of the at least two starting elements is a reinforcing element and/or at least one of the at least two starting elements is a functional element.

### Claim 25 (depends on 24)

The composite body of claim 24, wherein mechanical stresses in a bonding region of the surface of the reinforcing element and the surface of the functional element are configured such that a stress of less than 20 nm/cm is measurable by stress birefringence measurement.

### Claim 26 (depends on 24)

The composite body of claim 24, wherein at least one of the following is satisfied:
an averaged density of the reinforcing element is less than 0.3 g/cm3;
an averaged density of the composite body is less than 0.5 g/cm3; or
a ratio V=H·B/d2 is in a range from 100 to 2500, wherein H denotes a height of the reinforcing element, B denotes a width of the reinforcing element, and d denotes a thickness of inner walls of the reinforcing element.

### Claim 27 (depends on 22)

The composite body of claim 22, wherein the surface of one of the at least two starting elements is cohesively bonded to the surface of at least one other one of the at least two starting elements such that crystallites have grown through a bonding surface formed by the two surfaces and penetrate both surfaces.

### Claim 28 (depends on 22)

The composite body of claim 22, wherein the composite body is a lightweight mirror.