# US 2026/0022028 A1 · Sodium battery positive electrode material and preparation method therefor, positive electrode sheet and sodium battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0022028 A1
- Document ID: US20260022028A1
- Status: Published application
- Kind: A1
- Application number: 19/249,634
- Filed: 2025-06-25
- Published: 2026-01-22
- Earliest claimed: 2022-12-29
- Assignees: BYD Company Limited
- Applicants: BYD Company Limited
- Inventors: Mingxue Wang; Xiaoqiang Yin; Xiangyu Li; Lina Jin
- Web page: https://patentgrep.com/patent/US20260022028A1

## CPC

- C01G 31/04: Halides
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/1397: of electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/366: {as layered products}
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/625: {Carbon or graphite}
- H01M 10/054: Accumulators with insertion or intercalation of metals other than lithium, e.g. with magnesium or aluminium
- C01P 2002/82: by IR- or Raman-data
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/62: Submicrometer sized, i.e. from 0.1-1 micrometer
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- C01P 2004/80: Particles consisting of a mixture of two or more inorganic phases
- C01P 2006/40: Electric properties
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided are sodium battery positive electrode materials and preparation methods therefor, positive electrode sheets and sodium batteries. The positive electrode materials may comprise a core and a coating layer coating the surface of the core, where the general molecular formula of the core comprises Na3V2-xMx(PO4)2F3, wherein M represents a doping element capable of replacing V, element M comprises at least one of Fe, Cr, Mn, Co, Ti, Ni, Cu, Zn, Mo, Nb, Zr, La and Ce, and 0≤x<0.2. The material for the coating layer comprises a carbon material, wherein the ID/IG value of a Raman spectrum of the carbon material is y, and 0.9≤y<1. ID/IG is the peak intensity ratio of peak D to peak G of the Raman spectrum of the carbon material, a Raman shift of peak D ranges from 1300 cm−1 to 1360 cm−1, and a Raman shift of peak G ranges from 1580 cm−1 to 1600 cm−1.

## Claims

### Claim 1

A sodium battery positive electrode material comprising:
a core and a coating layer covering a surface of the core;
wherein a general molecular formula of the core comprises Na3V2-xMx(PO4)2F3, wherein M represents a doping element that can replace V, M comprises at least one of Fe, Cr, Mn, Co, Ti, Ni, Cu, Zn, Mo, Nb, Zr, La and Ce, and 0≤x<0.2; and
a material for the coating layer comprising a carbon material, wherein an ID/IG value of a Raman spectrum of the carbon material is y, and 0.9≤y<1, wherein the ID/IG is a peak intensity ratio of a D peak to a G peak of the Raman spectrum of the carbon material, a Raman shift of the D peak ranges from 1300 cm−1 to 1360 cm−1, and a Raman shift of the G peak ranges from 1580 cm−1 to 1600 cm−1.

### Claim 2 (depends on 1)

The positive electrode material according to claim 1, wherein 0.92≤y≤0.98.

### Claim 3 (depends on 1)

The positive electrode material according to claim 1, wherein an average particle size of the positive electrode material ranges from 50 nm to 2000 nm, and the average particle size is a corresponding particle size when a cumulative quantity percentage of the positive electrode material reaches 50%.

### Claim 4 (depends on 1)

The positive electrode material according to claim 1, wherein a mass percentage of the carbon material in the positive electrode material ranges from 7% to 15%.

### Claim 5 (depends on 1)

The positive electrode material according to claim 1, wherein a thickness of the coating layer ranges from 5 nm to 20 nm.

### Claim 6

A preparation method for a sodium battery positive electrode material, comprising:
mixing a core raw material and a carbon source to obtain a precursor material, wherein the carbon source comprises an aromatic hydrocarbon-containing substance; and
performing calcination on the precursor material to obtain the positive electrode material, wherein the positive electrode material comprises a core and a coating layer covering a surface of the core and comprising a coating material; wherein a general molecular formula of the core comprises Na3V2-xMx(PO4)2F3, wherein M represents a doping element that can replace V, M comprises at least one of Fe, Cr, Mn, Co, Ti, Ni, Cu, Zn, Mo, Nb, Zr, La and Ce, and 0≤x<0.2; and the coating material for the coating layer comprises a carbon material, wherein an ID/IG value of a Raman spectrum of the carbon material is y, and 0.9≤y<1.

### Claim 7 (depends on 6)

The preparation method according to claim 6, wherein the aromatic hydrocarbon comprises a monocyclic aromatic hydrocarbon and a polycyclic aromatic hydrocarbon.

### Claim 8 (depends on 6)

The preparation method according to claim 6, wherein the aromatic hydrocarbon-containing substance comprises at least one of sulfonated asphalt, an asphalt phenolate, oxidized asphalt, asphalt resin, and emulsified asphalt.

### Claim 9 (depends on 6)

The preparation method according to claim 6, wherein a calcination temperature of the calcination ranges from 600° C. to 800° C., and a calcination time ranges from 10 min to 480 min.

### Claim 10 (depends on 9)

The preparation method according to claim 9, wherein the calcination comprises microwave calcination, and holding time of the microwave calcination ranges from 10 min to 25 min.

### Claim 11 (depends on 6)

The preparation method according to claim 6, wherein the performing calcination on the precursor material comprises:
performing calcination on the precursor material under protective gas, wherein the protective gas may be at least one of nitrogen, argon, and helium.

### Claim 12 (depends on 6)

The preparation method according to claim 6, further comprising:
performing carbon composite processing on the coating layer, or performing nanonization processing on the positive electrode material.

### Claim 13 (depends on 6)

The preparation method according to claim 6, wherein an average particle size of the positive electrode material ranges from 50 nm to 2000 nm, and the average particle size is a corresponding particle size when a cumulative quantity percentage of the positive electrode material reaches 50%.

### Claim 14 (depends on 6)

The preparation method according to claim 6, wherein a mass percentage of the carbon material in the positive electrode material ranges from 7% to 15%.

### Claim 15 (depends on 1)

A positive electrode sheet, comprising the sodium battery positive electrode material according to claim 1.

### Claim 16 (depends on 15)

A sodium battery, comprising the positive electrode sheet according to claim 15.

### Claim 17 (depends on 6)

A positive electrode sheet, comprising the sodium battery positive electrode material prepared by using the preparation method according to claim 6.

### Claim 18 (depends on 17)

A sodium battery, comprising the positive electrode sheet according to claim 17.

### Claim 19 (depends on 2)

The positive electrode material according to claim 2, wherein an average particle size of the positive electrode material ranges from 50 nm to 2000 nm, and the average particle size is a corresponding particle size when a cumulative quantity percentage of the positive electrode material reaches 50%.

### Claim 20 (depends on 19)

The positive electrode material according to claim 19, wherein a mass percentage of the carbon material in the positive electrode material ranges from 7% to 15%.