# US 2026/0021649 A1 · Method for manufacturing smart window and smart window manufactured by the method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0021649 A1
- Document ID: US20260021649A1
- Status: Published application
- Kind: A1
- Application number: 19/275,069
- Filed: 2025-07-21
- Published: 2026-01-22
- Earliest claimed: 2024-07-22
- Assignees: Dongwoo Fine-Chem Co., Ltd.
- Applicants: Dongwoo Fine-Chem Co., Ltd.
- Inventors: Joon-Mo JUNG; Seung-Won SONG
- Web page: https://patentgrep.com/patent/US20260021649A1

## CPC

- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 17/10935: {as a preformed layer, e.g. formed by extrusion}
- B32B 3/02: characterised by features of form at particular places, e.g. in edge regions {(non-uniform thickness B32B3/263)}
- B32B 17/10036: {comprising two outer glass sheets}
- B32B 17/10293: {Edge features, e.g. inserts or holes}
- B32B 17/10504: {Liquid crystal layer}
- B32B 17/10697: {being cross-linked}
- B32B 17/10761: {containing vinyl acetal}
- B32B 17/10834: {using a fluid}
- B32B 27/08: of synthetic resin
- B32B 27/18: characterised by the use of special additives
- B32B 27/30: comprising vinyl {(co)polymers; comprising acrylic (co)polymers}
- B32B 27/306: {comprising vinyl acetate or vinyl alcohol (co)polymers}
- G02F 1/133305: {Flexible substrates, e.g. plastics, organic film}
- G02F 1/133354: {Arrangements for aligning or assembling substrates}
- G02F 1/133528: {Polarisers}
- G02F 1/133565: {inside the LC elements, i.e. between the cell substrates}
- B32B 2250/246: All polymers belonging to those covered by groups B32B27/32 and B32B27/30
- B32B 2250/40: Symmetrical or sandwich layers, e.g. ABA, ABCBA, ABCCBA
- B32B 2255/10: on synthetic resin layer or on natural or synthetic rubber layer
- B32B 2255/26: Polymeric coating
- B32B 2255/28: Multiple coating on one surface
- B32B 2307/202: Conductive
- B32B 2307/412: Transparent
- B32B 2307/42: Polarizing, birefringent, filtering
- B32B 2307/516: mono-axially
- B32B 2307/54: Yield strength; Tensile strength
- B32B 2307/7376: Thickness
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

Disclosed are a method for manufacturing a smart window and a smart window manufactured thereby. The method includes: a step of laminating a film laminate including an optical laminate, an adhesive layer, and a substrate; a pre-bonding step; and a main bonding step, wherein the main bonding step includes: step a) of maintaining a laminate resulting from the pre-bonding step at a pressure of 3.5 to 10 bar for 15 to 60 minutes; and step b) of maintaining a laminate resulting from step a) at a reduced pressure of 1 bar to 3 bar for 70 to 100 minutes. According to the disclosure, the unevenness of the pressure applied to the liquid crystal layer during glass bonding may be eliminated, thereby manufacturing a smart window in which the uneven distribution of liquid crystals does not occur.

## Claims

### Claim 1

A method for manufacturing a smart window, comprising:
a step of laminating a film laminate comprising an optical laminate, an adhesive layer, and a substrate;
a pre-bonding step; and
a main bonding step,
wherein the main bonding step comprises:
step a) of maintaining a laminate resulting from the pre-bonding step at a pressure of 3.5 to 10 bar for 15 to 60 minutes; and
step b) of maintaining a laminate resulting from step a) at a reduced pressure of 1 bar to 3 bar for 70 to 100 minutes.

### Claim 2 (depends on 1)

The method of claim 1, wherein steps a) and b) are performed at a temperature of 50 to 110° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein step a) is performed at a pressure of 3.5 to 6 bar.

### Claim 4 (depends on 1)

The method of claim 1, wherein step b) is performed at a pressure of 1 to 2 bar.

### Claim 5 (depends on 1)

The method of claim 1, wherein the pre-bonding step is performed at a pressure of 0.1 to 3 bar and comprises:
step S1) of heating to a temperature of 40 to 90° C.;
step S2) of maintaining the temperature of S1); and
step S3) of cooling to a temperature of 0 to 30° C.

### Claim 6 (depends on 1)

The method of claim 1, further comprising a step of manufacturing the film laminate comprising an optical laminate,
wherein the step of manufacturing the film laminate comprises a step of forming a gap layer at ends of the optical laminate.

### Claim 7 (depends on 6)

The method of claim 6, wherein the gap layer has a storage modulus (G′) of 103 to 106 kPa at 60° C. and a storage modulus (G′) of 5×102 to 5×103 kPa at 100° C., and is formed to have a thickness larger than that of the optical laminate.

### Claim 8 (depends on 6)

The method of claim 6, wherein the step of manufacturing the film laminate comprises a step of laminating a surface protective layer on at least one of upper and lower surfaces of the optical laminate.

### Claim 9 (depends on 8)

The method of claim 8, wherein the surface protective layer is a low-temperature curable polyvinyl butyral (PVB) film that is cured at a temperature of 90° C. or lower, and has a tensile modulus (E′) of 108 to 1010 Pa at 60° C. and 106 to 107 Pa at 90° C.

### Claim 10 (depends on 8)

The method of claim 8, wherein the surface protective layer comprises a polyvinyl butyral (PVB) film which has no flowability at 100° C. or lower under a load of 21.6 kg, and has a melt flow rate (MFR) of 0.02 g/10 min or less, as measured according to ASTM D1238 at 140° C. under a load of 2.16 kg.

### Claim 11 (depends on 1)

A smart window manufactured by the method of claim 1, the smart window comprising an optical laminate, wherein the optical laminate comprises:
a first polarizing plate;
a first transparent conductive layer formed on an inner surface of the first polarizing plate;
a second polarizing plate opposite to the first polarizing plate;
a second transparent conductive layer formed on an inner surface of the second polarizing plate and opposite to the first transparent conductive layer;
a liquid crystal layer provided between the first transparent conductive layer and the second transparent conductive layer; and
an alignment film formed between the transparent conductive layer and the liquid crystal layer,
wherein at least one of the first transparent conductive layer and the second transparent conductive layer is formed in direct contact with the first polarizing plate or the second polarizing plate.