# US 2026/0021646 A1 · Bendable glass stack assemblies, articles and methods of making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0021646 A1
- Document ID: US20260021646A1
- Status: Published application
- Kind: A1
- Application number: 19/339,587
- Filed: 2025-09-25
- Published: 2026-01-22
- Earliest claimed: 2014-01-29
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Theresa Chang; Polly Wanda Chu; Patrick Joseph Cimo; Adam James Ellison; Timothy Michael Gross; Guangli Hu; Nicholas James Smith; Butchi Reddy Vaddi; Natesan Venkataraman
- Web page: https://patentgrep.com/patent/US20260021646A1

## CPC

- B32B 17/10: of synthetic resin
- B32B 3/14: characterised by a face layer formed of separate pieces of material {which are juxtaposed side-by-side (B32B5/02 takes precedence)}
- B32B 3/263: {characterised by a layer having non-uniform thickness}
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 17/06: comprising glass as the main or only constituent of a layer, next to another layer of a specific {material}
- B32B 17/10009: {characterized by the number, the constitution or treatment of glass sheets}
- B32B 17/101: {having a predetermined coefficient of thermal expansion [CTE]}
- B32B 17/10137: {Chemical strengthening}
- B32B 27/36: comprising polyesters
- B32B 37/12: characterised by using adhesives
- B32B 37/16: with all layers existing as coherent layers before laminating
- C03C 3/083: containing aluminium oxide or an iron compound
- C03C 3/091: containing aluminium
- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- C03C 17/28: with organic material (C03C17/34, C03C17/44 take precedence)
- C03C 17/30: with silicon-containing compounds
- C03C 17/32: with synthetic or natural resins (C03C17/30 takes precedence)
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- G06F 1/1652: {the display being flexible, e.g. mimicking a sheet of paper, or rollable}
- H05K 1/028: {Bending or folding regions of flexible printed circuits (H05K1/0283 takes precedence)}
- H05K 1/0306: {Inorganic insulating substrates, e.g. ceramic, glass}
- H05K 3/46: Manufacturing multilayer circuits
- B32B 2255/00: Coating on the layer surface
- B32B 2255/26: Polymeric coating
- B32B 2307/51: Elastic
- B32B 2307/536: Hardness
- B32B 2307/546: Flexural strength; Flexion stiffness
- B32B 2307/558: Impact strength, toughness
- B32B 2307/5825: Tear resistant
- B32B 2315/08: Glass
- B32B 2367/00: Polyesters, e.g. PET, i.e. polyethylene terephthalate
- B32B 2457/00: Electrical equipment
- B32B 2457/20: Displays, e.g. liquid crystal displays, plasma displays
- G02F 1/133305: {Flexible substrates, e.g. plastics, organic film}
- G09F 9/301: {flexible foldable or roll-able electronic displays, e.g. thin LCD, OLED}
- H04M 1/0268: {including a flexible display panel}
- Y10T 428/24942: including components having same physical characteristic in differing degree
- Y10T 428/26: Web or sheet containing structurally defined element or component, the element or component having a specified physical dimension
- Y10T 428/266: of base or substrate
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- G06F: ELECTRIC DIGITAL DATA PROCESSING (computer systems based on specific computational models G06N)
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- G09F: DISPLAYING; ADVERTISING; SIGNS; LABELS OR NAME-PLATES; SEALS
- H04M: TELEPHONIC COMMUNICATION (circuits for controlling other apparatus via a telephone cable and not involving telephone switching apparatus G08)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A glass element having a thickness from 25 μm to 125 μm, a first primary surface, a second primary surface, and a compressive stress region extending from the first primary surface to a first depth, the region defined by a compressive stress σI of at least about 100 MPa at the first primary surface. Further, the glass element has a stress profile such that it does not fail when it is subject to 200,000 cycles of bending to a target bend radius of from 1 mm to 20 mm, by the parallel plate method. Still further, the glass element has a puncture resistance of greater than about 1.5 kgf when the first primary surface of the glass element is loaded with a tungsten carbide ball having a diameter of 1.5 mm.

## Claims

### Claim 1

An article, comprising:
a glass element comprising a plurality of glass layers, each of the glass layers having a thickness in a range from 1 μm to 125 μm,
wherein the glass element is characterized by:
(a) a topmost one of the plurality of glass layers, defining a first primary surface of the glass element, is strengthened so as to exhibit a compressive stress region extending from the first primary surface, the compressive stress region comprising a compressive stress of at least 100 MPa at the first primary surface;
(b) an absence of failure when the glass element is held so that the first primary surface exhibits a minimum bend radius of 10 mm for at least 60 minutes at about 25° C. and about 50% relative humidity, the absence of failure being characterized by a lack of delamination between layers of the article; and
(c) a puncture resistance of greater than about 1.5 kgf when the first primary surface of the glass element is loaded with a tungsten carbide ball having a diameter of 0.5 mm.

### Claim 2 (depends on 1)

The article of claim 1, wherein the topmost one of the plurality of glass layers is chemically strengthened so that the compressive stress at the first primary surface is from 600 MPa to 1000 MPa.

### Claim 3 (depends on 2)

The article of claim 2, wherein each of the plurality of glass layers is chemically strengthened to exhibit a surface compressive stress that is from 600 MPa to 1000 MPa.

### Claim 4 (depends on 1)

The article of claim 1, wherein the glass element comprises a pencil hardness of greater than or equal to 8H.

### Claim 5 (depends on 1)

The article of claim 1, wherein at least some of the plurality of glass layers are stacked directly together in contact with one another.

### Claim 6 (depends on 1)

The article of claim 1, wherein there are one or more compliant interlayers disposed between adjacent ones of the plurality of glass layers.

### Claim 7 (depends on 6)

The article of claim 6, wherein each of the one or more compliant interlayers are configured to allow movement between the plurality of glass layers with respect to one another upon bending of the article so as to decouple bending stresses in each of the plurality of glass layers.

### Claim 8 (depends on 1)

The article of claim 1, wherein at least the topmost one of the plurality of glass layers comprises an edge compressive stress region extending inward from an edge thereof.

### Claim 9 (depends on 1)

The article of claim 1, wherein the plurality of glass layers comprises a core region and clad regions adjacent and in contact with the core region, wherein the topmost one of the plurality of glass layers is one of the clad regions, wherein the core region comprises a coefficient of thermal expansion greater than the core regions to induce compressive stress in the core regions.

### Claim 10 (depends on 1)

The article of claim 1, wherein the plurality of glass layers comprises three glass layers, wherein each of the glass layers comprises a thickness that is about 8 μm.

### Claim 11 (depends on 1)

The article of claim 1, wherein, when the first primary surface of the glass element is subject to a 1 kgf load from a Vickers indenter, there is introduced a flaw of ≤100 microns in the first primary surface, wherein the glass element has a Vickers hardness of 550 to 650 kgf/mm2.

### Claim 12 (depends on 1)

The article of claim 1, comprising F/w≤0.76 N/mm, wherein F is the closing force to put the glass element at the bend radius, and w is the dimension of the glass element in a direction parallel to the axis around which the glass is bent.

### Claim 13 (depends on 1)

The article of claim 1, wherein:
the thickness of the glass element is from about 50 μm to about 100 μm,
the compressive stress at the first primary surface of the glass element is less than or equal to 2000 MPa, and
the compressive stress region extends to a first depth that is one third of the thickness of the glass element or less from the first primary surface of the glass element.

### Claim 14

An article, comprising:
a glass element comprising a glass layer and a glass structure that are monolithic regard to one another to form a monolithic glass body, the monolithic glass body comprising:
a central region where the monolithic glass body only comprises the glass layer and comprises a central thickness, the central region disposed between and spaced apart from parallel edges of the glass element; and
peripheral regions extending between the central region and each of the peripheral edges, wherein:
within the peripheral regions, additional material of the glass structure is present so that the peripheral regions have a greater thickness than the central thickness,
the central thickness is from 20 μm to 125 μm,
a first compressive stress region extends throughout the glass layer and the glass structure, the first compressive stress region extending from a first primary surface of the glass layer to a first depth,
the first compressive stress region comprises a compressive stress of at least 100 MPa at the first primary surface, and
the article is characterized by an absence of failure when the glass element is held so that the first primary surface exhibits a minimum bend radius of 5 mm for at least 60 minutes at about 25° C. and about 50% relative humidity, when the first primary surface is placed in tension by bending.

### Claim 15 (depends on 14)

The article according to claim 14, wherein the article is characterized a puncture resistance of greater than about 1.5 kgf when the first primary surface of the glass element at one of the peripheral regions is loaded with a tungsten carbide ball having a diameter of 1.5 mm.

### Claim 16 (depends on 15)

The article according to claim 15, wherein a second primary surface of the monolithic body comprises an etched portion that is recessed from a remainder of the second primary surface, the etched portion being an area where material was selectively removed from the second primary surface to form the central region and peripheral regions.

### Claim 17 (depends on 16)

The article according to claim 16, wherein:
a second compressive stress region extends throughout the glass layer and the glass structure, the second compressive stress region extending from the second primary surface to a first depth,
the second compressive stress region comprises a compressive stress of at least 100 MPa at the second primary surface.

### Claim 18 (depends on 17)

The article according to claim 17, wherein the first and second compressive stress regions are from chemically strengthening the monolithic glass body so that compressive stress at the first and second primary surfaces is developed by immersing both the glass layer and the glass structure in an submersion step.

### Claim 19 (depends on 18)

The article according to claim 18, wherein a thickness of the monolithic glass body in the peripheral regions is greater than or equal to 125 μm.

### Claim 20 (depends on 18)

The article according to claim 18, wherein the central thickness is from 20 μm to 30 μm.