# US 2026/0018664 A1 · Production Method For Anode-Supported Cell

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0018664 A1
- Document ID: US20260018664A1
- Status: Published application
- Kind: A1
- Application number: 19/266,259
- Filed: 2025-07-11
- Published: 2026-01-15
- Earliest claimed: 2024-07-12
- Assignees: Mitsui Mining & Smelting Co., Ltd.; Honda Motor Co., Ltd.
- Applicants: Mitsui Mining & Smelting Co., Ltd.; Honda Motor Co., Ltd.
- Inventors: Minoru KAHATA; Shingo IDE; Yuya KOMORI; Miki KUREHA; Tsutomu HIGUCHI; Takayuki YAMADA; Yukihisa KANAO
- Web page: https://patentgrep.com/patent/US20260018664A1

## CPC

- H01M 10/0562: Solid materials
- H01M 8/1213: characterised by the electrode/electrolyte combination or the supporting material
- H01M 8/1246: the electrolyte consisting of oxides
- H01M 2008/1293: {Fuel cells with solid oxide electrolytes}
- H01M 2300/0071: Oxides
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A production method includes: heating a first stacked body at 1000° C. or more, the first stacked body having: a layer containing an oxide represented by the composition formula: La2Si2O7; a first layer provided on one side of the oxide-containing layer and containing cerium oxide doped with a lanthanum element; and a layer provided on the first layer opposite to the oxide-containing layer and containing nickel oxide, and thereby generating, from the oxide represented by the composition formula, a solid electrolyte that has an apatite structure and is c-axis oriented; placing a second layer containing cerium oxide doped or not doped with an Ln element (a rare earth element other than cerium), on the solid electrolyte-containing layer opposite to the cerium oxide-containing layer, and thereby obtaining a second stacked body; and heating the second stacked body at 1000° C. or more.

## Claims

### Claim 1

A production method for producing an anode-supported cell, the method comprising:
heating a first stacked body, in which a layer, a first layer and a nickel oxide-containing layer are stacked, at 1000° C. or more,
wherein the layer contains an oxide represented by a composition formula: La2Si2O7,
the first layer is provided on a first side of the layer and contains cerium oxide doped with a lanthanum element, and
the nickel oxide-containing layer is provided on a first side of the first layer opposite to a second side of the first layer that faces the layer and contains nickel oxide,
and thereby generating, from the oxide represented by the composition formula, a solid electrolyte that has an apatite structure and is c-axis oriented;
placing a second layer that contains cerium oxide that is doped or not doped with an Ln element, where Ln represents a rare earth element other than cerium, on a second side of the layer, which contains the solid electrolyte, opposite to the first side of the layer that faces the first layer, and thereby obtaining a second stacked body; and
heating the second stacked body at 1000° C. or more,
wherein the nickel oxide-containing layer has a thickness of 300 μm or more and 3000 μm or less.

### Claim 2

A production method for producing an anode-supported cell, the method comprising:
heating a first stacked body, in which a layer, a first layer, a nickel oxide-containing layer and an auxiliary support layer are stacked, at 1000° C. or more,
wherein the layer contains an oxide represented by a composition formula: La2Si2O7,
the first layer is provided on a first side of the layer and contains cerium oxide doped with a lanthanum element,
the nickel oxide-containing layer is provided on a first side of the first layer opposite to a second side of the first layer that faces the layer and contains nickel oxide, and
the auxiliary support layer is provided on a first side of the nickel oxide-containing layer opposite to a second side of the nickel oxide-containing layer that faces the first layer,
and thereby generating, from the oxide represented by the composition formula, a solid electrolyte that has an apatite structure and is c-axis oriented;
placing a second layer that contains cerium oxide that is doped or not doped with an Ln element, where Ln represents a rare earth element other than cerium, on a second side of the layer, which contains solid electrolyte, opposite to the first side of the layer that faces the first layer, and thereby obtaining a second stacked body; and
heating the second stacked body at 1000° C. or more.

### Claim 3 (depends on 1)

The production method according to claim 1,
wherein the Ln element comprises at least one selected from the group consisting of La, Nd, and Sm.

### Claim 4 (depends on 1)

The production method according to claim 1,
wherein the solid electrolyte comprising a composite oxide of lanthanum and silicon is generated.

### Claim 5 (depends on 1)

The production method according to claim 1,
wherein the solid electrolyte represented by a formula described below is generated:
A9.33+x[T6.00]O26.00+z,
wherein A represents one or more elements selected from the group consisting of La, Ce, Nd, and Sm,
T represents Si,
x represents a number of −1.33 or more and 3.00 or less,
z represents a number of −5.00 or more and 5.20 or less, and
a ratio (A/T) of the number of moles of A relative to the number of moles of T is 1.33 or more and 3.61 or less.

### Claim 6 (depends on 1)

The production method according to claim 1, further comprising:
after heating the second stacked body to obtain a sintered second stacked body having a sintered second layer, placing a layer made of a material for an air electrode on a second side of the sintered second layer opposite to a first side of the sintered second layer that faces the layer, and thereby obtaining a third stacked body; and
heating the third stacked body.

### Claim 7 (depends on 2)

The production method according to claim 2, further comprising:
after heating the second stacked body to obtain a sintered second stacked body having a sintered second layer, placing a layer made of a material for an air electrode on a second side of the sintered second layer opposite to a first side of the sintered second layer that faces the layer, and thereby obtaining a third stacked body; and
heating the third stacked body.

### Claim 8 (depends on 2)

The production method according to claim 2,
wherein the Ln element comprises at least one selected from the group consisting of La, Nd, and Sm.

### Claim 9 (depends on 2)

The production method according to claim 2,
wherein the solid electrolyte comprising a composite oxide of lanthanum and silicon is generated.

### Claim 10 (depends on 2)

The production method according to claim 2,
wherein the solid electrolyte represented by a formula described below is generated:
A9.33+x[T6.00]O26.00+z,
wherein A represents one or more elements selected from the group consisting of La, Ce, Nd, and Sm,
T represents Si,
x represents a number of −1.33 or more and 3.00 or less,
z represents a number of −5.00 or more and 5.20 or less, and
a ratio (A/T) of the number of moles of A relative to the number of moles of T is 1.33 or more and 3.61 or less.