# US 2026/0018458 A1 · Semiconductor devices and methods of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0018458 A1
- Document ID: US20260018458A1
- Status: Published application
- Kind: A1
- Application number: 18/769,944
- Filed: 2024-07-11
- Published: 2026-01-15
- Earliest claimed: 2024-07-11
- Assignees: EMD Performance Materials Corp.
- Applicants: Samsung Electronics Co., Ltd.; Merck Patent GmbH
- Inventors: Younghun Sung; Guo Liu; Bhushan Zope; Soyoung Lee; Hyunho Kim; Youn Joung Cho; Byungkeun Hwang; Sunhye Hwang
- Web page: https://patentgrep.com/patent/US20260018458A1

## CPC

- H10W 20/083: {the openings being via holes penetrating underlying conductors}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W 20/077: {on sidewalls or on top surfaces of conductors (H10W20/076 takes precedence)}
- H10W 20/42: Vias, e.g. via plugs
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of manufacturing a semiconductor device comprising: forming a first layer in which first conductive patterns and first dielectric patterns are alternately arranged; forming passivation layers on the first conductive patterns, respectively; and forming second dielectric patterns on the first dielectric patterns, respectively, by an area-selective atomic layer deposition at a first temperature, wherein the first temperature is 350° C. or less, wherein the area-selective atomic layer deposition includes: pulsing a metal catalyst; performing a primary purge by a purge gas; sub-pulsing a reaction precursor at least once; and performing a secondary purge by the purge gas after each of the sub-pulsing.

## Claims

### Claim 1

A method of manufacturing a semiconductor device comprising:
forming a first layer in which first conductive patterns and first dielectric patterns are alternately arranged;
forming passivation layers on the first conductive patterns, respectively; and
forming second dielectric patterns on the first dielectric patterns, respectively, by an area-selective atomic layer deposition at a first temperature, wherein the first temperature is 350° C. or less,
wherein the area-selective atomic layer deposition includes:
pulsing a metal catalyst;
performing a primary purge by a purge gas;
sub-pulsing a reaction precursor at least once; and
performing a secondary purge by the purge gas after each of the sub-pulsing.

### Claim 2 (depends on 1)

The method of claim 1, wherein the purge gas is continuously supplied with a constant flow rate and a constant pressure during the area-selective atomic layer deposition.

### Claim 3 (depends on 2)

The method of claim 2, wherein the constant pressure of the purge gas is 1 Torr or less.

### Claim 4 (depends on 1)

The method of claim 1, wherein the area-selective atomic layer deposition further includes pumping the purge gas between the sub-pulsing the reaction precursor and the secondary purge.

### Claim 5 (depends on 4)

The method of claim 4, wherein the purge gas of the performing the primary purge has a first flow rate and a first pressure,
wherein the purge gas of the pumping the purge gas has a second flow rate and a second pressure, and
wherein the purge gas of the performing the second purge has a third flow rate and a third pressure.

### Claim 6 (depends on 5)

The method of claim 5, wherein, the first flow rate is greater than the second flow rate,
wherein the third flow rate is greater than the second flow rate,
wherein the first pressure is greater than the second pressure, and
wherein the third pressure is greater than the second pressure.

### Claim 7 (depends on 6)

The method of claim 6, wherein the second flow rate is zero (0) standard cubic centimeters per minute (sccm), and
wherein the second pressure is 0.1 Torr or less.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first temperature is 150° C. to 350° C.

### Claim 9 (depends on 1)

The method of claim 1, wherein the metal catalyst includes trimethylaluminum, triethylaluminum, dimethylaluminum iso-propoxide, and/or a combination thereof.

### Claim 10 (depends on 1)

The method of claim 1, wherein the reaction precursor is a silanol precursor, and
wherein the second dielectric patterns include silicon oxide.

### Claim 11 (depends on 10)

The method of claim 10, wherein the silanol precursor includes tris(t-pentoxy)silanol, bis(t-pentoxy)(t-butoxy)silanol, and/or a combination thereof.

### Claim 12 (depends on 1)

The method of claim 1, wherein
the forming the passivation layers includes supplying a self-assembled molecule that includes a thiol group material, an amine group material, and/or a carboxylic group material.

### Claim 13 (depends on 12)

The method of claim 12, wherein the supplying the self-assembled molecule is performed at a second temperature of 100° C. to 350° C.

### Claim 14 (depends on 13)

The method of claim 13, wherein the forming the passivation layers further includes performing additional purge after the supplying the self-assembled molecule.

### Claim 15 (depends on 1)

The method of claim 1, further comprising:
repeating the area-selective atomic layer deposition until the second dielectric patterns reach to a desired thickness, and
performing a tertiary purge before the repeating the area-selective atomic layer deposition.

### Claim 16 (depends on 1)

The method of claim 1, wherein the second dielectric patterns include a dielectric material that has a dielectric constant of 2.5 to 6.0.

### Claim 17 (depends on 1)

The method of claim 1, wherein the second dielectric patterns include a dielectric material that has a leakage current of 3×10−7 A/cm2 or less at 5 MV/cm.

### Claim 18 (depends on 1)

The method of claim 1, wherein the first dielectric patterns and the second dielectric patterns each include silicon oxide.

### Claim 19 (depends on 1)

The method of claim 1, further comprising:
forming vias electrically connected to the first conductive patterns; and
forming second conductive patterns electrically connected to the first conductive patterns through the vias.

### Claim 20

A semiconductor device comprising:
a first layer including first conductive patterns and first dielectric patterns;
second dielectric patterns on the first dielectric patterns, wherein the second dielectric patterns have same planar shapes as the first dielectric patterns, respectively, and include a dielectric material that has a dielectric constant of 2.5 to 6.0 and a leakage current of 3×10−7 A/cm2 or less at 5 MV/cm;
a second layer electrically connected to the first conductive patterns, wherein the second layer includes vias that are in contact with the second dielectric patterns; and
a third layer including second conductive patterns that are electrically connected to the first conductive patterns through the vias,
wherein the semiconductor device is manufactured by a method comprising:
forming the first layer in which the first conductive patterns and the first dielectric patterns are alternately arranged;
forming passivation layers on the first conductive patterns, respectively; and
forming the second dielectric patterns on the first dielectric patterns, respectively, by an area-selective atomic layer deposition at a first temperature, wherein the first temperature is 350° C. or less, and
wherein the area-selective atomic layer deposition includes:
pulsing a metal catalyst;
performing a primary purge by a purge gas;
sub-pulsing a reaction precursor at least once; and
performing a secondary purge by the purge gas after each of the sub-pulsing.