# US 2026/0015769 A1 · Methods to enhance and characterize oxygen precipitation induced defects during a wafer polishing sequence

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0015769 A1
- Document ID: US20260015769A1
- Status: Published application
- Kind: A1
- Application number: 19/260,878
- Filed: 2025-07-07
- Published: 2026-01-15
- Earliest claimed: 2024-07-10
- Assignees: GlobalWafers Co., Ltd.
- Applicants: GlobalWafers Co., Ltd.
- Inventors: Zheng Lu; Shan-Hui Lin
- Web page: https://patentgrep.com/patent/US20260015769A1

## CPC

- C30B 33/02: Heat treatment (C30B33/04, C30B33/06 take precedence)
- H10P 74/203: {Structural properties, e.g. testing or measuring thicknesses, line widths, warpage, bond strengths or physical defects}
- C30B 15/20: Controlling or regulating (controlling or regulating in general G05)
- C30B 29/06: Silicon
- G01N 21/9501: {Semiconductor wafers (manufacturing processes per se of semiconductor devices implementing a measuring step H10P74/20)}
- G01N 2021/8411: {Application to online plant, process monitoring}
- H10P 74/23: {characterised by multiple measurements, corrections, marking or sorting processes}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

Methods for detecting oxygen precipitation induced defects during a polishing sequence. The methods are suited for detecting oxygen precipitates in heavily doped boron single crystal silicon wafers or in lightly doped wafers that are COP-free. The methods may involve inspecting a silicon wafer for LLS defects after a thermal anneal followed by a polishing sequence.

## Claims

### Claim 1

A method for detecting oxygen precipitates in silicon wafers during a polishing sequence, the method comprising:
annealing a silicon wafer to at least 1000° C. for at least 0.5 hours to increase the size of oxygen precipitates present in the silicon wafer, the silicon wafer being boron doped and having a resistivity of less than 20 mohm-cm;
polishing the silicon wafer in a first polishing step after annealing the silicon wafer, the first polishing step being a double-side polish;
polishing the silicon wafer in a second polishing step after the first polishing step, the second polishing step being a finish polish;
inspecting the silicon wafer for defects in an inspection step, the inspection step being after the second polishing step, the inspection step comprising:
directing light to a front surface of the silicon wafer and detecting scattered reflected light; and
identifying light scattering events on the front surface of the silicon wafer based on the reflected light.

### Claim 2 (depends on 1)

The method as set forth in claim 1 wherein the silicon wafer is annealed to at least 1000° C. for at least 1 hour.

### Claim 3 (depends on 1)

The method as set forth in claim 1 wherein the silicon wafer is annealed to at least 1000° C. for at least 2 hours.

### Claim 4 (depends on 1)

The method as set forth in claim 1 wherein the silicon wafer is annealed to at least 1000° C. for at least 4 hours.

### Claim 5 (depends on 1)

The method as set forth in claim 1 wherein:
(1) directing light to a front surface of the silicon wafer and detecting scattered reflected light and (2) identifying light scattering events on the front surface of the silicon wafer based on the reflected light comprises:
placing the silicon wafer on a wafer inspection tool; and
operating the wafer inspection tool to inspect the silicon wafer for defects.

### Claim 6 (depends on 5)

The method as set forth in claim 5 wherein the wafer inspection tool outputs a particle map of the silicon wafer.

### Claim 7 (depends on 1)

The method as set forth in claim 1 wherein the silicon wafer has a resistivity of less than 15 mohm-cm.

### Claim 8 (depends on 1)

The method as set forth in claim 1 wherein the silicon wafer has a resistivity of less than 10 mohm-cm.

### Claim 9 (depends on 1)

The method as set forth in claim 1 wherein the silicon wafer has a resistivity of at least 5 mohm-cm.

### Claim 10 (depends on 1)

The method as set forth in claim 1 wherein:
the first polishing step is proceeded by an initial wafer polishing sequence comprising:
polishing the silicon wafer in a double-side polish; and
polishing the silicon wafer in a finish polish after the double-side polish.

### Claim 11 (depends on 1)

The method as set forth in claim 1 wherein the silicon wafer is a first silicon wafer, the method comprising:
polishing a second silicon wafer in the first polishing step, the second silicon wafer being boron doped and having a resistivity of less than 20 mohm-cm;
polishing the second silicon wafer in a second polishing step after the first polishing step, the second polishing step being a finish polish;
inspecting the second silicon wafer for defects in the wafer inspection step, the inspection step being after the second polishing step, the second silicon wafer not being annealed before the silicon wafer inspection step; and
comparing a density of light scattering events on the front surface of the first silicon wafer to a density of light scattering events on the front surface of the second silicon wafer.

### Claim 12 (depends on 11)

A method for producing silicon wafers with reduced defects, the method comprising:
detecting oxygen precipitates according to the method of claim 11:
heating a charge of silicon disposed within a crucible to cause a silicon melt to form in the crucible;
contacting a silicon seed crystal with the silicon melt; and
withdrawing the silicon seed crystal to grow a single crystal silicon ingot, wherein one or more growth conditions of the single crystal silicon ingot are selected based on, at least in part, the comparison of the density of light scattering events on the front surface of the first silicon wafer to the density of light scattering events on the front surface of the second silicon wafer.