# US 2026/0015740 A1 · Preparation of a molybdenum-silicon- phosphorus-transitional metal composite coating bath and process for zinc-nickel plating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0015740 A1
- Document ID: US20260015740A1
- Status: Published application
- Kind: A1
- Application number: 18/768,788
- Filed: 2024-07-10
- Published: 2026-01-15
- Earliest claimed: 2024-07-10
- Assignees: Goodrich Corporation
- Applicants: Goodrich Corporation
- Inventors: Weilong Zhang; Andrew Spaeth
- Web page: https://patentgrep.com/patent/US20260015740A1

## CPC

- C23F 11/185: {Refractory metal-containing compounds}
- C09D 5/084: {Inorganic compounds}
- C23C 10/02: Pretreatment of the material to be coated (C23C10/04 takes precedence)
- C23C 10/20: only one element being diffused
- C23C 10/60: After-treatment
- C23F 11/04: in markedly acid liquids
- C23F 11/173: Macromolecular compounds
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A method of disposing a corrosion resistant system to a substrate is disclosed. The method includes applying a plating material to the substrate, forming a chemical conversion coating solution by combining a solvent, at least one corrosion inhibitive cation comprising at least one of zirconium, titanium, cerium, vanadium species, manganese, or niobium, and at least one corrosion inhibitive anion comprising at least one of phosphate, molybdate, or silicate, and applying the chemical conversion coating solution to the plating material on the substrate.

## Claims

### Claim 1

A method of disposing a corrosion resistant system to a substrate, comprising:
applying a plating material to the substrate;
forming a chemical conversion coating solution by combining a solvent, at least one corrosion inhibitive cation comprising at least one of zirconium, titanium, cerium, vanadium species, manganese, or niobium, and at least one corrosion inhibitive anion comprising at least one of phosphate, molybdate, or silicate; and
applying the chemical conversion coating solution to the plating material on the substrate.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
prior to applying the chemical conversion coating solution to the plating material on the substrate, activating the plating material with an activator, wherein the activator is at least one of nitric acid or alkaline immersion cleaner.

### Claim 3 (depends on 2)

The method of claim 2, further comprising:
prior to activating the plating material with an activator, degreasing the plating material on the substrate, wherein the plating material on the substrate is degreased with at least one of acetone or methyl acetate.

### Claim 4 (depends on 1)

The method of claim 1, wherein the chemical conversion coating solution is applied to the plating material on the substrate by dipping the substrate plated with the plating material into a bath of the chemical conversion coating solution for between 2 minutes to 20 minutes, wherein the chemical conversion coating solution comprises at least one complexing agent, at least one oxidizer, and at least one organic polymer additive, wherein the at least one complexing agent is at least one of sulfuric acid, nitric acid, a fluorosilicic acid solution, Ethylenediaminetetraacetic acid (EDTA), tartaric acid, oxalic acid, phytic acid, citric acid, or glycine, wherein the at least one oxidizer is at least one of hydrogen peroxide (H2O2) or a permanganate compound, and wherein the at least one polymer additive is at least one of tannic acid, polyacrylic acid, polyvinyl alcohol, or polyvinylpyrrolidone.

### Claim 5 (depends on 1)

The method of claim 1, further comprising:
drying the substrate plated with the plating material and coated with a chemical conversion coating for at least two hours at between 30° C. (86° F.) and 200° C. (392° F.).

### Claim 6 (depends on 1)

The method of claim 1, wherein the chemical conversion coating solution has a pH of between 3.5 and 12.

### Claim 7 (depends on 1)

The method of claim 1, further comprising:
forming a corrosion inhibition composition solution by combining at least one of phosphate, molybdate, or silicate; and
applying the corrosion inhibition composition solution to the substrate plated with the plating material and coated with a chemical conversion coating.

### Claim 8 (depends on 7)

The method of claim 7, wherein the corrosion inhibition composition solution is applied to the substrate plated with the plating material and coated with the chemical conversion coating on by dipping the substrate plated with the plating material and coated with the chemical conversion coating into a bath of the corrosion inhibition composition solution for between 3 minutes to 12 minutes.

### Claim 9 (depends on 7)

The method of claim 7, further comprising:
drying the substrate plated with the plating material, coated with the chemical conversion coating, and coated with a corrosion inhibition composition coating for at least two hours at between 30° C. (86° F.) and 200° C. (392° F.).

### Claim 10

A corrosion inhibition system disposed on a substrate, comprising:
the substrate;
a plating material disposed on the substrate; and
a chemical conversion coating disposed on the plating material and comprising a corrosion inhibitive cation comprising at least one of zirconium, titanium, cerium, vanadium species, manganese, or niobium, and a corrosion inhibitive anion comprising at least one of phosphate, molybdate, or silicate.

### Claim 11 (depends on 10)

The corrosion inhibition system of claim 10, comprising:
an activator applied to the plating material prior to disposing the chemical conversion coating disposed on the plating material, the activator being at least one of nitric acid or alkaline immersion cleaner.

### Claim 12 (depends on 11)

The corrosion inhibition system of claim 11, wherein the plating material is degreased prior to disposing the activator on the plating material and wherein the plating material on the substrate is degreased with at least one of acetone or methyl acetate.

### Claim 13 (depends on 10)

The corrosion inhibition system of claim 10, wherein the chemical conversion coating is applied to the plating material on the substrate by dipping the substrate plated with the plating material into a bath of a chemical conversion coating solution for between 2 minutes to 20 minutes, wherein the chemical conversion coating solution comprises at least one complexing agent, at least one oxidizer, and at least one organic polymer additive, wherein the at least one complexing agent is at least one of sulfuric acid, nitric acid, a fluorosilicic acid solution, Ethylenediaminetetraacetic acid (EDTA), tartaric acid, oxalic acid, phytic acid, citric acid, or glycine, wherein the at least one oxidizer is at least one of hydrogen peroxide (H2O2) or a permanganate compound, and wherein the at least one polymer additive is at least one of tannic acid, polyacrylic acid, polyvinyl alcohol, or polyvinylpyrrolidone.

### Claim 14 (depends on 10)

The corrosion inhibition system of claim 10, wherein the substrate is plated with the plating material and coated with the chemical conversion coating is dried for at least two hours at between 30° C. (86° F.) and 200° C. (392° F.).

### Claim 15 (depends on 10)

The corrosion inhibition system of claim 10, wherein the chemical conversion coating has a pH of between 3.5 and 12.

### Claim 16 (depends on 10)

The corrosion inhibition system of claim 10, further comprising:
a corrosion inhibition composition coating disposed on the chemical conversion coating and comprising at least one of phosphate, molybdate, or silicate.

### Claim 17 (depends on 16)

The corrosion inhibition system of claim 16, wherein the corrosion inhibition composition coating is applied to the substrate plated with the plating material and coated with the chemical conversion coating on by dipping the substrate plated with the plating material and coated with the chemical conversion coating into a bath of a corrosion inhibition composition solution for between 3 minutes to 12 minutes.

### Claim 18 (depends on 16)

The corrosion inhibition system of claim 16, wherein the substrate plated with the plating material, coated with the chemical conversion coating, and coated with the corrosion inhibition composition coating is dried for at least two hours at between 30° C. (86° F.) and 200° C. (392° F.).

### Claim 19

A chemical conversion coating solution, comprising:
a solvent;
at least one corrosion inhibitive cation comprising at least one of zirconium, titanium, cerium, vanadium species, manganese, or niobium;
at least one corrosion inhibitive anion comprising at least one of phosphate, molybdate, or silicate;
at least one complexing agent;
at least one oxidizer; and
at least one organic polymer additive,
wherein the at least one complexing agent is at least one of sulfuric acid, nitric acid, a fluorosilicic acid solution, Ethylenediaminetetraacetic acid (EDTA), tartaric acid, oxalic acid, phytic acid, citric acid, or glycine,
wherein the at least one oxidizer is at least one of hydrogen peroxide (H2O2) or a permanganate compound, and
wherein the at least one polymer additive is at least one of tannic acid, polyacrylic acid, polyvinyl alcohol, or polyvinylpyrrolidone.

### Claim 20 (depends on 19)

The chemical conversion coating solution of claim 19, wherein the chemical conversion coating solution has a pH of between 3.5 and 12.