# US 2026/0015703 A1 · Porous metal structure and method for preparing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0015703 A1
- Document ID: US20260015703A1
- Status: Published application
- Kind: A1
- Application number: 19/333,009
- Filed: 2025-09-18
- Published: 2026-01-15
- Earliest claimed: 2023-11-07
- Assignees: Contemporary Amperex Technology Co., Limited
- Applicants: Contemporary Amperex Technology Co., Limited
- Inventors: Zun LI; Manman WANG; Xiaoming GE; Chuying OUYANG
- Web page: https://patentgrep.com/patent/US20260015703A1

## CPC

- C22C 9/05: with manganese as the next major constituent
- C22F 1/08: of copper or alloys based thereon
- C22F 1/002: {by rapid cooling or quenching; cooling agents used therefor}
- C22F 1/02: in inert or controlled atmosphere or vacuum (adjusting the composition of the atmosphere C21D1/76)
- C22F 1/16: of other metals or alloys based thereon
- C23F 1/00: Etching metallic material by chemical means (manufacture of printing surfaces B41C; manufacture of printed circuits H05K)
- C23F 1/34: for etching copper or alloys thereof
- C25F 3/02: Etching
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 4/662: {Alloys (collectors of lead alloys H01M4/685)}
- H01M 4/742: {perforated material}
- H01M 4/80: Porous plates, e.g. sintered carriers
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- C25F: PROCESSES FOR THE ELECTROLYTIC REMOVAL OF MATERIALS FROM OBJECTS; APPARATUS THEREFOR
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method includes: providing a cold-rolled alloy foil material; carrying out recrystallization annealing treatment on the alloy foil material, and then carrying out first cooling treatment to obtain an alloy foil material having a first component phase; carrying out phase separation thermal treatment on the alloy foil material, and then carrying out second cooling treatment to separate out a second component phase and obtain an alloy foil material having both the first and second component phase, where the temperature of the phase separation thermal treatment is smaller than the temperature of the recrystallization annealing treatment, and an average cooling rate of the second cooling treatment is smaller than an average cooling rate of the first cooling treatment; and carrying out dealloying treatment on the alloy foil material, carrying out reduction annealing treatment in a reducing gas atmosphere, and carrying out third cooling treatment to obtain a porous metal structure.

## Claims

### Claim 1

A method for preparing a porous metal structure, comprising:
providing a cold-rolled alloy foil material;
carrying out recrystallization annealing treatment on the alloy foil material, and then carrying out first cooling treatment to obtain an alloy foil material having a first component phase;
carrying out phase separation thermal treatment on the alloy foil material having the first component phase, and then carrying out second cooling treatment to separate out a second component phase and obtain an alloy foil material having both the first component phase and the second component phase, wherein the temperature of the phase separation thermal treatment is smaller than the temperature of the recrystallization annealing treatment, and an average cooling rate of the second cooling treatment is smaller than an average cooling rate of the first cooling treatment; and
carrying out dealloying treatment on the alloy foil material having the first component phase and the second component phase, carrying out reduction annealing treatment in a reducing gas atmosphere, and carrying out third cooling treatment to obtain a porous metal structure.

### Claim 2 (depends on 1)

The method according to claim 1, wherein:
the average cooling rate of the first cooling treatment is greater than or equal to 100° C./min, and is optionally greater than or equal to 200° C./min; and/or
the average cooling rate of the second cooling treatment is smaller than or equal to 2° C./min.

### Claim 3 (depends on 1)

The method according to claim 1, wherein:
the first cooling treatment process is a water cooling process; and/or
the second cooling treatment process is a furnace cooling process.

### Claim 4 (depends on 1)

The method according to claim 1, wherein:
the temperature reaches 50° C. or below in the first cooling treatment; and/or
the temperature reaches 50° C. or below in the second cooling treatment.

### Claim 5 (depends on 1)

The method according to claim 1, wherein:
the recrystallization annealing treatment is carried out in a muffle furnace; and/or
the phase separation thermal treatment is carried out in a tube furnace, and optionally, a temperature rise rate of the tube furnace is 2° C./min to 10° C./min, and is optionally 5° C./min to 10° C./min.

### Claim 6 (depends on 1)

The method according to claim 1, wherein:
a reducing gas in the reduction annealing treatment comprises a mixed gas of ammonia gas or hydrogen gas with an inert gas; and/or
a flow rate of the reducing gas in the reduction annealing treatment is 100 SCCM to 2000 SCCM.

### Claim 7 (depends on 1)

The method according to claim 1, wherein:
the reduction annealing treatment is carried out in a tube furnace, and optionally, a temperature rise rate of the tube furnace is 2° C./min to 10° C./min, and is optionally 5° C./min to 10° C./min; and/or
an average cooling rate of the third cooling treatment is smaller than or equal to 2° C./min, and optionally, the third cooling treatment process is a furnace cooling process; and/or
the temperature reaches 50° C. or below in the third cooling treatment.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the alloy foil material is a copper alloy foil material, the copper alloy foil material comprises a Cu element and a non-Cu metallic element, a standard electrode potential of the non-Cu metallic element is smaller than a standard electrode potential of the Cu element, and optionally, the non-Cu metallic element comprises one or more of Mn, Zn, Ni, Al, and Fe.

### Claim 9 (depends on 8)

The method according to claim 8, wherein an atomic content of the non-Cu metallic element in the copper alloy foil material is 60 at. % or more, and is optionally 65 at. % to 80 at. %.

### Claim 10 (depends on 1)

The method according to claim 1, wherein:
the first component phase comprises a γ phase; and/or
the second component phase comprises an a phase.

### Claim 11 (depends on 1)

The method according to claim 1, wherein:
a temperature of the recrystallization annealing treatment is 720° C. to 850° C.; and/or
a heat insulation time at the temperature of the recrystallization annealing treatment is 10 min to 60 min; and/or
a temperature of the phase separation thermal treatment is 620° C. to 700° C.; and/or
a heat insulation time at the temperature of the phase separation thermal treatment is 60 min to 360 min; and/or
a temperature of the reduction annealing treatment is 700° C. to 900° C., and is optionally 720° C. to 900° C.; and/or
a heat insulation time at the temperature of the reduction annealing treatment is 30 min to 120 min.

### Claim 12 (depends on 1)

The method according to claim 1, wherein a process of carrying out the dealloying treatment on the alloy foil material having the first component phase and the second component phase comprises a free corrosion dealloying process and an electrochemical corrosion dealloying process.

### Claim 13 (depends on 1)

A porous metal structure prepared by the method according to claim 1, wherein optionally, the porous metal structure is a porous copper structure.