# US 2026/0015697 A1 · Floating seal material and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0015697 A1
- Document ID: US20260015697A1
- Status: Published application
- Kind: A1
- Application number: 18/855,737
- Filed: 2023-05-01
- Published: 2026-01-15
- Earliest claimed: 2022-05-11
- Assignees: Eagle Industry Co., Ltd.
- Applicants: Eagle Industry Co., Ltd.
- Inventors: Jiro OKADO; Takeshi MORISAKI; Yasushi FUJIWARA
- Web page: https://patentgrep.com/patent/US20260015697A1

## CPC

- C22C 37/10: containing aluminium or silicon
- B22D 13/00: Centrifugal casting; Casting by using centrifugal force
- C22C 37/06: containing chromium
- F16J 15/344: {the pressing force being applied by means of an elastic ring supporting the slip-ring}
- F16J 15/3496: {use of special materials}
- F16J 15/441: {with floating ring}
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- F16J: PISTONS {(specially adapted for dampers F16F9/32)}; CYLINDERS; SEALINGS

## Abstract

Provided is a floating seal material containing at least Fe, C, Si, Mn, Cr, and Mo, in which the content of C is 2.3% by weight or more and 3.8% by weight or less, the content of Si is 0.7% by weight or more and 2.5% by weight or less, the content of Mn is 0.3% by weight or more and 1.3% by weight or less, the content of Cr is 3% by weight or more and 13% by weight or less, the content of Mo is 1.8% by weight or more and 15% by weight or less, and the remainder is made up of Fe and unavoidable impurities.

## Claims

### Claim 1

A floating seal material, comprising at least Fe, C, Si, Mn, Cr, and Mo,
wherein the content of C is 2.3% by weight or more and 3.8% by weight or less, the content of Si is 0.7% by weight or more and 2.5% by weight or less, the content of Mn is 0.3% by weight or more and 1.3% by weight or less, the content of Cr is 3% by weight or more and 13% by weight or less, the content of Mo is 1.8% by weight or more and 15% by weight or less, and the remainder is made up of Fe and unavoidable impurities.

### Claim 2 (depends on 1)

The floating seal material according to claim 1, comprising at least one of carbides represented by MC and M7C3 (wherein, M represents Fe, Si, Mn, Cr, or Mo) that are composed of at least a portion of the Fe, Si, Mn, Cr, or Mo, and at least a portion of the C.

### Claim 3 (depends on 1)

The floating seal material according to claim 1, comprising a carbide represented by M6C (wherein, M represents Fe, Si, Cr, or Mo) that is composed of at least a portion of the Fe, Si, Cr, or Mo, and at least a portion of the C.

### Claim 4 (depends on 1)

The floating seal material according to claim 1, having a phase-separated structure comprising at least one dispersed phase in a matrix phase,
wherein the dispersed phase comprises a particulate phase that is formed of at least one of a carbide represented by MC (wherein, M represents Fe, Si, Mn, Cr, or Mo) that are composed of at least a portion of the Fe, Si, Mn, Cr, or Mo, and at least a portion of the C, a carbide represented by M7C3 (wherein, M represents Fe, Si, Mn, Cr, or Mo) that are composed of at least a portion of the Fe, Si, Mn, Cr, or Mo, and at least a portion of the C, and a carbide represented by M6C (wherein, M represents Fe, Si, Cr, or Mo) that is composed of at least a portion of the Fe, Si, Cr, or Mo, and at least a portion of the C, and has an average particle size of 1 μm or less.

### Claim 5 (depends on 1)

A floating seal device, comprising the floating seal material according to claim 1.

### Claim 6

A method of producing a floating seal material, the method comprising:
the molten metal preparation step of preparing a molten metal comprising at least Fe, C, Si, Mn, Cr, and Mo, in which the content of C is 2.3% by weight or more and 3.8% by weight or less, the content of Si is 0.7% by weight or more and 2.5% by weight or less, the content of Mn is 0.3% by weight or more and 1.3% by weight or less, the content of Cr is 3% by weight or more and 13% by weight or less, the content of Mo is 1.8% by weight or more and 15% by weight or less, and the remainder is made up of Fe and unavoidable impurities; and
the casting step of casting the molten metal into a die.

### Claim 7 (depends on 6)

The method of producing a floating seal material according to claim 6, wherein, in the casting step, the molten metal is cast into the die by a centrifugal casting method.

### Claim 8 (depends on 6)

The method of producing a floating seal material according to claim 6, comprising the step of cooling the die to cool and solidify the molten metal after the casting step.