# US 2026/0015692 A1 · Advanced systems and methods for leaching rare earths from ore

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0015692 A1
- Document ID: US20260015692A1
- Status: Published application
- Kind: A1
- Application number: 19/335,614
- Filed: 2025-09-22
- Published: 2026-01-15
- Earliest claimed: 2021-01-15
- Assignees: Colorado School of Mines
- Applicants: Colorado School of Mines
- Inventors: Grant T. Colligan; Corby G. Anderson; Brock O'Kelley
- Web page: https://patentgrep.com/patent/US20260015692A1

## CPC

- C22B 59/00: Obtaining rare earth metals
- C22B 3/10: Hydrochloric acid {, other halogenated acids or salts thereof}
- C22B 26/10: Obtaining alkali metals
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

With the world's rapid advancement of technology, the demand and need for the materials that make up that technology has exploded. An important group of materials needed in this rapid advancement are the rare earth elements (REE) used in countless necessary applications. One source of rare earths found in the United States is bastnaesite, a rare earth bearing fluorocarbonate, mined at the Mountain Pass Mine in California. To increase production, it has been essential to optimize existing processes and create new ones to exploit current reserves. This research program was run to expand the understanding of the bastnaesite leaching system. A novel single stage hydrochloric leach system was created to optimize the rare earth extraction from bastnaesite. Typically, this process has utilized a two-stage leach system involving a high temperature hydrochloric acid leach followed by a caustic crack.

## Claims

### Claim 1

A method of leaching at least one rare earth element from an ore material, the method comprising:
(a) combining the ore material and an acid-containing liquid to form a solution, wherein the solution has a normality between about 1N and 6N, the solution has a solids concentration of greater than about 4 g/L and less than about 25 g/L, and the ore has not been roasted prior to forming the solution;
(b) heating the solution up to between about 60 degrees Celsius and 100 degrees Celsius;
(c) allowing the at least one rare earth element in the ore material to dissolve and leach out of the ore to create a liquor comprising the at least one rare earth element;
(d) a separating step; and
(e) a precipitation step.

### Claim 2 (depends on 1)

The method of claim 1 wherein the at least one rare earth element is selected from cerium, lanthanum, praseodymium and neodymium.

### Claim 3 (depends on 2)

The method of claim 2, wherein the at least one rare earth element is cerium.

### Claim 4 (depends on 1)

The method of claim 1, wherein the ore material comprises at least one mineral selected from monazite, xenotime, allanite, cerite, euxenite, fergusonite, bastnaesite, and gadolinite.

### Claim 5 (depends on 4)

The method of claim 4, wherein the at least one mineral is bastnaesite.

### Claim 6 (depends on 1)

The method of claim 1, wherein the acid-containing liquid comprises hydrochloric acid.

### Claim 7 (depends on 5)

The method of claim 5, wherein the normality is between 3N and 6N, inclusive.

### Claim 8 (depends on 1)

The method of claim 1, wherein the solids concentration is between about 15 g/L and about 20 g/L.

### Claim 9 (depends on 8)

The method of claim 8, wherein greater than about 80% of the at least one rare earth element in the ore material is leached into the liquor.

### Claim 10 (depends on 9)

The method of claim 9, wherein the solids concentration is about 15 g/L.

### Claim 11 (depends on 9)

The method of claim 9, wherein the solids concentration is about 20 g/L.

### Claim 12 (depends on 1)

The method of claim 1, wherein the ore material is ground, prior to step (a), to a size having a p80 of about 45 to 25 μm, and the solids concentration is between about 15 g/L and about 20 g/L.

### Claim 13 (depends on 12)

The method of claim 12, wherein about 80% of the ground ore material passes 400 mesh.

### Claim 14 (depends on 1)

The method of claim 1, wherein the solids concentration is between about 15 g/L and about 20 g/L, and further comprising a step (d), after step (c), of separating the liquor from solids in the solution.

### Claim 15 (depends on 14)

The method of claim 14, wherein greater than about 80% of the at least one rare earth element in the ore material is leached into the liquor.

### Claim 16 (depends on 1)

The method of claim 1, further comprising a step (b′), after step (a), of agitating the solution.

### Claim 17 (depends on 1)

The method of claim 1, wherein step (b) includes agitating the solution.

### Claim 18

A method of leaching cerium from a bastnaesite containing ore material, the method comprising:
(a) combining the ore material and a liquid comprising HCl at a ratio of about 15-20 g ore material per liter of liquid, to form a solution, wherein the solution has a normality between about 3N and 5N, the ore material has a p80 size between about 45 and 25 μm, and the ore material has not been roasted prior to forming the solution;
(b) heating the solution up to at least 85 degrees Celsius;
(c) agitating the solution;
(d) allowing the cerium in the ore material to dissolve and leach out of the ore material to create a cerium liquor.

### Claim 19 (depends on 18)

The method of leaching cerium of claim 18, further comprising separating the cerium liquor from solids in the solution.

### Claim 20 (depends on 19)

The method of claim 19, wherein greater than about 80% of the cerium in the ore material leaches into the cerium liquor.