# US 2026/0015684 A1 · Method of manufacturing a stainless steel sheet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0015684 A1
- Document ID: US20260015684A1
- Status: Published application
- Kind: A1
- Application number: 19/259,256
- Filed: 2025-07-03
- Published: 2026-01-15
- Earliest claimed: 2020-04-30
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Masataka YOSHINO; Shino HIROTA; Takuya MATSUMOTO; Ayako TA
- Web page: https://patentgrep.com/patent/US20260015684A1

## CPC

- C21D 9/46: for sheet metals
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 1/22: Martempering
- C21D 1/25: Hardening, combined with annealing between 300 degrees Celsius and 600 degrees Celsius, i.e. heat refining ("Vergüten")
- C21D 1/26: Methods of annealing
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/004: {containing Cr and Ni}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 6/02: Hardening by precipitation
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0247: characterised by the heat treatment
- C21D 8/0263: {following hot rolling}
- C21D 8/0273: {Final recrystallisation annealing}
- C21D 9/18: for knives, scythes, scissors, or like hand cutting tools
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/40: with nickel
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/52: with cobalt
- C22C 38/54: with boron
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A method of manufacturing a stainless steel is provided. The stainless steel contains C, Si, Mn, P, S, Cr, Ni, and N in predetermined amounts. A total volume fraction of Cr-based carbides with a grain size of 2.0 μm or more is ≤10%. A steel slab is held at 1200° C.-1350° C. for at least 30 minutes and then hot rolled to obtain a hot-rolled steel sheet. The hot-rolled steel sheet is coiled, where at least three rolling passes with a finish temperature of ≥1050° C. and a rolling reduction of ≥20% are performed, and a coiling temperature of the hot-rolled steel sheet is ≥600° C. The hot-rolled steel sheet is subjected to hot-rolled sheet annealing to obtain a hot-rolled and annealed steel sheet, where a holding temperature is 750° C.-900° C. and a holding time is ≥10 minutes.

## Claims

### Claim 1

A method of manufacturing a stainless steel, the stainless steel comprising:
a chemical composition containing, in mass %,
C: 0.45% or more and 0.60% or less,
Si: 0.05% or more and 1.00% or less,
Mn: 0.05% or more and 1.00% or less,
P: 0.05% or less,
S: 0.020% or less,
Cr: 13.0% or more and less than 16.0%,
Ni: 0.10% or more and 1.00% or less, and
N: 0.010% or more and 0.200% or less with the balance being Fe and inevitable impurities,
wherein a total volume fraction of Cr-based carbides with a grain size of 2.0 μm or more is 10% or less,
the method comprising:
a first step in which a steel slab having the chemical composition is held at 1200° C. or higher and 1350° C. or lower for at least 30 minutes,
a second step in which the steel slab is hot rolled to obtain a hot-rolled steel sheet and the hot-rolled steel sheet is coiled, and
a third step in which the hot-rolled steel sheet is subjected to hot-rolled sheet annealing to obtain a hot-rolled and annealed steel sheet
wherein in hot rolling of the second step, at least three rolling passes with a finish temperature of 1050° C. or higher and a rolling reduction of 20% or more are performed, and a coiling temperature of the hot-rolled steel sheet is 600° C. or higher, and
in the hot-rolled sheet annealing of the third step, a holding temperature is 750° C. or higher and 900° C. or lower and a holding time is 10 minutes or more.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the chemical composition further contains, in mass %, at least one selected from the group consisting of
Mo: 0.05% or more and 1.00% or less,
Cu: 0.05% or more and 1.00% or less,
Co: 0.05% or more and 0.50% or less,
Al: 0.001% or more and 0.100% or less,
Ti: 0.01% or more and 0.10% or less,
Nb: 0.01% or more and 0.10% or less,
V: 0.05% or more and 0.50% or less,
Zr: 0.01% or more and 0.10% or less,
Mg: 0.0002% or more and 0.0050% or less,
B: 0.0002% or more and 0.0050% or less,
Ca: 0.0003% or more and 0.0030% or less, and
REM: 0.01% or more and 0.10% or less.

### Claim 3 (depends on 1)

The method according to claim 1, comprising the fourth step in which the hot-rolled and annealed steel sheet is cold rolled to obtain a cold-rolled steel sheet.

### Claim 4 (depends on 3)

The method according to claim 3, comprising the fifth step in which the cold-rolled steel sheet is subjected to cold-rolled sheet annealing to obtain a cold-rolled and annealed steel sheet
wherein in the cold-rolled sheet annealing, a holding temperature is 700° C. or higher and 850° C. or lower and a holding time is 5 seconds or more.

### Claim 5 (depends on 1)

The method according to claim 1, comprising the sixth step in which the hot-rolled and annealed steel sheet is subjected to quenching treatment
wherein in the quenching treatment, a holding temperature is 950° C. or higher and 1200° C. or lower, a holding time is 5 seconds or more and 30 minutes or less, and an average cooling rate after holding is 1° C./s or more.

### Claim 6 (depends on 3)

The method according to claim 3, comprising the sixth step in which the cold-rolled steel sheet is subjected to quenching treatment
wherein in the quenching treatment, a holding temperature is 950° C. or higher and 1200° C. or lower, a holding time is 5 seconds or more and 30 minutes or less, and an average cooling rate after holding is 1° C./s or more.

### Claim 7 (depends on 4)

The method according to claim 4, comprising the sixth step in which the cold-rolled and annealed steel sheet is subjected to quenching treatment
wherein in the quenching treatment, a holding temperature is 950° C. or higher and 1200° C. or lower, a holding time is 5 seconds or more and 30 minutes or less, and an average cooling rate after holding is 1° C./s or more.

### Claim 8 (depends on 5)

The method according to claim 5, comprising the seventh step in which the steel sheet subjected to quenching treatment is subjected to a tempering treatment
wherein in the tempering treatment, a holding temperature is 100° C. or higher and 800° C. or lower and a holding time is 5 minutes or more.

### Claim 9 (depends on 6)

The method according to claim 6, comprising the seventh step in which the steel sheet subjected to quenching treatment is subjected to a tempering treatment
wherein in the tempering treatment, a holding temperature is 100° C. or higher and 800° C. or lower and a holding time is 5 minutes or more.

### Claim 10 (depends on 7)

The method according to claim 7, comprising the seventh step in which the steel sheet subjected to quenching treatment is subjected to a tempering treatment
wherein in the tempering treatment, a holding temperature is 100° C. or higher and 800° C. or lower and a holding time is 5 minutes or more.

### Claim 11 (depends on 2)

The method according to claim 2, comprising the fourth step in which the hot-rolled and annealed steel sheet is cold rolled to obtain a cold-rolled steel sheet.

### Claim 12 (depends on 11)

The method according to claim 11, comprising the fifth step in which the cold-rolled steel sheet is subjected to cold-rolled sheet annealing to obtain a cold-rolled and annealed steel sheet
wherein in the cold-rolled sheet annealing, a holding temperature is 700° C. or higher and 850° C. or lower and a holding time is 5 seconds or more.

### Claim 13 (depends on 2)

The method according to claim 2, comprising the sixth step in which the hot-rolled and annealed steel sheet is subjected to quenching treatment
wherein in the quenching treatment, a holding temperature is 950° C. or higher and 1200° C. or lower, a holding time is 5 seconds or more and 30 minutes or less, and an average cooling rate after holding is 1° C./s or more.

### Claim 14 (depends on 11)

The method according to claim 11, comprising the sixth step in which the cold-rolled steel sheet is subjected to quenching treatment
wherein in the quenching treatment, a holding temperature is 950° C. or higher and 1200° C. or lower, a holding time is 5 seconds or more and 30 minutes or less, and an average cooling rate after holding is 1° C./s or more.

### Claim 15 (depends on 12)

The method according to claim 12, comprising the sixth step in which the cold-rolled and annealed steel sheet is subjected to quenching treatment
wherein in the quenching treatment, a holding temperature is 950° C. or higher and 1200° C. or lower, a holding time is 5 seconds or more and 30 minutes or less, and an average cooling rate after holding is 1° C./s or more.

### Claim 16 (depends on 13)

The method according to claim 13, comprising the seventh step in which the steel sheet subjected to quenching treatment is subjected to a tempering treatment
wherein in the tempering treatment, a holding temperature is 100° C. or higher and 800° C. or lower and a holding time is 5 minutes or more.

### Claim 17 (depends on 14)

The method according to claim 14, comprising the seventh step in which the steel sheet subjected to quenching treatment is subjected to a tempering treatment
wherein in the tempering treatment, a holding temperature is 100° C. or higher and 800° C. or lower and a holding time is 5 minutes or more.

### Claim 18 (depends on 15)

The method according to claim 15, comprising the seventh step in which the steel sheet subjected to quenching treatment is subjected to a tempering treatment
wherein in the tempering treatment, a holding temperature is 100° C. or higher and 800° C. or lower and a holding time is 5 minutes or more.