# US 2026/0015449 A1 · Method of preparing vinyl cyanide compound-conjugated diene rubber-aromatic vinyl compound graft copolymer, method of preparing thermoplastic resin composition including the same, and thermoplastic resin composition including the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0015449 A1
- Document ID: US20260015449A1
- Status: Published application
- Kind: A1
- Application number: 19/330,638
- Filed: 2025-09-16
- Published: 2026-01-15
- Earliest claimed: 2020-10-08
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Young Hwan JEONG; Jaemin SUK; Young Min KIM
- Web page: https://patentgrep.com/patent/US20260015449A1

## CPC

- C08F 136/06: Butadiene
- C08F 279/04: Vinyl aromatic monomers and nitriles as the only monomers
- C08C 1/07: characterised by the agglomerating agents used
- C08F 2/24: with the aid of emulsifying agents
- C08F 2/38: Polymerisation using regulators, e.g. chain terminating agents {, e.g. telomerisation}
- C08F 2/44: Polymerisation in the presence of compounding ingredients, e.g. plasticisers, dyestuffs, fillers
- C08F 4/40: Redox systems
- C08F 6/003: {from polymer solutions, suspensions, dispersions or emulsions without recovery of the polymer therefrom}
- C08F 6/18: Increasing the size of the dispersed particles
- C08L 25/12: with unsaturated nitriles
- C08L 55/02: ABS [Acrylonitrile-Butadiene-Styrene] polymers
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08C: TREATMENT OR CHEMICAL MODIFICATION OF RUBBERS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A thermoplastic resin including 15 to 35% by weight of a vinyl cyanide compound-conjugated diene rubber-aromatic vinyl compound graft copolymer and 65 to 85% by weight of an aromatic vinyl compound-vinyl cyanide compound copolymer. The conjugated diene rubber has an average particle diameter of 2,800 to 3,800 Å and a full width at half maximum of 1,400 to 2,700 Å in particle size distribution. The thermoplastic resin composition has an Izod impact strength of 40 kgf·cm/cm or more as measured using a specimen having a thickness of ⅛″ according to ASTM D256.

## Claims

### Claim 1

A thermoplastic resin composition, comprising 15 to 35% by weight of a vinyl cyanide compound-conjugated diene rubber-aromatic vinyl compound graft copolymer and 65 to 85% by weight of an aromatic vinyl compound-vinyl cyanide compound copolymer,
wherein the conjugated diene rubber has an average particle diameter of 2,800 to 3,800 Å and a full width at half maximum of 1,400 to 2,700 Å in particle size distribution, and
the thermoplastic resin composition has an Izod impact strength of 40 kgf·cm/cm or more as measured using a specimen having a thickness of ⅛″ according to ASTM D256.

### Claim 2 (depends on 1)

The thermoplastic resin composition according to claim 1, wherein the thermoplastic resin composition has a reflection haze of 1.1 or less as measured using RhopointQ equipment (manufacturer: Rhopoint instruments Co.) according to ASTM E430.

### Claim 3 (depends on 1)

The thermoplastic resin composition according to claim 1, wherein the thermoplastic resin composition has a gloss of 97 or more as measured at 45° according to ASTM D528.

### Claim 4 (depends on 1)

The thermoplastic resin composition according to claim 1, wherein, when 100 kg of a resin is injected in a cycle of 30 seconds at a cylinder temperature of 230° C. and a mold temperature of 25° C. using an injection machine (ENGEL Co., clamping force: 150 tons), in a case of the thermoplastic resin composition, an amount of injection mold deposits remaining on a plate is 93 mg or less.

### Claim 5 (depends on 1)

The thermoplastic resin composition according to claim 1, wherein, when 100 kg of a resin is injected in a cycle of 30 seconds at a cylinder temperature of 220° C. and a mold temperature of 30° C. using an injection machine (VICTORY, ENGEL Co., clamping force: 150 tons), in a case of the thermoplastic resin composition, an amount of injection mold deposits remaining on a plate is 93 mg or less.

### Claim 6 (depends on 1)

A molded article, comprising the thermoplastic resin composition according to claim 1.