# US 2026/0015442 A1 · Resin-Based Flooring Product, Process, and Composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0015442 A1
- Document ID: US20260015442A1
- Status: Published application
- Kind: A1
- Application number: 19/266,418
- Filed: 2025-07-11
- Published: 2026-01-15
- Earliest claimed: 2024-07-12
- Assignees: Lionweld Kennedy Flooring Limited
- Applicants: Lionweld Kennedy Flooring Limited
- Inventors: Reece Thompson
- Web page: https://patentgrep.com/patent/US20260015442A1

## CPC

- C08F 124/00: Homopolymers of compounds having one or more unsaturated aliphatic radicals, each having only one carbon-to-carbon double bond, and at least one being terminated by a heterocyclic ring containing oxygen (cyclic esters of polyfunctional acids C08F118/00; cyclic anhydrides of unsaturated acids C08F120/00, C08F122/00)
- C08J 5/043: {with glass fibres}
- C08J 5/10: characterised by the additives used in the polymer mixture
- C08J 5/244: {using glass fibres}
- C08L 71/14: Furfuryl alcohol polymers
- B29C 70/345: {using matched moulds}
- B29K 2086/00: Use of specific polymers obtained by polycondensation or polyaddition, not provided for in a single one of main groups {B29K2059/00 - B29K2085/00}, as moulding material
- B29K 2309/08: Glass
- B29K 2311/10: Natural fibres, e.g. wool or cotton
- B29L 2031/10: Building elements, e.g. bricks, blocks, tiles, panels, posts, beams {(frameless domes B29L2025/00, doors B29L2031/724)}
- C08J 2371/14: Furfuryl alcohol polymers
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

A resin composition for forming a structural element such as a flooring panel includes a resin system including: 45-60 wt % of a plant-derived polyfurfuryl alcohol resin; up to 15 wt % of a non-structural filler such as talc or jute fibre; and 35-40 wt % of a glass fibre. 5 A method of making the structural element includes mixing the resin and filler to produce the resin system; laying up multiple layers of the resin system and the glass fibre in a mould; subjecting the mould to an initial heating profile in an initial resin curing step so that the resin system undergoes a condensation reaction and such that substantially all of the water produced in the condensation reaction has been removed, wherein the heating profile comprises a first, an intermediate, and a final temperature. The product is subsequently subjected to a post-curing step comprising a Diels-Alder reaction.

## Claims

### Claim 1

A method of making a structural element by moulding a resin composition, comprising:
a resin system comprising:
45-60 wt % of a plant-derived polyfurfuryl alcohol resin; and
up to 15 wt % of a non-structural filler; and
35-40 wt % of a glass fibre,
the method comprising:
mixing the plant-derived polyfurfuryl alcohol resin and non-structural filler to produce the resin system;
laying up multiple layers of the resin system and the glass fibre in a mould;
subjecting the mould to an initial heating profile in an initial resin curing step so that the resin system undergoes a condensation reaction and such that substantially all of the water produced in the condensation reaction has been removed, wherein the heating profile comprises:
holding the mould at a starting temperature for a first predefined period;
raising the temperature of the mould to an intermediate temperature;
holding the mould at the intermediate temperature for a second predefined period;
raising the temperature of the mould to a final temperature;
holding the mould at the final temperature for a third predefined period;
cooling the mould to ambient temperature; and
removing the product from the mould; and
subsequently subjecting the product to a further heating profile so as to undergo a post-curing step comprising a Diels-Alder reaction, the further heating step comprising:
heating the product to a fourth temperature that is higher than the third temperature;
holding the product at the fourth temperature for a fourth predefined period; and
cooling the product to ambient temperature.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein:
the first temperature is about 50° C., and the first predetermined period is about 4 hours
the second temperature is about 60° C., and the second predetermined period is about 1 hour;
the third temperature is about 80° C., and the third predetermined period is about three hours; and
the fourth temperature is about 110° C., and the fourth predetermined period is about three hours.

### Claim 3 (depends on 1)

The method as claimed in claim 1, comprising performing the initial heating profile with the mould in an oven or using a self-heating mould.

### Claim 4 (depends on 1)

The method as claimed in claim 1, further comprising at least one of adding an internal release agent to the resin composition and coating the surface of the mould with external release agent before laying up.

### Claim 5 (depends on 1)

The method as claimed in claim 1, further comprising adding grit to the final layer of resin when laying up.

### Claim 6 (depends on 1)

The method as claimed in claim 1, further comprising laying up at least one layers of jute fibre as final layers.

### Claim 7 (depends on 1)

The method as claimed in claim 1, comprising laying up 10 layers of glass fibre, or nine layers of glass fibre and two layers of jute, or 11 layers of glass fibre and one layer of jute.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein one layer comprises four rovings of glass fibre or jute fibre in the mould.

### Claim 9 (depends on 1)

The method as claimed in claim 1, wherein the resin system further comprises:
up to 5 wt % of a solvent such as water; and
4-6 wt % of a catalyst system.

### Claim 10 (depends on 1)

The method as claimed in claim 1, wherein the glass fibre is an E-glass or E-CR glass having a tensile strength of greater than 2000 MPa.

### Claim 11 (depends on 1)

The method as claimed in claim 1, wherein the non-structural filler comprises:
up to 5 wt % talcum powder; and
up to 10 wt % jute fibre.

### Claim 12 (depends on 1)

The method as claimed in claim 1, wherein the structural element is a load bearing element such as a flooring panel.

### Claim 13 (depends on 12)

The method as claimed in claim 12, wherein the load bearing element comprises a load bearing surface in the form of an open grating or mesh, or a panel with a substantially solid load bearing surface.

### Claim 14

A resin composition, comprising:
a resin system comprising:
45-60 wt % of a plant-derived polyfurfuryl alcohol resin; and
up to 15 wt % of a non-structural filler; and
35-40 wt % of a glass fibre.

### Claim 15 (depends on 14)

The resin composition as claimed in claim 14, wherein the resin system further comprises:
up to 5 wt % of a solvent such as water; and
4-6 wt % of a catalyst system.

### Claim 16 (depends on 14)

The resin composition as claimed in claim 14, wherein the glass fibre is an E-glass or E-CR glass having a tensile strength of greater than 2000 MPa.

### Claim 17 (depends on 14)

The resin composition as claimed in claim 14, wherein the non-structural filler comprises:
up to 5 wt % talcum powder; and
up to 10 wt % jute fibre.

### Claim 18 (depends on 14)

The structural element having a predetermined shape formed by moulding the composition of claim 14.

### Claim 19 (depends on 18)

The structural element as claimed in claim 18, comprising a load bearing element such as a flooring panel.

### Claim 20 (depends on 19)

The structural element as claimed in claim 19, wherein the load bearing element comprises a load bearing surface in the form of an open grating or mesh, or a panel with a substantially solid load bearing surface.