# US 2026/0008891 A1 · Rubber filler, rubber composite comprising the same, and preparation method therefor and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0008891 A1
- Document ID: US20260008891A1
- Status: Published application
- Kind: A1
- Application number: 18/992,635
- Filed: 2023-11-09
- Published: 2026-01-08
- Earliest claimed: 2023-06-13
- Assignees: PetroChina Company Limited
- Applicants: Petrochina Company Limited
- Inventors: Gongchang SHI; Zhichao ZHAO; Hailong YANG; Yongfeng WANG; Wei SHAO; Qilin ZHONG; Qiang GUI; Zhiqiang ZHANG; Jing DONG; Guangbi GONG
- Web page: https://patentgrep.com/patent/US20260008891A1

## CPC

- C08J 3/126: {Polymer particles coated by polymer, e.g. core shell structures}
- B60C 1/0016: {Compositions of the tread}
- B60C 11/0008: {characterised by the tread rubber}
- C08K 3/36: Silica
- C08K 9/04: Ingredients treated with organic substances {(treated with macromolecular compounds C08K9/08)}
- C08L 9/00: Compositions of homopolymers or copolymers of conjugated diene hydrocarbons
- C08L 9/06: Copolymers with styrene
- C08L 23/22: Copolymers of isobutene; Butyl rubber; Homopolymers or copolymers of other iso-olefins
- C09C 1/56: Treatment of carbon black {; Purification}
- C09C 3/10: Treatment with macromolecular organic compounds {(C09C3/006 takes precedence)}
- B60C 2011/0025: {Modulus or tan delta}
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- C08F 112/36: Divinylbenzene
- C08J 2325/16: Homopolymers or copolymers of alkyl-substituted styrenes
- C08J 2479/02: Polyamines
- C08K 2201/011: Nanostructured additives
- C08K 2201/013: Additives applied to the surface of polymers or polymer particles
- C08L 2207/53: Core-shell polymer
- Y02T 10/86: Optimisation of rolling resistance, e.g. weight reduction
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B60C: VEHICLE TYRES; TYRE INFLATION; TYRE CHANGING; CONNECTING VALVES TO INFLATABLE ELASTIC BODIES IN GENERAL; DEVICES OR ARRANGEMENTS RELATED TO TYRES
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09C: TREATMENT OF INORGANIC MATERIALS, OTHER THAN FIBROUS FILLERS, TO ENHANCE THEIR PIGMENTING OR FILLING PROPERTIES (treatment of materials specially adapted to enhance their filling properties in mortars, concrete or artificial stone C04B14/00, C04B18/00, C04B20/00); PREPARATION OF CARBON BLACK {; PREPARATION OF INORGANIC MATERIALS WHICH ARE NO SINGLE CHEMICAL COMPOUNDS AND WHICH ARE MAINLY USED AS PIGMENTS OR FILLERS}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION

## Abstract

The present disclosure discloses a rubber filler, a rubber composite including the same, a preparation method therefor, and use thereof. The rubber filler includes polydivinylbenzene microspheres and polydopamine-modified white carbon black loaded on the polydivinylbenzene microspheres; wherein the mass ratio of the polydivinylbenzene microspheres to the polydopamine-modified white carbon black is 1:(0.5-20). The rubber composite includes: a solution polymerized crude rubber and the rubber filler; wherein the rubber filler is added in an amount of 10-60 wt % of the dry basis mass of the solution polymerized crude rubber. The present disclosure uses polydivinylbenzene microspheres loaded with polydopamine-modified white carbon black as the filler, solving the problem that the white carbon black is apt to agglomerate and the white carbon black has poor binding force with the rubber. The rubber composite obtained by the present disclosure is suitable for manufacturing green tires.

## Claims

### Claim 1

A rubber filler comprising: polydivinylbenzene microspheres and polydopamine-modified white carbon black loaded on the polydivinylbenzene microspheres, wherein the mass ratio of the polydivinylbenzene microspheres to the polydopamine-modified white carbon black is 1:(0.5-20).

### Claim 2 (depends on 1)

The rubber filler according to claim 1, wherein the mass ratio of the polydivinylbenzene microspheres to the polydopamine-modified white carbon black is 1:(1-10); or the mass ratio of the white carbon black and polydopamine in the polydopamine-modified white carbon black is 1:(0.05-1).

### Claim 3 (depends on 1)

The rubber filler according to claim 1, wherein the polydivinylbenzene microspheres have a particle size within the range of 0.1-1 m.

### Claim 4 (depends on 1)

The rubber filler according to claim 1, wherein the white carbon black has a particle size within the range of 20-60 nm.

### Claim 5

A method for preparing the rubber filler comprising:
(1) carrying out a first reaction on the white carbon black and dopamine in a first buffer solution to obtain a polydopamine-modified white carbon black;
(2) subjecting the polydivinylbenzene microspheres to a second reaction in a second buffer solution with the polydivinylbenzene microspheres obtained in step (1) to obtain the polydivinylbenzene microspheres loaded with polydopamine-modified white carbon black; wherein the mass ratio of the polydivinylbenzene microspheres to the polydopamine-modified white carbon black is 1:(0.5-20).

### Claim 6 (depends on 5)

The method according to claim 5, wherein step (1) specifically comprising:
adding an inorganic acid or inorganic base into a weak alkalinity buffering agent solution to obtain a first buffer solution with a pH of 7.5-10.5, wherein the concentration of the buffering agent in the first buffer solution is within the range of 3-15 mmol/L;
adding white carbon black and dopamine into the first buffer solution, carrying out the reaction for 0.5-2 h at room temperature, and then filtering, washing, and drying to obtain the polydopamine-modified white carbon black.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the mass ratio of the white carbon black and dopamine is 1:(0.05-1);
or the mass ratio of the white carbon black to the first buffer solution is 1:(5-50);
or the weak alkalinity buffering agent is one or more selected from the group consisting of trihydroxymethyl aminomethane, barbital, barbital-sodium chloride composite buffering agent, boric acid-potassium chloride composite buffering agent, borax-calcium chloride composite buffering agent, disodium hydrogen phosphate, and dipotassium hydrogen phosphate-potassium dihydrogen phosphate composite buffering agent;
or the inorganic acid is one or more of hydrochloric acid, nitric acid, sulfuric acid, and phosphoric acid;
or the inorganic base is potassium hydroxide and/or sodium hydroxide.

### Claim 8 (depends on 5)

The method according to claim 5, wherein step (2) specifically comprising:
adding an inorganic acid or inorganic base into a weak alkalinity buffering agent solution to obtain a second buffer solution with a pH of 7.5-10.5, wherein the concentration of the buffering agent in the second buffer solution is within the range of 3-15 mmol/L;
adding polydivinylbenzene microspheres and the polydopamine-modified white carbon black obtained in step (1) into the second buffer solution, carrying out the reaction with magnetic stirring at room temperature for 1-4 h, then filtering, washing, and drying the reaction product to obtain the polydivinylbenzene microspheres loaded with the polydopamine-modified white carbon black.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the mass ratio of the polydivinylbenzene microspheres to the polydopamine-modified white carbon black is 1:(1-10);
or the mass ratio of the polydivinylbenzene microspheres and the second buffer solution is 1(50-500);
or the weak alkalinity buffering agent is one or more selected from the group consisting of trihydroxymethyl aminomethane, barbital, barbital-sodium chloride composite buffering agent, boric acid-potassium chloride composite buffering agent, borax-calcium chloride composite buffering agent, disodium hydrogen phosphate, and dipotassium hydrogen phosphate-potassium dihydrogen phosphate composite buffering agent;
or the inorganic acid is one or more of hydrochloric acid, nitric acid, sulfuric acid, and phosphoric acid;
or the inorganic base is potassium hydroxide and/or sodium hydroxide.

### Claim 10 (depends on 1)

A rubber composite comprising: a solution polymerized crude rubber, a first filler, and a second filler, wherein the first filler is the rubber filler according to claim 1, and the second filler is a polydopamine-modified white carbon black; the total addition amount of the first rubber filler and the second rubber filler is 10-60 wt % of the dry basis mass of the solution polymerized crude rubber.

### Claim 11 (depends on 10)

The rubber composite according to claim 10, wherein the mass ratio of the first filler and the second filler is 1:(0.5-20).

### Claim 12 (depends on 10)

The rubber composite according to claim 10, wherein the addition amount of the second rubber filler is 10-40 wt % of the dry basis mass of the solution polymerized crude rubber.

### Claim 13 (depends on 10)

The rubber composite according to claim 10, wherein the rubber composite further comprises an auxiliary agent.

### Claim 14 (depends on 13)

The rubber composite according to claim 13, wherein the auxiliary agent is one or more selected from the group consisting of a vulcanizing agent, an anti-aging agent, an accelerant, and an activator.

### Claim 15 (depends on 10)

The rubber composite according to claim 10, wherein the solution-polymerized crude rubber is one or more selected from the group consisting of solution-polymerized styrene-butadiene rubber, polyisoprene rubber, cis-butadiene rubber, and butyl rubber.

### Claim 16 (depends on 1)

A method for preparing the rubber composite comprising:
mixing the solution polymerized crude rubber with a first filler and a second filler, and then vulcanizing the mixture to prepare a rubber composite; wherein the first filler is the rubber filler according to claim 1, and the second filler is a polydopamine-modified white carbon black; the total addition amount of the first rubber filler and the second rubber filler is 10-60 wt % of the dry basis mass of the solution polymerized crude rubber.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the mass ratio of the first filler and the second filler is 1:(0.5-20);
or the addition amount of the second rubber filler is 10-40 wt % of the dry basis mass of the solution polymerized crude rubber.

### Claim 18

(canceled)

### Claim 19 (depends on 16)

The method according to claim 16, wherein an auxiliary agent is further added in the mixing step:
or the auxiliary agent is one or more selected from the group consisting of a vulcanizing agent, an anti-aging agent, an accelerant, and an activator.

### Claim 20

(canceled)

### Claim 21 (depends on 16)

The method according to claim 16, wherein the solution-polymerized crude rubber is one or more selected from the group consisting of solution-polymerized styrene-butadiene rubber, polyisoprene rubber, cis-butadiene rubber, and butyl rubber.

### Claim 22 (depends on 10)

A tire comprising the rubber composite according to claim 10.