# US 2026/0008097 A1 · Material and process for high throughput binder jet printing of titanium & particle reinforced titanium alloy parts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0008097 A1
- Document ID: US20260008097A1
- Status: Published application
- Kind: A1
- Application number: 18/763,477
- Filed: 2024-07-03
- Published: 2026-01-08
- Earliest claimed: 2024-07-03
- Assignees: Spirit AeroSystems, Inc.
- Applicants: Spirit AeroSystems, Inc.
- Inventors: Rahbar Nasserrafi; Gerald Hicks; Paul Ray Toivonen; Daniel Klenosky
- Web page: https://patentgrep.com/patent/US20260008097A1

## CPC

- B22F 1/09: {Mixtures of metallic powders}
- B22F 3/1021: {Removal of binder or filler (removal of binder from ceramics C04B35/638)}
- B22F 3/26: Impregnating {(making ferrous alloys by impregnation C22C33/0242)}
- B22F 10/14: by jetting of binder onto a bed of metal powder
- B22F 10/22: Direct deposition of molten metal
- B22F 10/32: of the atmosphere, e.g. composition or pressure in a building chamber
- B22F 10/368: Temperature or temperature gradient, e.g. temperature of the melt pool
- B22F 10/64: by thermal means (control of energy beam parameters for post heating B22F10/364)
- B33Y 10/00: Processes of additive manufacturing
- B33Y 40/20: Post-treatment, e.g. curing, coating or polishing
- B33Y 70/00: Materials specially adapted for additive manufacturing
- C22C 1/0458: {Alloys based on titanium, zirconium or hafnium}
- C22C 14/00: Alloys based on titanium
- C22F 1/183: {of titanium or alloys based thereon}
- B22F 2201/20: Use of vacuum
- B22F 2203/11: temperature, temperature profile
- B22F 2301/205: Titanium, zirconium or hafnium
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

Titanium-based alloy powder formulations and methods for use with the powder formulations are disclosed. The formulations and methods disclosed herein enable rapid binder jet manufacturing of large high performance titanium parts.

## Claims

### Claim 1

A powder formulation comprising:
a titanium alloy; and
one or more of:
from about 5 wt. % to about 19 wt. % tin (Sn);
no greater than 5 wt. % aluminum (Al);
no greater than 5 wt. % antimony (Sb); and
no greater than 2 wt. % bismuth (Bi).

### Claim 2 (depends on 1)

The powder formulation of claim 1 further comprising:
from about 0.05 wt. % to about 0.25 wt. % oxygen (O);
from about 0.1 wt. % to about 0.4 wt. % carbon (C);
not greater than 0.03 wt. %. nitrogen (N).

### Claim 3 (depends on 2)

The powder formulation of claim 2
wherein the sum of C, O, and N, is no greater than 0.45 wt. %.

### Claim 4 (depends on 1)

The powder formulation of claim 1, wherein the sum of Sn, Sb and Bi is no greater than 20 wt. %.

### Claim 5 (depends on 1)

The powder formulation of claim 1 further comprising a beta stabilizing element selected from the group consisting of molybdenum (Mo), vanadium (V), chromium (Cr), iron (Fe), manganese (Mn), niobium (Nb) or any combination thereof.

### Claim 6 (depends on 1)

The powder formulation of claim 1 further comprising one or more highly reactive element selected from the group consisting of Erbium (Er), yttrium (Y), gallium (Ga), germanium (Ge), and scandium (Sc).

### Claim 7

A method of metal binder jet printing for forming a metal part, the method comprising:
depositing a powder formulation onto a build platform to form a powder formulation layer, the powder formulation comprising:
a titanium alloy; and
one or more of:
from about 5 to about 19 wt. % tin (Sn);
no greater than 5 wt. % aluminum (Al);
no greater than 5 wt. % antimony (Sb); and
no greater than 2 wt. % bismuth (Bi);
depositing binder onto the powder formulation layer to bond the powder formulation layer into a bound layer; and
curing of the bound layer to form a metal part.

### Claim 8 (depends on 7)

The method of claim 7, wherein the powder formulation further comprises a beta stabilizing element is selected from the group consisting of molybdenum (Mo), vanadium (V), chromium (Cr), niobium (Nb), iron (Fe), manganese (Mn), or any combination thereof.

### Claim 9 (depends on 7)

The method of claim 7, wherein the powder formulation comprises one or more highly reactive element selected from the group consisting of erbium (Er), yttrium (Y), gallium (Ga), germanium (Ge), and scandium (Sc).

### Claim 10 (depends on 7)

The method of claim 7, comprising repeating the steps of depositing the powder formulation onto the build platform and depositing binder onto the powder formulation layer to bond the powder formulation to provide a powder stack, each powder formulation deposited will independently have a thickness of from about 50 to about 250 micrometers.

### Claim 11 (depends on 7)

The method of claim 7 comprising depositing from about 0.001″ to about 0.003″ binder onto the powder formulation.

### Claim 12 (depends on 7)

The method of claim 7 further comprising one or more of the following:
de-binding the bound layer;
vacuum sintering the de-bonded layer; and
heat treating the layer to form the metal part.

### Claim 13

A method of metal binder jet printing for forming a metal part, the method comprising:
depositing a powder formulation comprising a titanium alloy onto a build platform to form a powder formulation layer;
depositing a binder onto the powder formulation layer to bond the powder formulation layer into a bound layer;
curing the bound layer and removing the cured layer from any lose powder formulation;
de-binding the cured layer;
partially sintering the de-bonded layer;
liquid metal infiltrating the partially-sintered metal part with a composition of one or more of:
from about 5 wt. % to about 19 wt. % tin (Sn);
no greater than 5 wt. % aluminum (Al);
no greater than 5 wt. % antimony (Sb); and
no greater than 2 wt. % bismuth (Bi); and
heat treating the infiltrated partially-sintered metal part for a time period to solidify the metal part.

### Claim 14 (depends on 13)

The method of claim 13, wherein the surface of the infiltrated partially-sintered metal part is covered with a protective layer prior to heating, wherein the protective layer comprises ceramic or glass.

### Claim 15 (depends on 13)

The method of claim 13, wherein the infiltrated partially-sintered metal part has a ramp rate of from about 50° F./hour to about 1000° F./hour.

### Claim 16 (depends on 13)

The method of claim 13, where the infiltrated partially-sintered metal part has a hold time of from about 30 minutes to about 4 hours at infiltration temperature.

### Claim 17 (depends on 13)

The method of claim 13, where the temperature of the infiltrating liquid metal is below 850° F.

### Claim 18 (depends on 13)

The method of claim 13, wherein the powder formulation comprises a beta stabilizing element selected from the group consisting of molybdenum (Mo), vanadium (V), chromium (Cr), niobium (Nb), iron (Fe), manganese (Mn), or any combination thereof.

### Claim 19 (depends on 13)

The method of claim 13, wherein the powder formulation further comprises one or more highly reactive element selected from the group consisting of Erbium (Er), yttrium (Y), gallium (Ga), germanium (Ge), and scandium (Sc).

### Claim 20 (depends on 13)

The method of claim 13, wherein the binder is a composition of one or more of:
from about 5 to about 19 wt. % tin (Sn);
no greater than 5 wt. % aluminum (Al);
no greater than 5 wt. % antimony (Sb); and
no greater than 2 wt. % bismuth (Bi).