# US 2026/0008035 A1 · Catalyst for reforming methane, method for producing same, and method for reforming methane

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0008035 A1
- Document ID: US20260008035A1
- Status: Published application
- Kind: A1
- Application number: 18/729,996
- Filed: 2023-09-21
- Published: 2026-01-08
- Earliest claimed: 2022-10-21
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Suji Kim; Jun Yeon Cho; Jae Soon Choi; Jun Seon Choi; Sangjin Kim; Sojin Kim; Yongseon Kim; Hyun A Choi
- Web page: https://patentgrep.com/patent/US20260008035A1

## CPC

- B01J 23/002: {Mixed oxides other than spinels, e.g. perovskite}
- B01J 23/83: with rare earths or actinides
- B01J 21/06: Silicon, titanium, zirconium or hafnium; Oxides or hydroxides thereof
- B01J 23/00: Catalysts comprising metals or metal oxides or hydroxides, not provided for in group B01J21/00 (B01J21/16 takes precedence)
- B01J 23/02: of the alkali- or alkaline earth metals or beryllium
- B01J 23/10: of rare earths
- B01J 23/755: Nickel
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C01B 3/40: characterised by the catalyst
- C01B 2203/0227: containing a catalytic reforming step
- C01B 2203/0233: the reforming step being a steam reforming step
- C01B 2203/0238: the reforming step being a carbon dioxide reforming step
- C01B 2203/0244: the reforming step being an autothermal reforming step, e.g. secondary reforming processes
- C01B 2203/0261: containing a catalytic partial oxidation step [CPO]
- C01B 2203/1047: Group VIII metal catalysts
- C01B 2203/1052: Nickel or cobalt catalysts
- C01B 2203/1058: Nickel catalysts
- C01B 2203/1064: Platinum group metal catalysts
- Y02P 20/52: using catalysts, e.g. selective catalysts
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided are a catalyst for methane reformation, a method for manufacturing the same, and a methane reforming method, wherein the catalyst is represented by Chemical Formula 1 below: wherein all the variables are described herein.

## Claims

### Claim 1

A catalyst for methane reformation, wherein the catalyst is represented by Chemical Formula 1:
in Chemical Formula 1,
A is Y, La or Ba,
B is Ni, Co, Fe, Mn, Cr, Mo, Ru or Rh,
0<x<0.8,
0<y <0.3, and
0≤δ<1.

### Claim 2 (depends on 1)

The catalyst of claim 1, wherein in Chemical Formula 1,
0<x<0.2, and
0<y<0.25.

### Claim 3 (depends on 1)

The catalyst of claim 1, wherein in Chemical Formula 1 A is Y and B is Ni.

### Claim 4 (depends on 1)

The catalyst of claim 1, which is applied to a steam reforming process, a carbon dioxide (CO2) reforming process, a catalytic partial oxidation process, an autothermal reforming process, a tri-reforming process, or a mixed reforming process.

### Claim 5

A method for manufacturing a catalyst for methane reformation, wherein the catalyst is represented by Chemical Formula 1,
in Chemical Formula 1,
A is Y, La or Ba,
B is Ni, Co, Fe, Mn, Cr, Mo, Ru or Rh,
0<x<0.8,
0<y<0.3, and
0≤δ<1,
the method comprising:
preparing a solution comprising a calcium (Ca) precursor, a precursor comprising the A of Chemical Formula 1, a zirconium (Zr) precursor, and a precursor comprising the B of Chemical Formula 1;
stirring the solution; and
drying and firing the stirred solution.

### Claim 6 (depends on 5)

The method of claim 5, wherein the calcium precursor, the precursor comprising the A of Chemical Formula 1, the zirconium precursor, and the precursor comprising the B of Chemical Formula 1 are each one or more selected from the group consisting of a nitrate, a carbonate, a chloride, and an ammonium salt of calcium, the A or the B or a hydrate thereof, respectively.

### Claim 7 (depends on 5)

The method of claim 5, wherein the A of Chemical Formula 1 is 5 mol % to 20 mol % relative to calcium in the solution.

### Claim 8 (depends on 5)

The method of claim 5, wherein the B of Chemical Formula 1 is 3 mol % to 25 mol % relative to zirconium in the solution.

### Claim 9 (depends on 5)

The method of claim 5, wherein in Chemical Formula 1,
0<x<0.2,
0<y<0.25, and
0≤δ<1.

### Claim 10 (depends on 5)

The method of claim 5, wherein in Chemical Formula 1, A is Y and B is Ni.

### Claim 11 (depends on 1)

A method for forming methane, comprising:
filling a reactor with the catalyst according to claim 1;
activating the catalyst;
supplying a feed gas to the reactor; and
applying heat and pressure to the feed gas.

### Claim 12 (depends on 5)

The method of claim 5, wherein the calcium (Ca) precursor is Ca(NO3)2·H2O, the precursor comprising the A of Chemical Formula 1 is Y(NO3)2, the zirconium (Zr) precursor is ZrO(NO3)2·H2O, and the precursor comprising the B of Chemical Formula 1 is Ni(NO3)2.

### Claim 13 (depends on 5)

The method of claim 5, wherein the solution comprises a solvent of distilled water, citric acid, ethylene glycol, urea, or a combination thereof.

### Claim 14 (depends on 5)

The method of claim 5, wherein the step of stirring the solution is carried out at temperatures ranging from 60° C. to 90° C. for 1 hour to 5 hours.

### Claim 15 (depends on 11)

The method of claim 11, wherein the step of activating the catalyst is carried out at 700° C. to 900° C. under H2 and N2.

### Claim 16 (depends on 11)

The method of claim 11, wherein the feed gas comprises methane (CH4), carbon dioxide (CO2) and nitrogen (N2).

### Claim 17 (depends on 16)

The method of claim 16, wherein a volume ratio of methane (CH4), carbon dioxide (CO2) and nitrogen (N2) is 1:1 to 1.4:0.1 to 1.

### Claim 18 (depends on 11)

The method of claim 11, wherein the step of applying heat and pressure to the feed gas is carried out at 700° C. to 900° C., and 0.5 bar to 1.5 bar.