# US 2026/0008034 A1 · Low-carbon alkane dehydrogenation catalyst, preparation method therefor and application thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0008034 A1
- Document ID: US20260008034A1
- Status: Published application
- Kind: A1
- Application number: 18/992,137
- Filed: 2023-07-06
- Published: 2026-01-08
- Earliest claimed: 2022-07-07
- Assignees: Rezel Engineering Co., Ltd
- Applicants: Rezel Engineering Co., Ltd
- Inventors: Ruiling ZHAO; Runsheng ZHUO; Qiushi SUN; Bing LIU; Xingyue LAN; Chunxue ZHANG; Yusen RAO; Xinsheng LIU
- Web page: https://patentgrep.com/patent/US20260008034A1

## CPC

- B01J 23/62: with gallium, indium, thallium, germanium, tin or lead
- B01J 6/001: {Calcining}
- B01J 23/10: of rare earths
- B01J 23/626: {with tin}
- B01J 23/6562: {Manganese}
- B01J 35/613: {10-100 m2/g}
- B01J 35/638: {more than 1.0 ml/g}
- B01J 35/647: {2-50 nm}
- B01J 37/02: Impregnation, coating or precipitation ({B01J37/0009 and B01J37/0018 take precedence } ; protection by coating B01J33/00)
- B01J 37/0201: {Impregnation}
- B01J 37/036: {to form a gel or a cogel}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C07C 5/325: {of the platinum group}
- C07C 5/3337: {of the platinum group}
- C07C 9/08: Propane
- C07C 9/12: Iso-butane
- C07C 2521/04: Alumina
- C07C 2523/06: of zinc, cadmium or mercury
- C07C 2523/08: of gallium, indium or thallium
- C07C 2523/14: of germanium, tin or lead
- C07C 2523/42: Platinum
- C07C 2523/44: Palladium
- C07C 2523/46: Ruthenium, rhodium, osmium or iridium
- C07C 2523/63: with rare earths or actinides
- Y02P 20/52: using catalysts, e.g. selective catalysts
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention provides a light alkane dehydrogenation catalyst, and a preparation method and application thereof, and belongs to the technical field of petrochemical technology. The catalyst uses at least one of precious metals Pt, Pd, Ru and Rh as an active component, at least one of transition metals Ga, V, In, Sn, Mn, Ce, Fe and Ni as a promoter, and a modified zinc aluminate carrier as a carrier; the chemical composition of the modified zinc aluminate carrier is of the general formula ZnMxAlyO4, where x is 0.01-0.99, y is 0.01-1.99, and it satisfies x+y=2; M is selected from at least one of the rare earth elements La, Ce, Pr, Sm and Er. The catalyst prepared by such a modified zinc aluminate carrier has the characteristics of high propane conversion rate, high selectivity for product propylene, strong resistance to sintering, good stability, etc.

## Claims

### Claim 1

A light alkane dehydrogenation catalyst, wherein the catalyst uses at least one of precious metals Pt, Pd, Ru and Rh as an active component, at least one of transition metals Ga, V, In, Sn, Mn, Fe and Ni as a promoter, and modified zinc aluminate as a carrier;
the modified zinc aluminate carrier has a chemical composition of the general formula ZnMxAlyO4, where x is 0.01-0.99, y is 0.01-1.99, and it satisfies x+y=2; M is selected from at least one of the rare earth elements La, Ce, Pr, Sm and Er.

### Claim 2 (depends on 1)

The light alkane dehydrogenation catalyst according to claim 1, wherein based on the total mass of the catalyst on a dry basis, the content by mass percentage of the active component is 1-40 wt %, the content by mass percentage of the promoter is 1-20 wt %, with the balance being the modified zinc aluminate carrier.

### Claim 3 (depends on 1)

The light alkane dehydrogenation catalyst according to claim 1, wherein the specific surface area of the modified zinc aluminate carrier is 10-100 m2/g, the pore size range is 3 nm-30 nm, and the pore volume range is 0.1-0.7 g/mL.

### Claim 4 (depends on 1)

The light alkane dehydrogenation catalyst according to claim 1, wherein a precursor of the rare earth element is one or more of nitrate of the rare earth element, rare earth metal oxide, rare earth metal sulfate and rare earth metal organic acid salt.

### Claim 5 (depends on 1)

The light alkane dehydrogenation catalyst according to claim 1, wherein a precursor of the precious metal is selected from one or more of metal halides, metal nitrates and metal complexes; and preferably, a precursor of the transition metal is one or more of oxides, inorganic salts or complexes of a metal element.

### Claim 6 (depends on 1)

The light alkane dehydrogenation catalyst according to claim 1, wherein the modified zinc aluminate carrier is prepared by a gel sol method, an impregnation method, a precipitation method, a coprecipitation method or a hydrothermal synthesis method.

### Claim 7 (depends on 6)

The light alkane dehydrogenation catalyst according to claim 6, wherein the modified zinc aluminate carrier is prepared by a precipitation method or a coprecipitation method, and the precipitant used is at least one of ammonia water, sodium hydroxide, potassium hydroxide, sodium carbonate and urea;
preferably, the modified zinc aluminate carrier is prepared by the gel sol method, and the gelling agent used is at least one of citric acid, nitric acid and hydrochloric acid.

### Claim 8 (depends on 1)

A preparation method of the light alkane dehydrogenation catalyst according to claim 1, comprising:
under stirring conditions, adding a solution containing the active component and the promoter dropwise to a dispersion containing the modified zinc aluminate carrier, stirring the mixture for 1-3 hours, recovering the solvent, oven-drying and then calcining.

### Claim 9 (depends on 8)

The preparation method of the light alkane dehydrogenation catalyst according to claim 8, wherein the temperature during the calcining process is 500-700° C. and the time is 3-5 hours.

### Claim 10 (depends on 1)

Application of the light alkane dehydrogenation catalyst according to claim 1, wherein the catalyst is used for propane dehydrogenation, isobutane dehydrogenation, or propane/isobutane mixed gas dehydrogenation, and the catalyst is applied to a fixed bed, a moving bed or a fluidized bed, with a reaction temperature of 550-620° C., a reaction pressure of 10-150 kPa, and a reaction space velocity of 0.1-2 h−1.