# US 2026/0008010 A1 · Exhaust gas purification catalyst and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0008010 A1
- Document ID: US20260008010A1
- Status: Published application
- Kind: A1
- Application number: 19/127,454
- Filed: 2024-03-18
- Published: 2026-01-08
- Earliest claimed: 2023-03-28
- Assignees: Mitsui Mining & Smelting Co., Ltd.
- Applicants: Mitsui Mining & Smelting Co., Ltd.
- Inventors: Yusuke NAGAI; Hiroki KURIHARA; Keitaro NOGUCHI; Akihide MAEDA
- Web page: https://patentgrep.com/patent/US20260008010A1

## CPC

- B01D 53/94: by catalytic processes
- F01N 3/2828: {Ceramic multi-channel monoliths, e.g. honeycombs}
- B01D 53/945: {characterised by a specific catalyst}
- B01J 23/63: with rare earths or actinides
- B01J 35/19: {Catalysts containing parts with different compositions}
- B01J 35/57: Honeycombs
- B01J 35/60: characterised by their surface properties or porosity
- B01J 35/633: {less than 0.5 ml/g}
- B01J 35/635: {0.5-1.0 ml/g}
- B01J 35/657: {larger than 1000 nm}
- B01J 35/66: Pore distribution
- B01J 37/02: Impregnation, coating or precipitation ({B01J37/0009 and B01J37/0018 take precedence } ; protection by coating B01J33/00)
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- F01N 3/022: characterised by specially adapted filtering structure, e.g. honeycomb, mesh or fibrous
- F01N 3/035: with catalytic reactors
- F01N 3/101: {Three-way catalysts}
- F01N 3/24: characterised by constructional aspects of converting apparatus (filtering in combination with catalytic reactors F01N3/035)
- F01N 3/28: Construction of catalytic reactors
- F01N 3/2803: {characterised by structure, by material or by manufacturing of catalyst support}
- B01D 2255/1025: Rhodium
- B01D 2255/407: Zr-Ce mixed oxides
- B01D 2255/9022: Two layers
- B01D 2255/908: O2-storage component incorporated in the catalyst
- B01D 2255/9155: Wall flow filters
- B01D 2255/9205: Porosity
- B01D 2258/01: Engine exhaust gases
- B01D 2258/012: Diesel engines and lean burn gasoline engines
- B01D 2258/014: Stoichiometric gasoline engines
- F01N 2330/30: Honeycomb supports characterised by their structural details
- F01N 2370/02: used in catalytic reactors
- F01N 2510/0684: having more than one coating layer, e.g. multi-layered coatings
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- F01N: GAS-FLOW SILENCERS OR EXHAUST APPARATUS FOR MACHINES OR ENGINES IN GENERAL; GAS-FLOW SILENCERS OR EXHAUST APPARATUS FOR INTERNAL-COMBUSTION ENGINES (arrangements in connection with gas exhaust of propulsion units in vehicles B60K13/00; combustion-air intake silencers specially adapted for, or arranged on, internal-combustion engines F02M35/00; protecting against, or damping, noise in general G10K11/16)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

An object of the present invention is to provide an exhaust gas purification catalyst that can realize improvement of PM collection performance and suppression of an increase in pressure loss, and the present invention provides an exhaust gas purification catalyst (1A) including: a wall-flow type substrate (10); a first catalyst layer (20); and a second catalyst layer (30), wherein, assuming that: Conditions 1 and 2 are defined as the conditions that, in a logarithmic differential pore volume distribution curve of the first catalyst layer (20), a peak value A present in a pore size range of 1 μm or more and 3 μm or less is 0.20 mL/g or more, and a peak value B present in a pore size range of more than 3 μm and 10 μm or less is 0.20 mL/g or more, respectively, Conditions 3 and 4 are defined as the conditions that, in a logarithmic differential pore volume distribution curve of the second catalyst layer (30), a peak value C present in a pore size range of 1 μm or more and 3 μm or less is 0.20 mL/g or more, and a peak value D present in a pore size range of more than 3 μm and 10 μm or less is 0.20 mL/g or more, respectively, the first catalyst layer (20) and the second catalyst layer (30) satisfy a predetermined combination of the conditions.

## Claims

### Claim 1

An exhaust gas purification catalyst comprising: a substrate extending in an exhaust gas flow direction; a first catalyst layer; and a second catalyst layer,
wherein the substrate comprises:
an inflow-side cell extending in the exhaust gas flow direction and having an open end on an exhaust gas inflow side thereof and a closed end on an exhaust gas outflow side thereof;
an outflow-side cell extending in the exhaust gas flow direction and having a closed end on an exhaust gas inflow side thereof and an open end on an exhaust gas outflow side thereof; and
a porous partition wall separating the inflow-side cell and the outflow-side cell from each other,
wherein the first catalyst layer is formed on an inflow-side cell side of the partition wall from an end on an exhaust gas inflow side of the partition wall along the exhaust gas flow direction,
wherein the second catalyst layer is formed on an outflow-side cell side of the partition wall from an end on an exhaust gas outflow side of the partition wall along a direction opposite to the exhaust gas flow direction, and
wherein,
assuming that:
Condition 1 is defined as the condition that, in a logarithmic differential pore volume distribution curve of the first catalyst layer obtained by mercury porosimetry, a peak value A is present in a pore size range of 1 μm or more and 3 μm or less and the peak value A is 0.20 mL/g or more;
Condition 2 is defined as the condition that, in the logarithmic differential pore volume distribution curve of the first catalyst layer obtained by mercury porosimetry, a peak value B is present in a pore size range of more than 3 μm and 10 μm or less and the peak value B is 0.20 mL/g or more;
Condition 3 is defined as the condition that, in a logarithmic differential pore volume distribution curve of the second catalyst layer obtained by mercury porosimetry, a peak value C is present in a pore size range of 1 μm or more and 3 μm or less and the peak value C is 0.20 mL/g or more; and
Condition 4 is defined as the condition that, in the logarithmic differential pore volume distribution curve of the second catalyst layer obtained by mercury porosimetry, a peak value D is present in a pore size range of more than 3 μm and 10 μm or less and the peak value D is 0.20 mL/g or more,
the second catalyst layer satisfies Condition 3 and does not satisfy Condition 4, or satisfies Condition 4 and does not satisfy Condition 3, or
satisfies Conditions 3 and 4, or satisfies none of Conditions 3 and 4, and
when the second catalyst layer satisfies Condition 3 and does not satisfy Condition 4, the first catalyst layer satisfies at least Condition 2 of Conditions 1 and 2,
when the second catalyst layer satisfies Condition 4 and does not satisfy Condition 3, the first catalyst layer satisfies at least Condition 1 of Conditions 1 and 2,
when the second catalyst layer satisfies Conditions 3 and 4, the first catalyst layer satisfies at least one of Conditions 1 and 2, or none of Conditions 1 and 2, and
when the second catalyst layer satisfies none of Conditions 3 and 4, the first catalyst layer satisfies Conditions 1 and 2.

### Claim 2 (depends on 1)

The exhaust gas purification catalyst as claimed in claim 1, wherein
the second catalyst layer satisfies Condition 3 and does not satisfy Condition 4, or satisfies Condition 4 and does not satisfy Condition 3, or satisfies Conditions 3 and 4, and
when the second catalyst layer satisfies Condition 3 and does not satisfy Condition 4, the first catalyst layer satisfies at least Condition 2 of Conditions 1 and 2,
when the second catalyst layer satisfies Condition 4 and does not satisfy Condition 3, the first catalyst layer satisfies at least Condition 1 of Conditions 1 and 2, and
when the second catalyst layer satisfies Conditions 3 and 4, the first catalyst layer satisfies at least one of Conditions 1 and 2.

### Claim 3 (depends on 1)

The exhaust gas purification catalyst as claimed in claim 1, wherein the peak value A in Condition 1 is 1.00 mL/g or less, and the peak value C in Condition 3 is 1.00 mL/g or less.

### Claim 4 (depends on 1)

The exhaust gas purification catalyst as claimed in claim 1, wherein the peak value B in Condition 2 is 1.00 mL/g or less, and the peak value D in Condition 4 is 1.00 mL/g or less.

### Claim 5 (depends on 1)

The exhaust gas purification catalyst as claimed in claim 1, wherein the peak value A in Condition 1 is 0.31 mL/g or more, and the peak value C in Condition 3 is 0.31 mL/g or more.

### Claim 6

A method for producing an exhaust gas purification catalyst comprising: a substrate extending in an exhaust gas flow direction; a first catalyst layer; and a second catalyst layer,
wherein the substrate comprises:
an inflow-side cell extending in the exhaust gas flow direction and having an open end on an exhaust gas inflow side thereof and a closed end on an exhaust gas outflow side thereof;
an outflow-side cell extending in the exhaust gas flow direction and having a closed end on an exhaust gas inflow side thereof and an open end on an exhaust gas outflow side thereof; and
a porous partition wall separating the inflow-side cell and the outflow-side cell from each other,
wherein the first catalyst layer is formed on an inflow-side cell side of the partition wall from an end on an exhaust gas inflow side of the partition wall along the exhaust gas flow direction,
wherein the second catalyst layer is formed on an outflow-side cell side of the partition wall from an end on an exhaust gas outflow side of the partition wall along a direction opposite to the exhaust gas flow direction,
wherein the method comprises the following steps of:
(1a) applying a first slurry containing a first pore forming agent onto the inflow-side cell side of the partition wall to form a first precursor layer;
(1b) applying a second slurry containing a second pore forming agent onto the outflow-side cell side of the partition wall to form a second precursor layer; and
(1c) calcining the first precursor layer and the second precursor layer to form the first catalyst layer and the second catalyst layer, respectively,
wherein, of the first and second pore forming agents, one pore forming agent has a median particle size D50 of more than 4 μm, and the other pore forming agent has a median particle size D50 of 4 μm or less,
wherein the first slurry contains an inorganic oxide particle, and the inorganic oxide particle contained in the first slurry has a median particle size D50 of 1 μm or more and 20 μm or less,
wherein an amount of the first pore forming agent contained in the first precursor layer is 10% by mass or more and 60% by mass or less based on a mass of the first catalyst layer,
wherein a mass of the first catalyst layer per unit volume of a portion of the substrate provided with the first catalyst layer is 5 g/L or more and 150 g/L or less,
wherein the second slurry contains an inorganic oxide particle, and the inorganic oxide particle contained in the second slurry has a median particle size D50 of 1 μm or more and 20 μm or less,
wherein an amount of the second pore forming agent contained in the second precursor layer is 10% by mass or more and 60% by mass or less based on a mass of the second catalyst layer, and
wherein a mass of the second catalyst layer per unit volume of a portion of the substrate provided with the second catalyst layer is 5 g/L or more and 150 g/L or less.

### Claim 7

A method for producing an exhaust gas purification catalyst comprising: a substrate extending in an exhaust gas flow direction; a first catalyst layer; and a second catalyst layer,
wherein the substrate comprises:
an inflow-side cell extending in the exhaust gas flow direction and having an open end on an exhaust gas inflow side thereof and a closed end on an exhaust gas outflow side thereof;
an outflow-side cell extending in the exhaust gas flow direction and having a closed end on an exhaust gas inflow side thereof and an open end on an exhaust gas outflow side thereof; and
a porous partition wall separating the inflow-side cell and the outflow-side cell from each other,
wherein the first catalyst layer is formed on an inflow-side cell side of the partition wall from an end on an exhaust gas inflow side of the partition wall along the exhaust gas flow direction,
wherein the second catalyst layer is formed on an outflow-side cell side of the partition wall from an end on an exhaust gas outflow side of the partition wall along a direction opposite to the exhaust gas flow direction,
wherein the second catalyst layer comprises: a lower layer formed on the outflow-side cell side of the partition wall; and an upper layer formed on the lower layer,
wherein the method comprises the following steps of:
(2a) applying a first slurry containing a first pore forming agent onto the inflow-side cell side of the partition wall to form a first precursor layer;
(2b) applying a third slurry containing a third pore forming agent onto the outflow-side cell side of the partition wall to form a third precursor layer;
(2c) applying a fourth slurry containing a fourth pore forming agent onto the third precursor layer to form a fourth precursor layer; and
(2d) calcining the first precursor layer, the third precursor layer and the fourth precursor layer to form the first catalyst layer, the lower layer and the upper layer, respectively,
wherein, of the first, third and fourth pore forming agents, one or two pore forming agents have a median particle size D50 of more than 4 μm, and the other one or two pore forming agents have a median particle size D50 of 4 μm or less,
wherein the first slurry contains an inorganic oxide particle, and the inorganic oxide particle contained in the first slurry has a median particle size D50 of 1 μm or more and 20 μm or less,
wherein an amount of the first pore forming agent contained in the first precursor layer is 10% by mass or more and 60% by mass or less based on a mass of the first catalyst layer,
wherein a mass of the first catalyst layer per unit volume of a portion of the substrate provided with the first catalyst layer is 5 g/L or more and 150 g/L or less,
wherein the third slurry contains an inorganic oxide particle, and the inorganic oxide particle contained in the third slurry has a median particle size D50 of 1 μm or more and 20 μm or less,
wherein an amount of the third pore forming agent contained in the third precursor layer is 10% by mass or more and 60% by mass or less based on a mass of the lower layer,
wherein a mass of the lower layer per unit volume of a portion of the substrate provided with the lower layer is 5 g/L or more and 90 g/L or less,
wherein the fourth slurry contains an inorganic oxide particle, and the inorganic oxide particle contained in the fourth slurry has a median particle size D50 of 1 μm or more and 20 μm or less,
wherein an amount of the fourth pore forming agent contained in the fourth precursor layer is 10% by mass or more and 60% by mass or less based on a mass of the upper layer, and
wherein a mass of the upper layer per unit volume of a portion of the substrate provided with the upper layer is 5 g/L or more and 60 g/L or less.

### Claim 8 (depends on 7)

The method as claimed in claim 7, wherein the third pore forming agent has a median particle size D50 of more than 4 μm, and the fourth pore forming agent has a median particle size D50 of 4 μm or less.

### Claim 9

A method for producing an exhaust gas purification catalyst comprising: a substrate extending in an exhaust gas flow direction; a first catalyst layer; and a second catalyst layer,
wherein the substrate comprises:
an inflow-side cell extending in the exhaust gas flow direction and having an open end on an exhaust gas inflow side thereof and a closed end on an exhaust gas outflow side thereof;
an outflow-side cell extending in the exhaust gas flow direction and having a closed end on an exhaust gas inflow side thereof and an open end on an exhaust gas outflow side thereof; and
a porous partition wall separating the inflow-side cell and the outflow-side cell from each other,
wherein the first catalyst layer is formed on an inflow-side cell side of the partition wall from an end on an exhaust gas inflow side of the partition wall along the exhaust gas flow direction,
wherein the second catalyst layer is formed on an outflow-side cell side of the partition wall from an end on an exhaust gas outflow side of the partition wall along a direction opposite to the exhaust gas flow direction,
wherein the first catalyst layer comprises: a lower layer formed on the inflow-side cell side of the partition wall; and an upper layer formed on the lower layer,
wherein the method comprises the following steps of:
(3a) applying a second slurry containing a second pore forming agent onto the outflow-side cell side of the partition wall to form a second precursor layer;
(3b) applying a fifth slurry containing a fifth pore forming agent onto the inflow-side cell side of the partition wall to form a fifth precursor layer;
(3c) applying a sixth slurry containing a sixth pore forming agent onto the fifth precursor layer to form a sixth precursor layer; and
(3d) calcining the second precursor layer, the fifth precursor layer and the sixth precursor layer to form the second catalyst layer, the lower layer and the upper layer, respectively,
wherein, of the second, fifth and sixth pore forming agents, one or two pore forming agents have a median particle size D50 of more than 4 μm, and the other one or two pore forming agents have a median particle size D50 of 4 μm or less,
wherein the second slurry contains an inorganic oxide particle, and the inorganic oxide particle contained in the second slurry has a median particle size D50 of 1 μm or more and 20 μm or less,
wherein an amount of the second pore forming agent contained in the second precursor layer is 10% by mass or more and 60% by mass or less based on a mass of the second catalyst layer,
wherein a mass of the second catalyst layer per unit volume of a portion of the substrate provided with the second catalyst layer is 5 g/L or more and 150 g/L or less,
wherein the fifth slurry contains an inorganic oxide particle, and the inorganic oxide particle contained in the fifth slurry has a median particle size D50 of 1 μm or more and 20 μm or less,
wherein an amount of the fifth pore forming agent contained in the fifth precursor layer is 10% by mass or more and 60% by mass or less based on a mass of the lower layer,
wherein a mass of the lower layer per unit volume of a portion of the substrate provided with the lower layer is 5 g/L or more and 90 g/L or less,
wherein the sixth slurry contains an inorganic oxide particle, and the inorganic oxide particle contained in the sixth slurry has a median particle size D50 of 1 μm or more and 20 μm or less,
wherein an amount of the sixth pore forming agent contained in the sixth precursor layer is 10% by mass or more and 60% by mass or less based on a mass of the upper layer, and
wherein a mass of the upper layer per unit volume of a portion of the substrate provided with the upper layer is 5 g/L or more and 60 g/L or less.

### Claim 10 (depends on 9)

The method as claimed in claim 9, wherein the fifth pore forming agent has a median particle size D50 of more than 4 μm, and the sixth pore forming agent has a median particle size D50 of 4 μm or less.