# US 2026/0005028 A1 · Pulsing deposition using fast response mfc

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0005028 A1
- Document ID: US20260005028A1
- Status: Published application
- Kind: A1
- Application number: 18/758,301
- Filed: 2024-06-28
- Published: 2026-01-01
- Earliest claimed: 2024-06-28
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Zheyuan Chen; Jianxin Lei; Allyson N. Vu
- Web page: https://patentgrep.com/patent/US20260005028A1

## CPC

- H10P 14/418: {the conductive layers comprising transition metals}
- C23C 14/0042: {Controlling partial pressure or flow rate of reactive or inert gases with feedback of measurements}
- C23C 14/0089: {in metallic mode}
- C23C 14/0641: {Nitrides (C23C14/0617 takes precedence)}
- C23C 14/3414: {Metallurgical or chemical aspects of target preparation, e.g. casting, powder metallurgy}
- C23C 14/3492: {Variation of parameters during sputtering}
- C23C 14/54: Controlling or regulating the coating process
- H10D 64/667: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN workfunction layers (having lateral variation H10D64/671)}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Methods for forming work function layers (e.g., titanium nitride work function layers) for transistors are described. The methods energizing a process gas disposed in an inner volume of a processing chamber to create a plasma, and pulsing the process gas between a poison regime and a metallic regime using a fast response mass flow controller to deposit the work function layer on the substrate surface.

## Claims

### Claim 1

A method of forming a work function layer for a transistor, the method comprising:
energizing a process gas disposed in an inner volume of a processing chamber to create a plasma, the processing chamber having a sputtering target and the plasma causing atoms to eject from the sputtering target toward a substrate surface; and
pulsing the process gas between a poison regime and a metallic regime using a fast response mass flow controller to deposit the work function layer on the substrate surface, the fast response mass flow controller having an ON response delay and an OFF response delay independently less than or equal to 0.25 seconds at a flow rate in the range of 5 sccm to 100 sccm.

### Claim 2 (depends on 1)

The method of claim 1, wherein the sputtering target comprises titanium.

### Claim 3 (depends on 1)

The method of claim 1, wherein the sputtering target comprises titanium nitride.

### Claim 4 (depends on 1)

The method of claim 1, wherein the process gas comprises nitrogen (N2).

### Claim 5 (depends on 4)

The method of claim 4, wherein the process gas further comprises argon.

### Claim 6 (depends on 5)

The method of claim 5, wherein the argon is flowed at a constant rate and the nitrogen is pulsed.

### Claim 7 (depends on 4)

The method of claim 4, wherein the metallic regime comprises a nitrogen flow rate in the range of 20 sccm to 30 sccm.

### Claim 8 (depends on 7)

The method of claim 7, wherein the poison regime comprises a nitrogen flow rate in the range of 25 sccm to 35 sccm, and the metallic regime flow rate is less than the poison regime flow rate.

### Claim 9 (depends on 8)

The method of claim 8, wherein the poison regime flow rate is greater than or equal to 2 sccm higher than the metallic regime flow rate.

### Claim 10 (depends on 8)

The method of claim 8, wherein the poison regime pulse has a duration in the range of 50 msec to 500 msec.

### Claim 11 (depends on 8)

The method of claim 8, wherein the metallic regime pulse has a duration in the range of 50 msec to 500 msec.

### Claim 12 (depends on 8)

The method of claim 8, wherein the poison regime pulse and the metallic regime pulse have substantially the same durations in the range of 75 msec to 125 msec.

### Claim 13 (depends on 8)

The method of claim 8, wherein the metallic regime reduces nitrogen incorporated into the work function layer at an edge of the wafer, relative to the poison regime.

### Claim 14 (depends on 8)

The method of claim 8, wherein a center-to-edge uniformity of the work function layer on the substrate surface is greater than a center-to-edge uniformity of a work function layer deposited without pulsing between the poison regime and the metallic regime.

### Claim 15 (depends on 14)

The method of claim 14, wherein a N/Ti ratio center-to-edge difference for the work function layer is less than or equal to 0.025 absolute.

### Claim 16 (depends on 14)

The method of claim 14, wherein a N/Ti ratio of the work function layer is in the range of 0.95 to 1.05.

### Claim 17

A method of forming a titanium nitride work function layer for a transistor, the method comprising:
flowing a process gas comprising argon and nitrogen into an inner volume of a processing chamber comprising a titanium target and a substrate with a substrate surface;
energizing the process gas to create a plasma in the inner volume to cause titanium atoms to eject from the sputtering target toward the substrate surface; and
pulsing the process gas between a poison regime and a metallic regime using a fast response mass flow controller to deposit the titanium nitride work function layer on the substrate surface,
wherein the fast response mass flow controller having an ON response delay and an OFF response delay independently less than or equal to 0.15 seconds at a flow rate in the range of 5 sccm to 100 sccm,
wherein the metallic regime has a nitrogen flow rate in the range of 20 sccm to 30 sccm, and the poison regime has a nitrogen flow rate in the range of 25 sccm to 35 sccm and is greater than the nitrogen flow rate of the metallic regime.

### Claim 18 (depends on 17)

The method of claim 17, wherein the poison regime pulse and the metallic regime pulse have substantially the same durations in the range of 75 msec to 125 msec.

### Claim 19 (depends on 17)

The method of claim 17, wherein the argon flowed of the process gas is maintained at a constant rate while the nitrogen flow is pulsed.

### Claim 20 (depends on 17)

The method of claim 17, wherein a center-to-edge uniformity of the titanium nitride work function layer on the substrate surface is greater than a center-to-edge uniformity of a titanium nitride function layer deposited without pulsing the nitrogen flow between the poison regime and the metallic regime.